公开(公告)号:US20220064346A1
公开(公告)日:2022-03-03
申请号:US17149739
申请日:2021-01-15
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoshifumi IIDA , Takashi HASEGAWA , Satomi KASHIWAGI , Takako KOBAYASHI , Satoshi INOUE
IPC: C08F212/08 , C08L25/14 , C08L33/08 , C09D125/14 , C09D133/08 , B41L43/02 , B41M5/50 , B41M5/00
Abstract: Pressure-responsive particles include pressure-responsive base particles and fatty acid metal salt particles, in which the pressure-responsive base particles contain a styrene-based resin which contains styrene and other vinyl monomers as polymerization components and a (meth)acrylic acid ester-based resin which contains at least two kinds of (meth)acrylic acid esters as polymerization components and in which amass ratio of the (meth)acrylic acid esters to all polymerization components is 90% by mass or higher, the pressure-responsive particles have at least two glass transition temperatures, and a difference between the lowest glass transition temperature and the highest glass transition temperature is 30° C. or higher.
-
公开(公告)号:US20240326505A1
公开(公告)日:2024-10-03
申请号:US18424853
申请日:2024-01-28
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Shiori CHONAN , Takashi HASEGAWA
CPC classification number: B42C9/0081 , B42D5/003
Abstract: A perfect-bound booklet includes a sheet set that is a stack of multiple sheets and multiple adhesive layers provided at an end of each sheet in the sheet set and interposed between the sheets and peelably bonding the sheets together, the multiple adhesive layers containing a thermoplastic adhesive agent, and the amount of the thermoplastic adhesive agent in the multiple adhesive layers changes from each of a first surface side and a second surface side of the booklet toward the middle of the booklet in the thickness direction.
-
公开(公告)号:US20220229377A1
公开(公告)日:2022-07-21
申请号:US17500917
申请日:2021-10-13
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Takako KOBAYASHI , Yoshifumi IIDA , Takashi HASEGAWA
Abstract: Pressure-responsive particles include pressure-responsive base particles and resin particles, in which the pressure-responsive base particles contain a styrene-based resin that contains styrene and other vinyl monomers as polymerization components and a (meth)acrylic acid ester-based resin that contains at least two kinds of (meth)acrylic acid esters as polymerization components, a ratio of a mass of the (meth)acrylic acid esters to a total mass of polymerization components is 90% by mass or more in the (meth)acrylic acid ester-based resin, the pressure-responsive particles have at least two glass transition temperatures, a difference between a lowest glass transition temperature and a highest glass transition temperature is 30° C. or higher, and a ratio of a mass of the resin particles to a total mass of the pressure-responsive particles is 0.05% by mass or more and 2.0% by mass or less.
-
公开(公告)号:US20220227906A1
公开(公告)日:2022-07-21
申请号:US17547164
申请日:2021-12-09
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoshifumi IIDA , Takako KOBAYASHI , Takashi HASEGAWA , Kiyohiro YAMANAKA , Takeshi IWANAGA , Satoshi KAMIWAKI , Mieko SEKI , Sumiaki YAMASAKI
IPC: C08F212/08 , C08K3/36 , C09D11/107 , C09D125/14
Abstract: Pressure-responsive particles include pressure-responsive base particles and silica particles, in which the pressure-responsive base particles contain a styrene-based resin that contains styrene and other vinyl monomers as polymerization components and a (meth)acrylic acid ester-based resin that contains at least two kinds of (meth)acrylic acid esters as polymerization components and in which a ratio of a mass of the (meth)acrylic acid esters to a total mass of polymerization components is 90% by mass or more, the pressure-responsive particles have at least two glass transition temperatures, a difference between a lowest glass transition temperature and a highest glass transition temperature is 30° C. or higher, and a ratio of a surface coating rate Cs2 by the silica particles after application of the following first stress to a surface coating rate Cs1 by the silica particles before application of stress satisfies a relationship of 0.4≤Cs2/Cs1≤0.8, first stress: 10 g of the pressure-responsive particles and 90 g of resin-coated ferrite particles are put in a V-shaped mixer with a rotary container having a volume of 0.5 L and rotated at a rotation speed of 40 rpm for 20 minutes at a temperature of 20° C. and a relative humidity of 50%.
-
公开(公告)号:US20220064425A1
公开(公告)日:2022-03-03
申请号:US17161702
申请日:2021-01-29
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Satomi KASHIWAGI , Satoshi INOUE , Sumiaki YAMASAKI , Yoshifumi IIDA , Takako KOBAYASHI , Takashi HASEGAWA
Abstract: Pressure-responsive particles include pressure-responsive base particles and inorganic oxide particles, in which the pressure-responsive base particles contain a styrene-based resin which contains styrene and other vinyl monomers as polymerization components and a (meth)acrylic acid ester-based resin which contains at least two kinds of (meth)acrylic acid esters as polymerization components and in which amass ratio of the (meth)acrylic acid esters to all polymerization components is 90% by mass or higher, a liberation rate of the inorganic oxide particles is 10% by mass or higher and 40% by mass or lower, the pressure-responsive particles have at least two glass transition temperatures, and a difference between a lowest glass transition temperature and a highest glass transition temperature is 30° C. or higher.
