IMPLANTABLE CAPSULE FOR LEADLESS CARDIAC PACING
    1.
    发明申请
    IMPLANTABLE CAPSULE FOR LEADLESS CARDIAC PACING 有权
    用于无铅心脏的可植入胶囊

    公开(公告)号:US20150374976A1

    公开(公告)日:2015-12-31

    申请号:US14744966

    申请日:2015-06-19

    申请人: SORIN CRM SAS

    摘要: The invention relates to an implantable capsule, particularly an autonomous capsule of cardiac stimulation, comprising a tubular body provided at the distal end of an anchoring element with a helical screw adapted to penetrate tissue a wall of an organ of a patient, the body housing a set of functional elements of the capsule. It comprises an annular support integral with the body and coaxial therewith, said support surrounding the base of the anchoring element and comprising a series of openings radially extending. The base of the anchoring element comprises a series of rods or tubes projecting in a generally radial direction, and engaged in said openings to thereby secure the anchoring element to the support.

    摘要翻译: 本发明涉及一种可植入胶囊,特别是心脏刺激的自主胶囊,其包括管状体,其设置在锚定元件的远端处,其具有适于穿透组织的患者的器官的壁上的组织的螺旋螺旋, 胶囊的功能元素集。 其包括与主体一体并与其同轴的环形支撑件,所述支撑件围绕锚固元件的基部并且包括径向延伸的一系列开口。 锚固元件的基部包括沿大致径向方向突出并且接合在所述开口中的一系列杆或管,从而将锚固元件固定到支撑件上。

    Zirconium-coated steel plates and chemical device elements produced with such plates
    3.
    发明授权
    Zirconium-coated steel plates and chemical device elements produced with such plates 失效
    镀锆钢板和用这种板材生产的化学元件元件

    公开(公告)号:US08505806B2

    公开(公告)日:2013-08-13

    申请号:US11817660

    申请日:2006-03-09

    IPC分类号: B23K31/02

    摘要: Method for producing coated assembly parts for chemical device elements including the following series of steps: (a) the formation of an initial assembly including a steel support part, typically a plate, a zirconium or zirconium alloy coating, typically a sheet having dimensions similar to those of the steel plate, and at least one brazing material between the support part and the coating, wherein said brazing material is an alloy including silver and copper; (b) the insertion of the initial assembly into a brazing chamber with a controlled atmosphere; (c) the formation of a controlled atmosphere in said chamber; (d) the reheating of said assembly to a temperature at least equal to the melting temperature of said brazing material; wherein, prior to the formation of said initial assembly, the deposition of a titanium or titanium alloy layer on said zirconium (or zirconium alloy) coating is performed, and in that said coating is placed so that its titanium- or (titanium alloy-) coated surface is in contact with said brazing material.

    摘要翻译: 用于生产用于化学装置元件的涂覆的组装部件的方法,包括以下一系列步骤:(a)形成初始组件,其包括钢支撑部分,通常为板,锆或锆合金涂层,通常为具有与 所述钢板和所述支撑部分和所述涂层之间的至少一个钎料,其中所述钎焊材料是包括银和铜的合金; (b)将初始组件插入具有受控气氛的钎焊室; (c)在所述室中形成受控气氛; (d)将所述组件再加热到至少等于所述钎焊材料的熔化温度的温度; 其中,在形成所述初始组装之前,执行钛或钛合金层在所述锆(或锆合金)涂层上的沉积,并且所述涂层被放置成使其钛 - 或(钛合金) - 涂覆表面与所述钎焊材料接触。

    Manufacturing method of a forged golf club head
    4.
    发明授权
    Manufacturing method of a forged golf club head 有权
    锻造高尔夫球杆头的制造方法

    公开(公告)号:US08434671B1

    公开(公告)日:2013-05-07

    申请号:US13568973

    申请日:2012-08-07

    申请人: Chi-Hung Su

    发明人: Chi-Hung Su

    IPC分类号: B23K31/02 A63B53/04

    摘要: A manufacturing method of a forged golf club head has acts of: providing pre-forged strike element and the pre-forged hosel made with different materials, welding the hosel on a connecting end of the strike element, and press-forging the blank to form a main component of the golf club head. The main component of the golf club head may accomplish the golf club head. Otherwise, a pre-forged secondary component is welded on a back part of the strike face of the main component to accomplish the golf club head. The strike element and the hosel made of different materials are directly secured to each other to precisely form a predetermined, shape so that the following surface treating steps and the manufacturing time are reduced and the quality of the golf club head is enhanced.

