Abstract:
There is provided a cellulose acylate film, containing a hindered amin-based compound, wherein the hindered amine-based compound is contained in an amount of 0.001% by mass to 5% by mass based on cellulose acylate, a minimum value of Knoop hardness is 170 N/mm2 to 220 N/mm2, and the Knoop hardness is measured several times by a Knoop indenter, the Knoop indenter is rotated by a given angle in each measurement, and a rotation axis of the Knoop indenter is orthogonal to an upper surface of the cellulose acylate film.
Abstract translation:提供了含有受阻胺基化合物的纤维素酰化物膜,其中受阻胺类化合物的含量相对于纤维素酰化物为0.001质量%至5质量%,诺普硬度的最小值为 170N / mm 2至220N / mm 2,并且通过Knoop压头测量Knoop硬度,在每次测量中将Knoop压头旋转给定角度,并且Knoop压头的旋转轴线正交于上表面 的纤维素酰化物膜。
Abstract:
An object of the present invention is to provide a film having a plated-layer precursor layer which is capable of forming a metal layer having excellent roll-to-roll productivity and excellent adhesiveness to a substrate. Another object of the present invention is to provide a film having a patterned plated layer as well as an electroconductive film and a touch panel using the same.The film having a plated-layer precursor layer of the present invention is a film having a plated-layer precursor layer including a substrate, and an undercoat and a plated-layer precursor layer disposed on the substrate in this order from the substrate side, in which the undercoat has a hardness on the surface thereof of 10 N/mm2 or less and a friction coefficient with release paper of 5 or less.
Abstract:
A cellulose ester film contains a compound having a structural unit denoted by —NR—(C═O)— in which R represents a hydrogen atom or a substituent, a surface having knoop hardness of greater than or equal to 210 N/mm2 is provided, and loss tangent tan δ at 25° C. is greater than or equal to 0.03.