公开(公告)号:US10941465B2
公开(公告)日:2021-03-09
申请号:US16073563
申请日:2017-02-21
申请人: Diamet Corporation
发明人: Yoshinari Ishii
IPC分类号: C22C9/06 , B22F3/11 , B22F1/00 , C22C9/02 , B22F5/00 , F16C33/10 , F16C17/02 , F16C33/12 , B22F5/10 , C22C1/04 , F16C33/14 , F16C17/10
摘要: The Cu-based sintered sliding material has a composition including, by mass %, 7% to 35% of Ni, 1% to 10% of Sn, 0.9% to 3% of P, and 0.5% to 5% of C, with a remainder of Cu and inevitable impurities, wherein the Cu-based sintered sliding material includes a sintered body including: alloy grains that contain Sn and C and contain a Cu—Ni-based alloy as a main component; grain boundary phases that contain Ni and P as main components and are dispersedly distributed in grain boundaries of the alloy grains; and free graphite that intervenes at the grain boundaries of the alloy grains, the Cu-based sintered sliding material has a structure in which pores are dispersedly formed in the grain boundaries of the alloy grains, and an amount of C in a metal matrix including the alloy grains and the grain boundary phases is, by mass %, 0.02% to 0.20%.
-
公开(公告)号:US11248654B2
公开(公告)日:2022-02-15
申请号:US16763500
申请日:2018-11-14
申请人: DIAMET CORPORATION
发明人: Hajime Kouno , Yoshinari Ishii , Tsuneo Maruyama , Jyun Katou , Kenji Orito
摘要: On an inner peripheral surface of a bearing hole into which a shaft is inserted, concave oil supply surfaces arranged dispersively like separated islands and a sliding surface continuous around the oil supply surfaces to hold an outer peripheral surface of the shaft are formed: a maximum height difference between the sliding surface and the oil supply surfaces is not less than 0.01% and not more than 0.5% of an inner diameter Di of the sliding surface; a surface aperture area ratio of pores at the sliding surface is not more than 10%; a surface aperture area ratio of pores at the oil supply surfaces is more than 10% and less than 40%; and an area of each of the oil supply surfaces is not less than 0.03 mm2 and not more than 0.2×Di2 (mm2).
-
公开(公告)号:US10683566B2
公开(公告)日:2020-06-16
申请号:US15507567
申请日:2015-09-04
申请人: Diamet Corporation
IPC分类号: C22C9/06 , B22F1/00 , B22F5/00 , B22F3/02 , B22F3/10 , C22C1/04 , F16C33/14 , B22F3/16 , B22F5/10 , F16C33/12
摘要: Provided is a Cu-based sintered bearing comprising: 15-36 mass % of Ni; 3-13 mass % of Sn; 0.05-0.55 mass % of P; and 0.02-4 mass % of C in total, the balance consisting of Cu and inevitable impurities, wherein the content of C forming an alloy with a matrix within Cu—Ni-based main phase grains is 0.02-0.10 mass %.
-
公开(公告)号:US10532406B2
公开(公告)日:2020-01-14
申请号:US15510561
申请日:2015-09-10
申请人: Diamet Corporation
发明人: Shinichi Takezoe , Yoshinari Ishii
IPC分类号: B22F7/00 , B22F5/10 , B22F3/11 , C22C9/06 , C22C19/03 , B22F1/00 , B22F3/16 , C22C19/00 , C22C30/02 , C22C30/04 , F16C33/12 , F16C33/14 , C22C1/04 , C22C1/08 , C22C1/10
摘要: A sintered sliding material with excellent corrosion resistance, heat resistance, and wear resistance is provided. The sintered sliding material has a composition made of: 36-86 mass % of Ni; 1-11 mass % of Sn; 0.05-1.0 mass % of P; 1-9 mass % of C; and the Cu balance including inevitable impurities. The sintered sliding material is made of a sintered material of a plurality of grains of alloy of Ni—Cu alloy or Cu—Ni alloy, the Ni—Cu alloy and the Cu—Ni alloy containing Sn, P, C, and Si; has a structure in which pores are dispersedly formed in grain boundaries of the plurality of the grains of alloy; and as inevitable impurities in a matrix constituted from the grains of alloy, a C content is 0.6 mass % or less and a Si content is 0.15 mass % or less.
