PROCESS FOR PRODUCTION OF SYNTHETIC QUARTZ GLASS
    1.
    发明申请
    PROCESS FOR PRODUCTION OF SYNTHETIC QUARTZ GLASS 有权
    合成石英玻璃生产工艺

    公开(公告)号:US20110179827A1

    公开(公告)日:2011-07-28

    申请号:US13080704

    申请日:2011-04-06

    IPC分类号: C03B8/04 C03B20/00

    摘要: The present invention relates to a process for production of a synthetic quartz glass having a fluorine concentration of 1,000 mass ppm or more, the process comprising: (a) a step of depositing and growing quartz glass fine particles obtained by flame hydrolysis of a glass forming raw material onto a substrate, to thereby form a porous glass body; (b) a step of keeping the porous glass body in a reaction vessel that is filled with elemental fluorine (F2) or a mixed gas comprising elemental fluorine (F2) diluted with an inert gas and contains a solid metal fluoride, to thereby obtain a fluorine-containing porous glass body; and (c) a step of heating the fluorine-containing porous glass body to a transparent vitrification temperature, to thereby obtain a fluorine-containing transparent glass body.

    摘要翻译: 本发明涉及一种氟浓度为1000质量ppm以上的合成石英玻璃的制造方法,其特征在于,包括:(a)沉积和生长通过玻璃成形的火焰水解得到的石英玻璃微粒子的工序 原料在基板上,从而形成多孔玻璃体; (b)将多孔玻璃体保持在填充有元素氟(F2)的反应容器或包含用惰性气体稀释的元素氟(F2)的混合气体并含有固体金属氟化物的步骤,从而获得 含氟多孔玻璃体; 和(c)将含氟多孔质玻璃体加热至透明玻璃化温度的步骤,得到含氟透明玻璃体。

    FLUOROPOLYMER THIN FILM AND METHOD FOR ITS PRODUCTION
    3.
    发明申请
    FLUOROPOLYMER THIN FILM AND METHOD FOR ITS PRODUCTION 审中-公开
    氟聚合物薄膜及其生产方法

    公开(公告)号:US20100080903A1

    公开(公告)日:2010-04-01

    申请号:US12581220

    申请日:2009-10-19

    IPC分类号: C23C14/24

    摘要: To provide a method for producing a fluoropolymer excellent in adhesion to a substrate and film strength.A method for producing a fluoropolymer thin film, which comprises forming a fluoropolymer thin film on a substrate by a physical vapor deposition method using, as an evaporation source, a fluoropolymer having a fluorinated aliphatic ring structure in its main chain and having a weight average molecular weight of from 3,000 to 80,000.

    摘要翻译: 提供一种制造具有优异的基材粘合性和膜强度的含氟聚合物的方法。 一种含氟聚合物薄膜的制造方法,其特征在于,包括在物理气相沉积法的基板上形成含氟聚合物薄膜作为蒸发源,在其主链中具有含氟脂肪族环结构的含氟聚合物,其重均分子量 重量从3,000到80,000。

    METHOD FOR TREATING SURFACE OF OXIDE GLASS WITH FLUORINATING AGENT
    4.
    发明申请
    METHOD FOR TREATING SURFACE OF OXIDE GLASS WITH FLUORINATING AGENT 有权
    用荧光剂处理氧化物表面的方法

    公开(公告)号:US20100089096A1

    公开(公告)日:2010-04-15

    申请号:US12640199

    申请日:2009-12-17

    IPC分类号: C03C15/00

    摘要: To provide a novel fluorination treatment method whereby the surface of oxide glass can be treated for fluorination at low cost and with excellent adhesiveness.A method for treating the surface of oxide glass, which comprises contacting the surface of oxide glass with a gas of a fluorinating agent or a mixed gas having a fluorinating agent diluted with an inert gas, wherein the fluorinating agent is an elemental fluorine, or a fluorine compound capable of cleaving a bond between an oxygen atom and a metal atom in the framework of the oxide glass and forming a bond between a fluorine atom and the metal atom; and the concentration of hydrogen fluoride at the surface of oxide glass with which the fluorinating agent is in contact, is controlled to be at most 1 mol %.

    摘要翻译: 为了提供一种新颖的氟化处理方法,可以将氧化物玻璃的表面以低成本和优异的粘合性处理氟化。 一种处理氧化物玻璃表面的方法,包括使氧化物玻璃的表面与氟化剂的气体或具有用惰性气体稀释的氟化剂的混合气体接触,其中氟化剂是元素氟,或 氟化合物,其能够在氧化物玻璃的骨架中切割氧原子和金属原子之间的键,并在氟原子和金属原子之间形成键; 并且与氟化剂接触的氧化物玻璃表面的氟化氢浓度控制在1摩尔%以下。