摘要:
The present invention relates to a method of prepairing a heat-resistant polyamide by carrying out condensation polymerisation with a monomer mixture including a diester compound and a diamine compound. The present invention provides an economical method of prepairing a heat-resistant polyamide in that a monomer, a raw material, is simply and chiefly prepared, and the polymerizing reaction time is short because it does not need solvent separately.
摘要:
The present invention relates to a method of prepairing a heat-resistant polyamide by carrying out condensation polymerization with a monomer mixture including a diester compound and a diamine compound. The present invention provides an economical method of prepairing a heat-resistant polyamide in that a monomer, a raw material, is simply and chiefly prepared, and the polymerizing reaction time is short because it does not need solvent separately.
摘要:
A polyester/polycarbonate blend having superior thermal stability and superior color stability is disclosed. The polyester/polycarbonate blend comprises: (a) P(ET-CT) (poly(ethylene terephthalate-co-1,4-cyclohexylene dimethylene terephthalate) which is copolymerized with 1,4-cyclohexanedimethanol (CHDM) of 40 to 90 mol % with respect to total diol components; (b) polyethylene terephthalate (PET); (c) polycarbonate (PC); and (d) germanium of 1 to 100 ppm (weight ratio) with respect to total polyester/polycarbonate blend, wherein with respect to total polyester/polycarbonate blend, the amount of the P(ET-CT) and PET is 50 to 90 weight %, the amount of the PET is 1 to 6 times in weight ratio with respect to the P(ET-CT), and the amount of the PC is 10 to 50 weight %.
摘要:
A polyester/polycarbonate blend having superior transparency and heat resistance which is useful for producing transparent polyester articles is disclosed. The blend of polyester and polycarbonate includes (a) polyethyleneterephthalate (PET) prepared with terephthalic acid component and ethylene glycol component, or copolymerized polyethyleneterephthalate prepared with terephthalic acid component and ethylene glycol component, and further copolymerized with 1 to 10 mol % of isophthalic acid, cyclohexane dimethanol (CHDM), di-ethylene glycol and/or alkylene glycol of 3 to 6 carbon atoms component with respect to acid or diol components; (b) polycarbonate (PC); and (c) CHDM modified PET prepared with 20 to 80 mol % CHDM with respect to diol components, wherein the amount of the PC is 10 to 60 wt % with respect to the mixture of (a) PET and (b) PC, and the amount of the (c) CHDM modified PET is 0.2 to 2.5 times by weight with respect to the amount of (b) PC.