-
公开(公告)号:US09663844B2
公开(公告)日:2017-05-30
申请号:US14372357
申请日:2013-02-21
申请人: Diamet Corporation
发明人: Yoshinari Ishii
IPC分类号: C22C9/00 , C22C1/04 , C22C9/02 , C22C9/04 , C22C9/06 , C22C19/03 , C22C1/05 , C22C1/10 , C22C30/02 , C22C30/06 , C22C32/00 , C22C38/00 , C22C38/16 , F16C33/12 , B22F1/00
CPC分类号: C22C1/0425 , B22F1/0059 , C22C1/05 , C22C1/10 , C22C9/00 , C22C9/02 , C22C9/04 , C22C9/06 , C22C19/03 , C22C30/02 , C22C30/06 , C22C32/0089 , C22C38/002 , C22C38/004 , C22C38/008 , C22C38/16 , F16C33/121
摘要: A sintered bearing has a structure in which Ni—P alloy particles having an average diameter of 10 to 100 μm are dispersed in an amount of 1 to 20% by mass in a Cu-based sintered alloy base, a Fe—Cu-based sintered alloy base or a Cu—Ni-based sintered alloy base. The Ni—P alloy particles are derived from a raw material powder comprising 1 to 12% by mass of P; and a remainder composed of Ni and inevitable impurities. The Cu-based sintered alloy base contains no less than 40% by mass of Cu. The Fe—Cu-based sintered alloy base contains no more than 50% by mass of Fe. The Cu—Ni-based sintered alloy base contains 20 to 40% by mass of Ni and 0.1 to 1.0% by mass of P; or contains 10 to 25% by mass of Ni, 10 to 25% by mass of Zn and 0.1 to 1.0% by mass of P.
-
公开(公告)号:US20150037196A1
公开(公告)日:2015-02-05
申请号:US14520479
申请日:2014-10-22
申请人: DIAMET CORPORATION
发明人: Yoshinari Ishii , Tsuneo Maruyama , Yoshiki Tamura
CPC分类号: B22F3/26 , B22F1/007 , B22F3/12 , B22F5/00 , B22F2003/248 , B22F2301/10 , B22F2302/40 , B22F2302/45 , C22C1/0425 , C22C9/02 , C22C9/06 , C22C32/0084 , C22C32/0089 , F16C33/121
摘要: A Cu-based sintered sliding member that can be used under high-load conditions. The sliding member is age-hardened, including 5 to 30 mass % Ni, 5 to 20 mass % Sn, 0.1 to 1.2 mass % P, and the rest including Cu and unavoidable impurities. In the sliding member, an alloy phase containing higher concentrations of Ni, P and Sn than their average concentrations in the whole part of the sliding member, is allowed to be present in a grain boundary of a metallic texture, thereby achieving excellent wear resistance. Hence, without needing expensive hard particles, there can be obtained, at low cost, a Cu-based sintered sliding member usable under high-load conditions. Even more excellent wear resistance is achieved by containing 0.3 to 10 mass % of at least one solid lubricant selected from among graphite, graphite fluoride, molybdenum disulfide, tungsten disulfide, boron nitride, calcium fluoride, talc and magnesium silicate mineral powders.
摘要翻译: 可在高负荷条件下使用的Cu基烧结滑动件。 滑动构件经时效硬化,其中包括5至30质量%的Ni,5至20质量%的Sn,0.1至1.2质量%的P,其余包括Cu和不可避免的杂质。 在滑动构件中,允许在金属组织的晶界中存在Ni,P和Sn的含量高于其在滑动构件的整个部分中的平均浓度的合金相,从而获得优异的耐磨性。 因此,在不需要昂贵的硬质颗粒的情况下,可以以低成本获得可在高负载条件下使用的Cu系烧结滑动构件。 通过含有0.3〜10质量%的选自石墨,氟化石墨,二硫化钼,二硫化钨,氮化硼,氟化钙,滑石粉和硅酸镁矿物粉末中的至少一种固体润滑剂,可以获得更优异的耐磨性。
-
公开(公告)号:US20140352495A1
公开(公告)日:2014-12-04
申请号:US14372357
申请日:2013-02-21
申请人: Diamet Corporation
发明人: Yoshinari Ishii
CPC分类号: C22C1/0425 , B22F1/0059 , C22C1/05 , C22C1/10 , C22C9/00 , C22C9/02 , C22C9/04 , C22C9/06 , C22C19/03 , C22C30/02 , C22C30/06 , C22C32/0089 , C22C38/002 , C22C38/004 , C22C38/008 , C22C38/16 , F16C33/121
摘要: A sintered bearing has a structure in which Ni—P alloy particles having an average diameter of 10 to 100 μm are dispersed in an amount of 1 to 20% by mass in a Cu-based sintered alloy base, a Fe—Cu-based sintered alloy base or a Cu—Ni-based sintered alloy base. The Ni—P alloy particles are derived from a raw material powder comprising 1 to 12% by mass of P; and a remainder composed of Ni and inevitable impurities. The Cu-based sintered alloy base contains no less than 40% by mass of Cu. The Fe—Cu-based sintered alloy base contains no more than 50% by mass of Fe. The Cu—Ni-based sintered alloy base contains 20 to 40% by mass of Ni and 0.1 to 1.0% by mass of P; or contains 10 to 25% by mass of Ni, 10 to 25% by mass of Zn and 0.1 to 1.0% by mass of P.
