Method for chemistry control in cooling systems
    1.
    发明授权
    Method for chemistry control in cooling systems 有权
    冷却系统化学控制方法

    公开(公告)号:US07632412B2

    公开(公告)日:2009-12-15

    申请号:US11556391

    申请日:2006-11-03

    IPC分类号: C02F1/42

    摘要: A method for controlling a cooling water tower comprising: providing a cooling tower system, which includes a recirculated evaporative cooling water stream, a source of make-up water, an evaporative cooling unit, a heat exchanger, a bleed off line, and a bleed-off valve which is in communication with said bleed-off line; providing a plurality of conduits through which said makeup water flows into said evaporative cooling water stream, wherein there is at least a first conduit that contains a weak acid cation ion exchange column and a second conduit that does not contain a weak acid ion exchange column, and wherein each conduit has at least one conduit valve; choosing a pH and a conductivity setpoint value and a deadband value above and below said setpoint value in said cooling tower system; measuring both the pH of said evaporative cooling water stream with one or more pH meters and conductivity of said evaporative cooling water stream with one or more conductivity meters; and implementing a response to said conductivity measurements and pH measurements is disclosed.

    摘要翻译: 一种用于控制冷却水塔的方法,包括:提供冷却塔系统,其包括再循环的蒸发冷却水流,补充水源,蒸发冷却单元,热交换器,排出管线和出口 与所述泄放线连通的阀; 提供多个导管,所述补充水通过该导管流入所述蒸发冷却水流中,其中至少包含弱酸性阳离子交换柱的第一导管和不含弱酸离子交换柱的第二导管, 并且其中每个导管具有至少一个导管阀; 在所述冷却塔系统中选择pH和电导率设定值以及高于和低于所述设定值的死区值; 用一个或多个pH计测量所述蒸发冷却水流的pH值,并用一个或多个电导率仪测量所述蒸发冷却水流的电导率; 并且公开了对所述电导率测量和pH测量的响应。

    METHOD FOR CHEMISTRY CONTROL IN COOLING SYSTEMS
    2.
    发明申请
    METHOD FOR CHEMISTRY CONTROL IN COOLING SYSTEMS 有权
    冷却系统中化学控制的方法

    公开(公告)号:US20080105621A1

    公开(公告)日:2008-05-08

    申请号:US11556391

    申请日:2006-11-03

    IPC分类号: C02F1/42

    摘要: A method for controlling a cooling water tower comprising: providing a cooling tower system, which includes a recirculated evaporative cooling water stream, a source of make-up water, an evaporative cooling unit, a heat exchanger, a bleed off line, and a bleed-off valve which is in communication with said bleed-off line; providing a plurality of conduits through which said makeup water flows into said evaporative cooling water stream, wherein there is at least a first conduit that contains a weak acid cation ion exchange column and a second conduit that does not contain a weak acid ion exchange column, and wherein each conduit has at least one conduit valve; choosing a pH and a conductivity setpoint value and a deadband value above and below said setpoint value in said cooling tower system; measuring both the pH of said evaporative cooling water stream with one or more pH meters and conductivity of said evaporative cooling water stream with one or more conductivity meters; and implementing a response to said conductivity measurements and pH measurements is disclosed.

    摘要翻译: 一种用于控制冷却水塔的方法,包括:提供冷却塔系统,其包括再循环的蒸发冷却水流,补充水源,蒸发冷却单元,热交换器,排出管线和出口 与所述泄放线连通的阀; 提供多个导管,所述补充水通过该导管流入所述蒸发冷却水流中,其中至少包含弱酸性阳离子交换柱的第一导管和不含弱酸离子交换柱的第二导管, 并且其中每个导管具有至少一个导管阀; 在所述冷却塔系统中选择pH和电导率设定值以及高于和低于所述设定值的死区值; 用一个或多个pH计测量所述蒸发冷却水流的pH值,并用一个或多个电导率仪测量所述蒸发冷却水流的电导率; 并且公开了对所述电导率测量和pH测量的响应。

