摘要:
Heterophasic propylene copolymer comprising a matrix (M) being a polypropylene, said polypropylene comprises at least three polypropylene fractions, the three polypropylene fractions differ from each other by the melt flow rate MFR2 (230° C.) and at least one of the three polypropylene fractions has a melt flow rate MFR2 (230° C.) in the range of 1.0 to 15.0 g/10 min, and an elastomeric propylene copolymer dispersed in said matrix, wherein the heterophasic propylene copolymer has a melt flow rate MFR2 (230° C.) of equal or more than 20.0 g/10 min, and the amorphous phase of the xylene cold soluble fraction of the heterophasic propylene copolymer has an intrinsic viscosity of equal or higher than 2.0 dl/g.
摘要:
Heterophasic propylene copolymer comprising —a matrix (M) being a polypropylene, said polypropylene comprises at least three polypropylene fractions, the three polypropylene fractions differ from each other by the melt flow rate MFR2 (230° C.) and at least one of the three polypropylene fractions has a melt flow rate MFR2 (230° C.) in the range of 1.0 to 15.0 g/10 min, and —an elastomeric propylene copolymer dispersed in said matrix, wherein —the heterophasic propylene copolymer has a melt flow rate MFR2 (230° C.) of equal or more than 20.0 g/10 min, and —the amorphous phase of the xylene cold soluble fraction of the heterophasic propylene copolymer has an intrinsic viscosity of equal or higher than 2.0 dl/g.
摘要:
Heterophasic propylene copolymer (HECO) comprising: (a) a polypropylene matrix comprising: (a1) a first propylene homopolymer fraction (PPH1) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >200 to 500 g/10 min, (a2-1) a second propylene homopolymer fraction (PPH2) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >30 to ≦200 g/10 min or, (a2-2) a second propylene homopolymer fraction (PPH2) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >5 to ≦30 g/10 min and, (a3-1) a third propylene homopolymer fraction (PPH3) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 0.03 to ≦5 g/10 min, if the second propylene homopolymer fraction is fraction (a2-1) or, (a3-2) a third propylene homopolymer fraction (PPH3) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >30 to ≦200 g/10 min, if the second propylene homopolymer fraction is fraction (a2-2), wherein the polypropylene matrix has a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 30 to 500 g/10 min and a xylene cold soluble fraction determined at 23° C. according to ISO 6427 in the range of 0.5 to
摘要:
Heterophasic propylene copolymer (HECO) comprising: (a) a polypropylene matrix comprising: (a1) a first propylene homopolymer fraction (PPH1) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >200 to 500 g/10 min, (a2-1) a second propylene homopolymer fraction (PPH2) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >30 to ≦200 g/10 min or, (a2-2) a second propylene homopolymer fraction (PPH2) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >5 to ≦30 g/10 min and, (a3-1) a third propylene homopolymer fraction (PPH3) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 0.03 to ≦5 g/10 min, if the second propylene homopolymer fraction is fraction (a2-1) or, (a3-2) a third propylene homopolymer fraction (PPH3) with a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of >30 to ≦200 g/10 min, if the second propylene homopolymer fraction is fraction (a2-2), wherein the polypropylene matrix has a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of 30 to 500 g/10 min and a xylene cold soluble fraction determined at 23° C. according to ISO 6427 in the range of 0.5 to
摘要:
The present invention relates to a polypropylene composition showing a high melt flow rate and high melt strength while maintaining high impact strength. The composition of the present invention is obtainable by using a low molecular weight linear isotactic polypropylene as melt flow enhancer for a high molecular weight polypropylene having a high melt strength and impact strength. The inventive composition could be used for the production of different articles.
摘要:
The invention relates to a polypropylene composition showing a high melt flow rate and simultaneously high stiffness and a process for the production thereof. The invention further relates to a material comprising the inventive polypropylene.
摘要:
The invention relates to a polypropylene composition showing a high melt flow rate and simultaneously high stiffness and a process for the production thereof. The invention further relates to a material comprising the inventive polypropylene.
摘要:
The present invention relates to a polypropylene composition showing a high melt flow rate and high melt strength while maintaining high impact strength. The composition of the present invention is obtainable by using a low molecular weight linear isotactic polypropylene as melt flow enhancer for a high molecular weight polypropylene having a high melt strength and impact strength. The inventive composition could be used for the production of different articles.
摘要:
Heterophasic propylene copolymer comprising (a) a matrix (M) being a polypropylene (PP), said polypropylene (PP) has a polydispersity index (PI) of at least 5.0, and (b) an elastomeric propylene copolymer (EC) dispersed in said matrix (M), wherein (i) said heterophasic propylene copolymer has a melt flow rate MFR2 (230° C.) of equal or below 1.0 g/10 min, (ii) the amorphous phase (AM) of the xylene cold soluble fraction (XCS) of the heterophasic propylene copolymer has an intrinsic viscosity (IV) of at least 3.5 dl/g.
摘要:
Heterophasic propylene copolymer comprising (a) a matrix (M) being a polypropylene (PP), said polypropylene (PP) has a polydispersity index (PI) of at least 5.0, and (b) an elastomeric propylene copolymer (EC) dispersed in said matrix (M), wherein (i) said heterophasic propylene copolymer has a melt flow rate MFR2 (230° C.) of equal or below 1.0 g/10 min, (ii) the amorphous phase (AM) of the xylene cold soluble fraction (XCS) of the heterophasic propylene copolymer has an intrinsic viscosity (IV) of at least 3.5 dl/g.