1.
公开(公告)号:US07748598B2
公开(公告)日:2010-07-06
申请号:US11816829
申请日:2005-08-10
Applicant: Donald Joseph Want
Inventor: Donald Joseph Want
IPC: B23K31/02
CPC classification number: B01J3/04 , B01J19/02 , B01J2219/0236 , B23K33/004 , B23K2101/12 , B23K2103/24 , F16B5/08 , Y10T428/12493
Abstract: A method for joining clad metal plates having a protective layer (27), e.g. titanium, and a substrate layer (28), e.g. carbon steel, includes firstly removing margins (29) of protective layer along edges of the clad metal plates to be joined. The substrate layers are then welded together to form an exposed substrate weld (31). Covering material (38) of the same type as the protective layer (27) is then located along the exposed substrate weld (31) to a level substantially flush with an outer surface of the protective layer (27). The substrate layer (28) is heated prior to welding the covering material so that the covering material is pre-stressed when cooled. The method may be used to fabricate reaction vessels having seams that do not stand proud of the remainder of the interior surface of the vessel. The low profile seams are less susceptible to erosion than has been the case in the past so that longer-life vessels can be produced. The invention encompasses vessels such as autoclaves, crucibles and reaction vessels formed of clad plate joined by the method.
Abstract translation: 一种用于接合具有保护层(27)的复合金属板的方法, 钛和基底层(28),例如, 碳钢,首先包括沿着要接合的复合金属板的边缘去除保护层的边缘(29)。 然后将基底层焊接在一起以形成暴露的基底焊缝(31)。 然后将与保护层(27)相同类型的覆盖材料(38)沿着暴露的基底焊缝(31)定位成与保护层(27)的外表面基本齐平的水平。 在焊接覆盖材料之前加热基底层(28),使得覆盖材料在冷却时被预应力。 该方法可用于制造具有接缝的反应容器,该接缝不会容纳容器内表面的其余部分。 低密度接缝比过去的情况不太受侵蚀,因此可以生产更长寿命的船只。 本发明包括诸如高压釜,坩埚和由通过该方法连接的复合板形成的反应容器的容器。
-
2.
公开(公告)号:US20080268279A1
公开(公告)日:2008-10-30
申请号:US11816829
申请日:2005-08-10
Applicant: Donald Joseph Want
Inventor: Donald Joseph Want
CPC classification number: B01J3/04 , B01J19/02 , B01J2219/0236 , B23K33/004 , B23K2101/12 , B23K2103/24 , F16B5/08 , Y10T428/12493
Abstract: A method for joining clad metal plates having a protective layer (27), e.g. titanium, and a substrate layer (28), e.g. carbon steel, includes firstly removing margins (29) of protective layer along edges of the clad metal plates to be joined. The substrate layers are then welded together to form an exposed substrate weld (31). Covering material (38) of the same type as the protective layer (27) is then located along the exposed substrate weld (31) to a level substantially flush with an outer surface of the protective layer (27). The substrate layer (28) is heated prior to welding the covering material so that the covering material is pre-stressed when cooled. The method may be used to fabricate reaction vessels having seams that do not stand proud of the remainder of the interior surface of the vessel. The low profile seams are less susceptible to erosion than has been the case in the past so that longer-life vessels can be produced. The invention encompasses vessels such as autoclaves, crucibles and reaction vessels formed of clad plate joined by the method.
Abstract translation: 一种用于接合具有保护层(27)的复合金属板的方法, 钛和基底层(28),例如, 碳钢,首先包括沿着要接合的复合金属板的边缘去除保护层的边缘(29)。 然后将基底层焊接在一起以形成暴露的基底焊缝(31)。 然后将与保护层(27)相同类型的覆盖材料(38)沿着暴露的基底焊缝(31)定位成与保护层(27)的外表面基本齐平的水平。 在焊接覆盖材料之前加热基底层(28),使得覆盖材料在冷却时被预应力。 该方法可用于制造具有接缝的反应容器,该接缝不会容纳容器内表面的其余部分。 低密度接缝比过去的情况不太受侵蚀,因此可以生产更长寿命的船只。 本发明包括诸如高压釜,坩埚和由通过该方法连接的复合板形成的反应容器的容器。
-