Abstract:
Various embodiments provide a process roasting a metal bearing material under oxidizing conditions to produce an oxidized metal bearing material, roasting the oxidized metal bearing material under reducing conditions to produce a roasted metal bearing material, and leaching the roasted metal bearing material in a basic medium to yield a pregnant leach solution.
Abstract:
The present disclosure provides a method of recovering copper, molybdenum, and a precious metal value from a metal-bearing material, the method comprising bulk flotation of the metal-bearing material to form a flotation product, wherein the metal-bearing material comprises a copper compound, a molybdenum compound, at least one precious metal value, and a silicate, pressure oxidizing the flotation product to form a pressure oxidized discharge, separating the pressure oxidized discharge to form a separated liquid and separated solid, extracting molybdenum, via a molybdenum solution extraction, from the separated liquid to form a molybdenum-containing stream and a copper-containing stream, extracting copper, via a copper solution extraction, from the copper-containing stream, and extracting the precious metal value, via a cyanide leaching process, from the separated solid.
Abstract:
Systems and methods for basic leaching are provided. In various embodiments, a method is provided comprising leaching a slurry comprising a copper bearing material and an ammonia leach medium, adding copper powder to the slurry, separating the slurry into a pregnant leach solution and solids, and performing a solvent extraction on the pregnant leach solution to produce an loaded aqueous stream.
Abstract:
Various embodiments provide a process roasting a metal bearing material under oxidizing conditions to produce an oxidized metal bearing material, roasting the oxidized metal bearing material under reducing conditions to produce a roasted metal bearing material, and leaching the roasted metal bearing material in a basic medium to yield a pregnant leach solution.