    METHOD FOR MINIMIZING CORROSION, SCALE, AND WATER CONSUMPTION IN COOLING TOWER SYSTEMS
    3.
    发明申请
    METHOD FOR MINIMIZING CORROSION, SCALE, AND WATER CONSUMPTION IN COOLING TOWER SYSTEMS 审中-公开
    在冷却塔系统中最小化腐蚀,规模和水消耗的方法

    公开(公告)号:US20090277841A1

    公开(公告)日:2009-11-12

    申请号:US12116677

    申请日:2008-05-07

    IPC分类号: C02F9/00 C02F1/42

    摘要: This invention is an improved process for operation of evaporative recirculating cooling systems. In addition to reducing the scaling and corrosive tendencies of the water, the method eliminates or reduces discharge from the system without creating any localized corrosive or scaling conditions as a result of the treatment process. The described measurement and control system generally comprises an array of measurements, a means of implementing control logic, and an array of control actions including activating an ion exchange device to treat makeup water. The measurements can include of physical measurements of flow rates, chemical measurements of water composition, and performance-related metrics such as water corrosiveness or scaling tendency. Preferably, the measurements include one or more of pH, conductivity, hardness, alkalinity, corrosiveness, scaling tendency, treatment additive dosage level, and treatment additive residual of the makeup, treated makeup, and recirculating water.

    摘要翻译: 本发明是蒸发循环冷却系统的改进方法。 除了降低水的结垢和腐蚀倾向之外,该方法消除或减少了系统的排放,而不会由于处理过程而产生任何局部的腐蚀性或结垢状况。 所描述的测量和控制系统通常包括测量阵列,实现控制逻辑的手段,以及包括激活离子交换装置以处理补充水的控制动作阵列。 测量可以包括流速的物理测量,水分组成的化学测量以及性能相关的指标,如水的腐蚀性或结垢倾向。 优选地,测量包括化妆,处理的化妆品和再循环水中的pH,电导率,硬度,碱度,腐蚀性,结垢倾向,处理添加剂剂量水平和处理添加剂残留物中的一种或多种。

    Compositions comprising transition metals for treating and monitoring
liquid systems
    7.
    发明授权
    Compositions comprising transition metals for treating and monitoring liquid systems 失效
    包含用于处理和监测液体体系的过渡金属的组合物

    公开(公告)号:US5200106A

    公开(公告)日:1993-04-06

    申请号:US585899

    申请日:1990-09-20

    IPC分类号: G01N33/18

    摘要: Methods for utilizing transition metals as tracers in aqueous liquid systems are provided by this invention. Transition metals with low background levels in system waters are identified as preferred when soluble in said aqueous liquid systems. The transition metals show low levels of deposition on equipment scale and provide reliable information as to the process history of the liquid systems.

    摘要翻译: 在水性液体体系中利用过渡金属作为示踪剂的方法由本发明提供。 在可溶于所述含水液体体系中,在系统水中具有低背景水平的过渡金属被确定为优选的。 过渡金属在设备规模上显示出低沉积水平,并为液体系统的工艺历史提供可靠的信息。

    Zinc stabilization with modified acrylamide based polymers and corrosion
inhibition derived therefrom
    8.
    发明授权
    Zinc stabilization with modified acrylamide based polymers and corrosion inhibition derived therefrom 失效
    具有改性丙烯酰胺基聚合物的锌稳定化及其衍生的腐蚀抑制

    公开(公告)号:US4973428A

    公开(公告)日:1990-11-27

    申请号:US422386

    申请日:1989-10-16

    IPC分类号: C02F5/12 C23F11/08

    CPC分类号: C23F11/08 C02F5/125

    摘要: New zinc stabilizing polymers containing at least 5 mole percent of a monomer represented by the structure: ##STR1## wherein: R is independently, at each occurrence, chosen from H and lower (C.sub.1 -C.sub.4) alkyl groups;R' is a hydrocarbonaceous bridging group containing from 1-12 carbon atom;X is chosen from --SO.sub.3 M, --OH, --COOM groups or mixtures thereof,M is hydrogen or some other cation species; andn ranges from 1-10,are described. Also, the use of these polymers in combination with zinc salts, and in further combination with phosphate salts, to inhibit corrosion of iron containing metals, and other metals, when these metals are exposed to industrial waters is demonstrated. Deposit control or scale inhibition on these metals exposed to industrial waters is also observed.

