摘要: A composite base metal oxide catalyst of improved high temperature stability is provided by prereacting a selected base metal oxide catalyst or its precursor compounds with a selected refractory high-surface-area spinel or its precursor compounds to form a crystalline solid solution of the catalyst and the spinel. This solid solution has the properties of good catalytic activity and high temperature structural and surface area stability. An example of such a composite catalyst is CuCr2O4 in solid solution with NiAl2O4.
摘要翻译: 通过将所选择的基体金属氧化物催化剂或其前体化合物与选定的耐火高表面积尖晶石或其前体化合物预反应以形成催化剂的结晶固溶体和 尖晶石 该固溶体具有良好的催化活性和高温结构和表面积稳定性。 这种复合催化剂的实例是具有NiAl 2 O 4的固溶体中的CuCr 2 O 4。