Abstract:
The present disclosure provides methods for producing an olefin polymer by contacting a C3-C40 olefin, ethylene and a diene with a catalyst system including an activator and a metallocene catalyst compound comprising a substituted or unsubstituted indacenyl group and obtaining a C3-C40 olefin-ethylene-diene terpolymer typically comprising from 1 to 35 mol % of ethylene, from 98.9 to 65 mol % C3-C40 olefin, and, optionally, from 0.1 to 10 mol % diene. Preferably, a propylene-ethylene-ethylidene norbornene is obtained.
Abstract:
A blended multimodal polymer product is disclosed that comprises a first polymer, wherein the first polymer is a homopolymer of propylene or a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer; and a second polymer, wherein the second polymer is a propylene homopolymer and a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer, and wherein the first polymer and second polymer have a difference in heat of fusion of about 25 J/g or more. Methods for making such a polymer product using at least two reactors in parallel and for separating a propylene-based polymer from a solvent using a liquid-phase separator are also disclosed.
Abstract:
The present disclosure provides methods for producing an olefin polymer by contacting a C3-C40 olefin, ethylene and a diene with a catalyst system including an activator and a metallocene catalyst compound comprising a substituted or unsubstituted indacenyl group and obtaining a C3-C40 olefin-ethylene-diene terpolymer typically comprising from 30 to 55 mol % ethylene, from 69.09 to 45 mol % C3 to C40 comonomer, and from 0.01 to 7 mol % diene wherein the Tg of the terpolymer is −28° C. or less. Preferably, a propylene-ethylene-ethylidene norbornene is obtained.
Abstract:
The present disclosure provides methods for producing an olefin polymer by contacting a C3-C40 olefin, ethylene and a diene with a catalyst system including an activator and a metallocene catalyst compound comprising a substituted or unsubstituted indacenyl group and obtaining a C3-C40 olefin-ethylene-diene terpolymer typically comprising from 30 to 55 mol % ethylene, from 69.09 to 45 mol % C3 to C40 comonomer, and from 0.01 to 7 mol % diene wherein the Tg of the terpolymer is −28° C. or less. Preferably, a propylene-ethylene-ethylidene norbornene is obtained.
Abstract:
Branched ethylene-propylene-diene elastomers (bEPDM) and processes for making the bEPDM's comprising combining a catalyst precursor and an activator at a temperature within a range from 90° C. to 160° C. with ethylene, a C3 to C12 α-olefin, a non-conjugated diene, and a dual-polymerizable diene, where the catalyst precursor is a metallocene catalyst precursor, preferably according to one of various structures including any two ligands selected from cyclopentadienyl ligands and ligands isolobal to the cyclopentadienyl group.
Abstract:
The invention relates to purification of plasticizer, particularly for use in a polymer production process and plant. More particularly, the invention relates to purification of plasticizer, such as by gas stripping, for use in a process for in-line blending of polymer and plasticizer.
Abstract:
A blended multimodal polymer product is disclosed that comprises a first polymer, wherein the first polymer is a homopolymer of propylene or a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer; and a second polymer, wherein the second polymer is a propylene homopolymer and a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer, and wherein the first polymer and second polymer have a difference in heat of fusion of about 25 J/g or more. Methods for making such a polymer product using at least two reactors in parallel and for separating a propylene-based polymer from a solvent using a liquid-phase separator are also disclosed.
Abstract:
A blended multimodal polymer product is disclosed that comprises a first polymer, wherein the first polymer is a homopolymer of propylene or a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer; and a second polymer, wherein the second polymer is a propylene homopolymer and a propylene copolymer having an ethylene or a C4 to C10 olefin comonomer, and wherein the first polymer and second polymer have a difference in heat of fusion of about 25 J/g or more. Methods for making such a polymer product using at least two reactors in parallel and for separating a propylene-based polymer from a solvent using a liquid-phase separator are also disclosed.
Abstract:
A method for making a polymer, having the steps of (a) polymerizing one or more monomers in the presence of a solvent and a catalyst to form a reaction product; (b) removing an effluent from the reaction product, where the effluent comprises an active catalyst and one or more unreacted monomers; (c) combining a quench, comprising carbon dioxide, with the effluent to form a quenched polymer stream, having a carboxyl metal complex; and (d) recovering a polymer from the quenched polymer stream.
Abstract:
A method for making a polymer, having the steps of (a) polymerizing one or more monomers in the presence of a solvent and a catalyst to form a reaction product; (b) removing an effluent from the reaction product, where the effluent comprises an active catalyst and one or more unreacted monomers; (c) combining a quench, comprising carbon dioxide, with the effluent to form a quenched polymer stream, having a carboxyl metal complex; and (d) recovering a polymer from the quenched polymer stream.