摘要翻译: 烧结轴承具有在Cu系烧结合金基体,Fe-Cu系烧结体中分散有平均粒径为10〜100μm的Ni-P系合金粒子1〜20质量% 合金基体或Cu-Ni系烧结合金基体。 Ni-P合金粒子由含有1〜12质量%的P的原料粉末衍生而成, 余量由Ni和不可避免的杂质组成。 Cu系烧结合金基体含有不少于40质量%的Cu。 Fe-Cu系烧结合金基质含有不超过50质量%的Fe。 Cu-Ni类烧结合金基体含有20〜40质量%的Ni和0.1〜1.0质量%的P, 或含有10〜25质量%的Ni,10〜25质量%的Zn和0.1〜1.0质量%的P.
-
公开(公告)号:US11073178B2
公开(公告)日:2021-07-27
申请号:US16472660
申请日:2017-12-20
发明人: Hajime Kouno , Yoshinari Ishii , Tsuneo Maruyama , Jyun Katou , Kenji Orito
摘要: An oil-impregnated sintered bearing comprises a bearing hole. In the bearing, sliding surfaces supporting an outer circumferential surface of a shaft and an oil supply surface whose diameter is larger than that of the sliding surfaces are formed on an inner circumferential surface of the bearing hole into which the shaft is inserted. The sliding surfaces and the oil supply surfaces are adjacent to each other in the axial direction of the bearing hole. A height gap “d1” between the sliding surfaces and the oil supply surface is not less than 0.01% and not more than 15% of an inner diameter of the sliding surfaces. A surface opening percentage of the sliding surfaces is not higher than 10%. A surface opening percentage of the oil supply surface is higher than 10%. An average circle-equivalent diameter of opening parts of pores on the sliding surfaces is not larger than 20 μm.
-
公开(公告)号:US10745780B2
公开(公告)日:2020-08-18
申请号:US15507567
申请日:2015-09-04
申请人: Diamet Corporation
IPC分类号: C22C9/06 , B22F3/10 , B22F3/16 , B22F5/00 , B22F5/10 , C22C1/04 , B22F1/00 , B22F3/02 , F16C33/12 , F16C33/14
摘要: Provided is a Cu-based sintered bearing comprising: 15-36 mass % of Ni; 3-13 mass % of Sn; 0.05-0.55 mass % of P; and 0.02-4 mass % of C in total, the balance consisting of Cu and inevitable impurities, wherein the content of C forming an alloy with a matrix within Cu—Ni-based main phase grains is 0.02-0.10 mass %.
-
公开(公告)号:US09849511B2
公开(公告)日:2017-12-26
申请号:US14520479
申请日:2014-10-22
申请人: Diamet Corporation
发明人: Yoshinari Ishii , Tsuneo Maruyama , Yoshiki Tamura
IPC分类号: B22F3/26 , C22C1/04 , C22C9/02 , C22C9/06 , C22C32/00 , F16C33/12 , B22F1/00 , B22F3/12 , B22F5/00 , B22F3/24
CPC分类号: B22F3/26 , B22F1/007 , B22F3/12 , B22F5/00 , B22F2003/248 , B22F2301/10 , B22F2302/40 , B22F2302/45 , C22C1/0425 , C22C9/02 , C22C9/06 , C22C32/0084 , C22C32/0089 , F16C33/121
摘要: A Cu-based sintered sliding member that can be used under high-load conditions. The sliding member is age-hardened, including 5 to 30 mass % Ni, 5 to 20 mass % Sn, 0.1 to 1.2 mass % P, and the rest including Cu and unavoidable impurities. In the sliding member, an alloy phase containing higher concentrations of Ni, P and Sn than their average concentrations in the whole part of the sliding member, is allowed to be present in a grain boundary of a metallic texture, thereby achieving excellent wear resistance. Hence, without needing expensive hard particles, there can be obtained, at low cost, a Cu-based sintered sliding member usable under high-load conditions. Even more excellent wear resistance is achieved by containing 0.3 to 10 mass % of at least one solid lubricant selected from among graphite, graphite fluoride, molybdenum disulfide, tungsten disulfide, boron nitride, calcium fluoride, talc and magnesium silicate mineral powders.
-
-
-
-
-
-
-
-
-