Polyester molding composition
    1.
    发明申请
    Polyester molding composition 有权
    聚酯成型组合物

    公开(公告)号:US20020115771A1

    公开(公告)日:2002-08-22

    申请号:US10022878

    申请日:2001-12-20

    Applicant: DEGUSSA AG

    CPC classification number: C08L67/02 C08L23/08 C08L33/06 C08L53/00 C08L2666/02

    Abstract: The present invention relates to a molding composition containing thermoplastic polyesters, impact-modifying component which contains anhydride groups, a copolymer of null-olefin, acrylic compound, olefinically unsaturated epoxide, carboxylic anhydride, carboximide, oxazoline and/or oxazinone, which has improved low-temperature impact strength; methods of making molding with the molding composition and molding containing the composition.

    Abstract translation: 本发明涉及包含热塑性聚酯的成型组合物,含有酸酐基团的冲击改性组分,α-烯烃,丙烯酸化合物,烯属不饱和环氧化物,羧酸酐,甲酰亚胺,恶唑啉和/或恶嗪酮的共聚物,其具有改进的低 - 冲击强度; 用模塑组合物成型和含有组合物的模塑方法。

    Molded object with better short-time deflection temperature under load properties
    3.
    发明申请
    Molded object with better short-time deflection temperature under load properties 失效
    模制对象在负载特性下具有更好的短时挠曲温度

    公开(公告)号:US20020180098A1

    公开(公告)日:2002-12-05

    申请号:US10117192

    申请日:2002-04-08

    Applicant: DEGUSSA AG

    Abstract: A molded object is manufactured by a process, comprising: a) preparing a shaped object by molding a formulation of: 35 to 100% by weight of a thermoplastic polyester, 0 to 60% by weight of filler or a reinforcing material, 0 to 20% by weight of an impact modifying rubber, 0 to 30% by weight of a flame retardant, 0 to 20% by weight of a synergist and 0 to 5% by weight of other additives and/or processing agents; and b) treating the molded object for at least 1 hour at a temperature ranging from 180 to 250null C., thereby preparing a molded object with improved short-time deflection temperature under load properties.

    Abstract translation: 模制品通过以下工艺制造,包括:a)通过模制以下配方来制备成形物体:35至100重量%的热塑性聚酯,0至60重量%的填料或增强材料,0至20 抗冲击改性橡胶,0〜30重量%的阻燃剂,0〜20重量%的增效剂和0〜5重量%的其他添加剂和/或加工剂的重量% 和b)在180-250℃的温度范围内处理模制物体至少1小时,由此在负载特性下制备具有改善的短时间挠曲温度的成型体。

Patent Agency Ranking