    摘要翻译: 含有至少5摩尔%的由以下结构表示的单体的新的锌稳定化聚合物:其中:R各自独立地选自H和低级(C 1 -C 4)烷基; R'是含有1-12个碳原子的烃基桥联基团; X选自-SO 3 M,-OH,-COOM基团或其混合物,M是氢或一些其它阳离子物质; 并描述n的范围为1-10。 此外,证明了当这些金属暴露于工业水中时,这些聚合物与锌盐的组合以及与磷酸盐的进一步组合用于抑制含铁金属和其它金属的腐蚀。 也观察到暴露于工业水域的这些金属的沉积物控制或垢垢抑制。

    Cooling water corrosion control method and composition
    9.
    发明授权
    Cooling water corrosion control method and composition 失效
    冷却水腐蚀控制方法及组成

    公开(公告)号:US4904413A

    公开(公告)日:1990-02-27

    申请号:US287633

    申请日:1988-12-20

    IPC分类号: C23F11/10

    CPC分类号: C23F11/10

    摘要: A composition and method for inhibiting corrosion in industrial cooling waters which contain hardness and have a pH of at least 8, which composition comprises a water-soluble organic phosphonate capable of inhibiting corrosion in an aqueous alkaline environment and a co- or terpolymer of acrylic acid and certain substituted acrylamides such as t-butyl acrylamide.

    摘要翻译: 一种用于抑制工业冷却水中腐蚀的组合物和方法,其含有硬度并且pH至少为8,该组合物包含能够在碱性水溶液环境中抑制腐蚀的水溶性有机膦酸酯和丙烯酸的共聚物或三元共聚物 和某些取代的丙烯酰胺如叔丁基丙烯酰胺。

    Zinc stabilization with modified acrylamide based polymers and corrosion
inhibition derived therefrom
    10.
    发明授权
    Zinc stabilization with modified acrylamide based polymers and corrosion inhibition derived therefrom 失效
    具有改性丙烯酰胺基聚合物的锌稳定化及其衍生的腐蚀抑制

    公开(公告)号:US4898686A

    公开(公告)日:1990-02-06

    申请号:US42927

    申请日:1987-04-27

    IPC分类号: C02F5/12 C23F11/08

    摘要: New zinc stabilizing polymers containing at least 5 mole percent of a monomer represented by the structure: ##STR1## wherein: R is independently, at each occurrence, chosen from H and lower (C.sub.1 -C.sub.4) alkyl groups;R' is a hydrocarbonaceous bridging group containing from 1-12 carbon atoms;X is chosen from --SO.sub.3 M, --OH, --COOM groups or mixtures thereof,M is hydrogen or some other cation species; andn ranges from 1-10, are described. Also, the use of these polymers in combination with zinc salts, and in further combination with phosphate salts, to inhibit corrosion of iron containing metals, and other metals, when these metals are exposed to industrial waters is demonstrated. Deposit control or scale inhibition on these metals exposed to industrial waters is also observed.

    摘要翻译: 含有至少5摩尔%的由以下结构表示的单体的新的锌稳定化聚合物:其中:R各自独立地选自H和低级(C 1 -C 4)烷基; R'是含有1-12个碳原子的烃基桥联基团; X选自-SO 3 M,-OH,-COOM基团或其混合物,M是氢或一些其它阳离子物质; 并描述n的范围为1-10。 此外,证明了当这些金属暴露于工业水中时,这些聚合物与锌盐的组合以及与磷酸盐的进一步组合用于抑制含铁金属和其它金属的腐蚀。 也观察到暴露于工业水域的这些金属的沉积物控制或垢垢抑制。