-
公开(公告)号:US20210294228A1
公开(公告)日:2021-09-23
申请号:US16984161
申请日:2020-08-04
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoichiro EMURA , Satoshi KAMIWAKI , Yoshifumi IIDA , Sumiaki YAMASAKI , Takashi HASEGAWA , Hiroshi SAEGUSA , Hajime SUGAHARA , Sachiko NISHIOKA
IPC: G03G9/087 , C08F212/08 , G03G15/08
Abstract: A method for producing a printed material includes providing pressure-induced phase transition particles on a recording medium having an arithmetic average roughness Ra of 0.07 μm or more and 3.80 μm or less to form a pressure-induced phase transition particle layer having a coverage C within a range of 30% to 90%; bonding the pressure-induced phase transition particles onto the recording medium; and folding the recording medium having the pressure-induced phase transition particles bonded thereon and pressure-bonding the folded recording medium, or pressure-bonding the recording medium having the pressure-induced phase transition particles bonded thereon and another recording medium placed on top of each other. The pressure-induced phase transition particles contain a styrene resin containing styrene and a vinyl monomer other than styrene as polymerization components, and a (meth)acrylic acid ester resin that contains at least two(meth)acrylic acid esters as polymerization components, and a mass ratio of the (meth)acrylic acid esters relative to a total of polymerization components of the (meth)acrylic acid ester resin is 90 mass % or more. The pressure-induced phase transition particles have at least two glass transition temperatures, and the difference between the lowest glass transition temperature and the highest glass transition temperature among the glass transition temperatures exhibited by the pressure-induced phase transition particles is 30° C. or more.
-
公开(公告)号:US20220308486A1
公开(公告)日:2022-09-29
申请号:US17643941
申请日:2021-12-13
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoshifumi IIDA , Takashi HASEGAWA , Satoshi KAMIWAKI , Takako KOBAYASHI , Satoshi INOUE , Sumiaki YAMASAKI , Mieko SEKI , Kiyohiro YAMANAKA , Takeshi IWANAGA
Abstract: A particle set for producing a printed matter includes: a chromatic color toner containing toner particles A; and pressure-responsive particles containing base particles B, in which the base particles B contain a styrene resin containing, as polymerization components, styrene and a vinyl monomer other than styrene, and a (meth)acrylate resin containing, as a polymerization component, a (meth)acrylate, a mass ratio of the styrene resin to the (meth)acrylate resin (styrene resin:(meth)acrylate resin) is 80:20 to 20:80, a difference between the lowest glass transition temperature and the highest glass transition temperature of the pressure-responsive particles is 30° C. or more, and when the toner particles A have a volume average particle diameter D50A and the base particles B have a volume average particle diameter D50B, the D50A and the D50B satisfy formula 1-1: 1.5 μm
-
公开(公告)号:US20220064424A1
公开(公告)日:2022-03-03
申请号:US17157959
申请日:2021-01-25
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoshifumi IIDA , Takashi HASEGAWA , Satomi KASHIWAGI , Takako KOBAYASHI , Satoshi INOUE
IPC: C08L25/14 , C08K3/36 , C08K3/22 , C08L33/10 , C09J125/14 , C09J133/10 , B42D15/02
Abstract: Pressure-responsive particles include pressure-responsive base particles and first inorganic oxide particles, in which the pressure-responsive base particles contain a styrene-based resin which contains styrene and other vinyl monomers as polymerization components and a (meth)acrylic acid ester-based resin which contains at least two kinds of (meth)acrylic acid esters as polymerization components and in which a mass ratio of the (meth)acrylic acid esters to all polymerization components is 90% by mass or higher, Db/Da which is a ratio of a number average particle diameter Db of the first inorganic oxide particles to a number average particle diameter Da of the pressure-responsive base particles is 0.05 or higher and 0.25 or lower, the pressure-responsive particles have at least two glass transition temperatures, and a difference between a lowest glass transition temperature and a highest glass transition temperature is 30° C. or higher.
-
9.
公开(公告)号:US20210277291A1
公开(公告)日:2021-09-09
申请号:US17003947
申请日:2020-08-26
Applicant: FUJIFILM Business Innovation Corp.
Inventor: Yoshifumi IIDA , Sachiko NISHIOKA , Takashi HASEGAWA , Hajime SUGAHARA , Satomi KASHIWAGI , Yuka ZENITANI , Satoshi INOUE
IPC: C09J125/06 , C09J133/10 , B41M7/00 , C09J133/02
Abstract: A pressure sensitive adhesive particle includes a pressure sensitive adhesive base particle that contains a styrene resin containing styrene and a vinyl monomer other than styrene as polymerization components, and a (meth)acrylate resin containing at least two (meth)acrylates as polymerization components, in which a mass ratio of the (meth)acrylates relative to a total of polymerization components of the (meth)acrylate resin is 90 mass % or more; and an external additive. The pressure sensitive adhesive particle has a surface having an arithmetic average roughness Ra within a range of 0.005 μm to 0.100 μm. The pressure sensitive adhesive particle has at least two glass transition temperatures, and the difference between the lowest glass transition temperature and the highest glass transition temperature among the glass transition temperatures of the pressure sensitive adhesive particle is 30° C. or more.
-
-
-
-
-
-
-
-