摘要: A cement clinker which necessitates no considerable change in the main chemical components and mineral components of cement, is free from preheater coating problems and adverse influences on cement properties, and is effective in reducing the heat quantity required for burning; and a process for producing the cement clinker. In the process for cement clinker production a substance having a melting point higher than the temperature of a liquid phase of the cement clinker and serving as crystal nuclei for C3S is incorporated include a fine powder of refractory brick, particles of an ordinary Portland cement clinker, a fine powder of a high-early-strength Portland cement clinker, a high-early-strength Portland cement, and a fine powder of quicklime. Due to this, alite generation is accelerated even at a low temperature. As a result, high-quality clinker can be produced through burning using a small unit heat quantity and no decrease in cement quality results. The process contributes to a reduction in preheater coating amount and prolongation of the life of the refractory bricks.
摘要翻译: 不需要水泥熟料的主要化学成分和矿物成分的水泥熟料,没有预热器涂层问题和对水泥性能的不利影响,有效降低燃烧所需的热量; 以及生产水泥熟料的方法。 在水泥熟料生产过程中,掺入熔点高于水泥熟料液相温度并用作C3S晶体的物质包括耐火砖细粉,普通硅酸盐水泥熟料颗粒, 高强度硅酸盐水泥熟料,高强度硅酸盐水泥和生石灰细粉的细粉。 由于这一点,即使在低温也促进了发生。 因此,通过使用小单位热量的燃烧可以生产高品质的熟料,并且不会降低水泥质量。 该方法有助于预热器涂层量的减少和耐火砖寿命的延长。
-
公开(公告)号:US20080190328A1
公开(公告)日:2008-08-14
申请号:US11720519
申请日:2005-12-02
IPC分类号: C04B2/10
摘要: A cement clinker which necessitates no considerable change in the main chemical components and mineral components of cement, is free from preheater coating problems and adverse influences on cement properties, and is effective in reducing the heat quantity required for burning; and a process for producing the cement clinker. In the process for cement clinker production a substance having a melting point higher than the temperature of a liquid phase of the cement clinker and serving as crystal nuclei for C3S is incorporated include a fine powder of refractory brick, particles of an ordinary Portland cement clinker, a fine powder of a high-early-strength Portland cement clinker, a high-early-strength Portland cement, and a fine powder of quicklime. Due to this, alite generation is accelerated even at a low temperature. As a result, high-quality clinker can be produced through burning using a small unit heat quantity and no decrease in cement quality results. The process contributes to a reduction in preheater coating amount and prolongation of the life of the refractory bricks.
摘要翻译: 不需要水泥熟料的主要化学成分和矿物成分的水泥熟料,没有预热器涂层问题和对水泥性能的不利影响,有效降低燃烧所需的热量; 以及生产水泥熟料的方法。 在水泥熟料生产过程中,掺入熔点高于水泥熟料的液相温度并作为C 3 S的晶核的物质包括耐火砖细粉 普通硅酸盐水泥熟料颗粒,高强度硅酸盐水泥熟料粉末,高强度硅酸盐水泥和生石灰细粉。 由于这一点,即使在低温也促进了发生。 因此,通过使用小单位热量的燃烧可以生产高品质的熟料,并且不会降低水泥质量。 该方法有助于预热器涂层量的减少和耐火砖寿命的延长。
-
公开(公告)号:US20150246849A1
公开(公告)日:2015-09-03
申请号:US14367494
申请日:2012-12-20
申请人: Makio Yamashita , Hisanobu Tanaka , Yukio Tanaka , Katsuhiko Ichihara , Kazuo Sakamoto , Kazuo Tabata
发明人: Makio Yamashita , Hisanobu Tanaka , Yukio Tanaka , Katsuhiko Ichihara , Kazuo Sakamoto , Kazuo Tabata
IPC分类号: C04B7/44
CPC分类号: C04B7/4446 , C04B7/425 , G01N23/20 , G01N23/223 , G01N33/38 , G01N2223/076 , Y02P40/121 , C04B7/361
摘要: The cement clinker production system includes: a first supplying section configured to supply a sulfur source and a fluorine source of mineralizer; a second supplying device configured to supply clinker raw material; a crusher configured to crush the mixed raw material obtained by mixing the clinker raw material with the fluorine source of the mineralizer; a kiln configured to burn the crushed mixed raw material; an introducing section configured to introduce the sulfur source of the mineralizer to the kiln; a third supplying section configured to supply fuel to the kiln; and a test sample-analyzing system configured to collect each of the mixed raw material before the burning and the clinker after the burning and to measure amounts of the fluorine, main components and free lime depending on the type collected.
摘要翻译: 所述水泥熟料生产系统包括:第一供应部分,其构造成供应硫源和矿化剂的氟源; 第二供给装置,其构造成供给熟料原料; 破碎机,其将通过将熟料原料与矿化剂的氟源混合而得到的混合原料粉碎; 窑炉,其被配置为燃烧被混合的原料; 导入部,其构造为将所述矿化剂的硫源引入所述窑内; 第三供给部,其构造成向所述窑内供给燃料; 以及被配置为在燃烧之后收集混合原料和燃烧后的熟料的测试样品分析系统,并根据收集的类型测量氟,主要成分和游离石灰的量。
-
公开(公告)号:US20130000524A1
公开(公告)日:2013-01-03
申请号:US13582761
申请日:2011-03-11
摘要: This burned cement clinker is a burned cement clinker including at least one selected from the group consisting of fluorine, sulfur, chlorine and bromine, and at least one metallic element(s) selected from the group consisting of elements in groups 3 through 12 of the periodic table. Preferably, the amount of fluorine is within a range from 300 to 750 mg/kg, the amount of sulfur (expressed in terms of SO3) is within a range from 1.5 to 3.0% by mass, the amount of at least one chlorine equivalent(s) selected from the group consisting of chlorine and bromine is within a range from 150 to 350 mg/kg, and the amount of at least one metallic element selected from the group consisting of elements in groups 3 through 12 of the periodic table is within a range from 0.2 to 0.8% by mass.
摘要翻译: 这种烧结的水泥熟料是包括选自由氟,硫,氯和溴组成的组中的至少一种的至少一种烧结的水泥熟料,以及至少一种金属元素,其选自第 周期表。 优选氟的量在300〜750mg / kg的范围内,硫的量(以SO 3表示)在1.5〜3.0质量%的范围内,至少1当量的氯当量( s)选自氯和溴的范围在150至350mg / kg的范围内,并且至少一种选自元素周期表第3至12族的元素的金属元素的量在 的范围为0.2〜0.8质量%。
-
公开(公告)号:US09650294B2
公开(公告)日:2017-05-16
申请号:US13582761
申请日:2011-03-11
摘要: This burned cement clinker is a burned cement clinker including at least one selected from the group consisting of fluorine, sulfur, chlorine and bromine, and at least one metallic element(s) selected from the group consisting of elements in groups 3 through 12 of the periodic table. Preferably, the amount of fluorine is within a range from 300 to 750 mg/kg, the amount of sulfur (expressed in terms of SO3) is within a range from 1.5 to 3.0% by mass, the amount of at least one chlorine equivalent(s) selected from the group consisting of chlorine and bromine is within a range from 150 to 350 mg/kg, and the amount of at least one metallic element selected from the group consisting of elements in groups 3 through 12 of the periodic table is within a range from 0.2 to 0.8% by mass.
-
-
-
-