    摘要翻译: 锻造高尔夫球杆头的制造方法具有以下动作:提供预锻件冲击元件和由不同材料制成的预锻造插鞘,将插鞘焊接在冲击元件的连接端上,并压制坯料以形成 高尔夫球杆头的主要部件。 高尔夫球杆头的主要部件可以实现高尔夫球杆头。 否则,将预锻造的次要部件焊接在主要部件的冲击面的后部,以实现高尔夫球杆头。 由不同材料制成的冲击元件和插鞘直接固定到彼此以精确地形成预定的形状,从而降低了后续的表面处理步骤和制造时间,提高了高尔夫球杆头的质量。

    Thermal stir welding apparatus
    8.
    发明授权
    Thermal stir welding apparatus 有权
    热搅拌焊接设备

    公开(公告)号:US07980449B2

    公开(公告)日:2011-07-19

    申请号:US10385168

    申请日:2003-02-28

    申请人: R. Jeffrey Ding

    发明人: R. Jeffrey Ding

    IPC分类号: B23K31/02

    摘要: A welding method and apparatus are provided for forming a weld joint between first and second elements of a workpiece. The method includes heating the first and second elements to form an interface of material in a plasticized or melted state interface between the elements. The interface material is then allowed to cool to a plasticized state if previously in a melted state. The interface material, while in the plasticized state, is then mixed, for example, using a grinding/extruding process, to remove any dendritic-type weld microstructures introduced into the interface material during the heating process.

    摘要翻译: 提供一种用于在工件的第一和第二元件之间形成焊接接头的焊接方法和装置。 该方法包括加热第一和第二元件以在元件之间的塑化或熔融状态界面中形成材料界面。 如果先前处于熔化状态,则允许界面材料冷却至塑化状态。 然后将界面材料在增塑状态下混合,例如使用研磨/挤出方法,以除去在加热过程中引入界面材料中的任何树枝状焊接微结构。

    Method of solid phase welding of metal plates
    9.
    发明授权
    Method of solid phase welding of metal plates 失效
    金属板固相焊接方法

    公开(公告)号:US07654439B2

    公开(公告)日:2010-02-02

    申请号:US12097155

    申请日:2006-12-12

    IPC分类号: B23K31/02

    摘要: In a method of welding of metal plates in a solid phase, wherein the metal plates are combined to form a package, and welded together by heating and deforming the package by contacting with two rotating cylinders, the improvement includes: providing a damping lining between the metal plates; placing the package between two cylinders such that the metal plate with the smallest yield value under welding temperature faces the cylinder with smaller diameter, heating and deforming the package in vacuum, such that during a first stage the temperature reaches 0.4-0.5 of melting temperature of a metal plate with the smallest yield value, during a second stage the package is heated by a high frequency which heats the damping lining up to 0.92-0.95 of its melting temperature, wherein angular velocities of the rotating cylinders and their radiuses are selected in accordance with a formula.

    摘要翻译: 在以固相方式焊接金属板的方法中,其中金属板组合形成封装,并且通过与两个旋转圆筒接触而使封装加热和变形来焊接在一起,改进之处在于:在 金属板; 将包装放置在两个气缸之间,使得在焊接温度下具有最小屈服值的金属板面对具有较小直径的气缸,在真空中加热和变形包装,使得在第一阶段期间温度达到0.4-0.5的熔融温度 具有最小屈服值的金属板,在第二阶段期间,封装被高频加热,其将阻尼衬层加热到其熔化温度的0.92-0.95,其中旋转圆柱体及其半径的角速度根据 用公式。

    ZIRCONIUM-COATED STEEL PLATES AND CHEMICAL DEVICE ELEMENTS PRODUCED WITH SUCH PLATES
    10.
    发明申请
    ZIRCONIUM-COATED STEEL PLATES AND CHEMICAL DEVICE ELEMENTS PRODUCED WITH SUCH PLATES 失效
    锆涂层钢板和化学设备元素与这些板材生产

    公开(公告)号:US20090136778A1

    公开(公告)日:2009-05-28

    申请号:US11817660

    申请日:2006-03-09

    摘要: Method for producing coated assembly parts for chemical device elements including the following series of steps: (a) the formation of an initial assembly including a steel support part, typically a plate, a zirconium or zirconium alloy coating, typically a sheet having dimensions similar to those of the steel plate, and at least one brazing material between the support part and the coating, wherein said brazing material is an alloy including silver and copper; (b) the insertion of the initial assembly into a brazing chamber with a controlled atmosphere; (c) the formation of a controlled atmosphere in said chamber; (d) the reheating of said assembly to a temperature at least equal to the melting temperature of said brazing material; wherein, prior to the formation of said initial assembly, the deposition of a titanium or titanium alloy layer on said zirconium (or zirconium alloy) coating is performed, and in that said coating is placed so that its titanium- or (titanium alloy-) coated surface is in contact with said brazing material.

    摘要翻译: 用于生产用于化学装置元件的涂覆的组装部件的方法,包括以下一系列步骤:(a)形成初始组件,其包括钢支撑部分,通常为板,锆或锆合金涂层,通常为具有与 所述钢板和所述支撑部分和所述涂层之间的至少一个钎料,其中所述钎焊材料是包括银和铜的合金; (b)将初始组件插入具有受控气氛的钎焊室; (c)在所述室中形成受控气氛; (d)将所述组件再加热到至少等于所述钎焊材料的熔化温度的温度; 其中,在形成所述初始组装之前,执行钛或钛合金层在所述锆(或锆合金)涂层上的沉积,并且所述涂层被放置成使其钛 - 或(钛合金) - 涂覆表面与所述钎焊材料接触。