TRANSPARENT COLORLESS GLASS OR GLASS-CERAMIC PANEL HAVING AN OPTICALLY DENSE COLORED COATING AND METHOD OF MAKING SAME
    3.
    发明申请
    TRANSPARENT COLORLESS GLASS OR GLASS-CERAMIC PANEL HAVING AN OPTICALLY DENSE COLORED COATING AND METHOD OF MAKING SAME 审中-公开
    透明无色玻璃或具有光学透明涂料的玻璃陶瓷面板及其制造方法

    公开(公告)号:US20080199622A1

    公开(公告)日:2008-08-21

    申请号:US12026262

    申请日:2008-02-05

    IPC分类号: B05D3/02

    摘要: A transparent, colorless glass or glass-ceramic panel has a visually dense, high-temperature-stable coating having an organic/inorganic network structure containing filling material particles and a color-imparting pigment. The mechanically stable, visually dense coating has no melt-reaction zone at the surface of the panel, which is coated with the coating, so that it does not impair the panel strength. The inorganic network structure can be made from a SiO2-based sol. The coating is made by introducing the color-imparting pigment and the filling material particles into a reactive organic/inorganic network structure; applying the resulting organic/inorganic network structure containing the pigment and the filling material particles to the panel to coat the panel and then burning-in the organic/inorganic network structure with the pigment and the filling material particles under thermal conditions to form the coating with no melt-reaction zone.

    摘要翻译: 透明无色的玻璃或玻璃陶瓷面板具有视觉密实的高温稳定涂层,其具有含有填充材料颗粒和赋颜色颜料的有机/无机网状结构。 机械稳定的,目视密实的涂层在面板的表面没有熔融反应区,涂覆有涂层,从而不会损害面板强度。 无机网状结构可以由SiO 2基的溶胶制成。 通过将着色颜料和填充材料颗粒引入反应性有机/无机网络结构中来制备涂层; 将所得的含有颜料和填充材料颗粒的有机/无机网络结构施加到面板上以涂覆面板,然后在有机/无机网状结构中用颜料和填充材料颗粒在热条件下燃烧以形成具有 无熔融反应区。

    Transparent colorless glass or glass-ceramic panel having an optically dense colored coating and method of making same
    4.
    发明授权
    Transparent colorless glass or glass-ceramic panel having an optically dense colored coating and method of making same 有权
    透明无色玻璃或具有光致密着色涂层的玻璃陶瓷面板及其制造方法

    公开(公告)号:US07361405B2

    公开(公告)日:2008-04-22

    申请号:US10993741

    申请日:2004-11-19

    IPC分类号: B32B17/06

    摘要: A transparent, colorless glass or glass-ceramic panel has a visually dense, high-temperature-stable coating having an organic/inorganic network structure containing filling material particles and a color-imparting pigment. The mechanically stable, visually dense coating has no melt-reaction zone at the surface of the panel, which is coated with the coating, so that it does not impair the panel strength. The inorganic network structure can be made from a SiO2-based sol. The coating is made by introducing the color-imparting pigment and the filling material particles into a reactive organic/inorganic network structure; applying the resulting organic/inorganic network structure containing the pigment and the filling material particles to the panel to coat the panel and then burning-in the organic/inorganic network structure with the pigment and the filling material particles under thermal conditions to form the coating with no melt-reaction zone.

    摘要翻译: 透明无色的玻璃或玻璃陶瓷面板具有视觉密实的高温稳定涂层,其具有含有填充材料颗粒和赋颜色颜料的有机/无机网状结构。 机械稳定的,目视密实的涂层在面板的表面没有熔融反应区,涂覆有涂层,从而不会损害面板强度。 无机网状结构可以由SiO 2基的溶胶制成。 通过将着色颜料和填充材料颗粒引入反应性有机/无机网络结构中来制备涂层; 将所得的含有颜料和填充材料颗粒的有机/无机网络结构施加到面板上以涂覆面板,然后在有机/无机网络结构中用颜料和填充材料颗粒在热条件下燃烧以形成涂层 无熔融反应区。

    Transparent colorless glass or glass-ceramic panel having an optically dense colored coating and method of making same
    5.
    发明申请
    Transparent colorless glass or glass-ceramic panel having an optically dense colored coating and method of making same 有权
    透明无色玻璃或具有光致密着色涂层的玻璃陶瓷面板及其制造方法

    公开(公告)号:US20050129959A1

    公开(公告)日:2005-06-16

    申请号:US10993741

    申请日:2004-11-19

    摘要: A transparent, colorless glass or glass-ceramic panel has a visually dense, high-temperature-stable coating having an organic/inorganic network structure containing filling material particles and a color-imparting pigment. The mechanically stable, visually dense coating has no melt-reaction zone at the surface of the panel, which is coated with the coating, so that it does not impair the panel strength. The inorganic network structure can be made from a SiO2-based sol. The coating is made by introducing the color-imparting pigment and the filling material particles into a reactive organic/inorganic network structure; applying the resulting organic/inorganic network structure containing the pigment and the filling material particles to the panel to coat the panel and then burning-in the organic/inorganic network structure with the pigment and the filling material particles under thermal conditions to form the coating with no melt-reaction zone.

    摘要翻译: 透明无色的玻璃或玻璃陶瓷面板具有视觉密实的高温稳定涂层,其具有含有填充材料颗粒和赋颜色颜料的有机/无机网状结构。 机械稳定的,目视密实的涂层在面板的表面没有熔融反应区,涂覆有涂层,从而不会损害面板强度。 无机网状结构可以由SiO 2基的溶胶制成。 通过将着色颜料和填充材料颗粒引入反应性有机/无机网络结构中来制备涂层; 将所得的含有颜料和填充材料颗粒的有机/无机网络结构施加到面板上以涂覆面板,然后在有机/无机网状结构中用颜料和填充材料颗粒在热条件下燃烧以形成具有 无熔融反应区。

    Transparent Glass Ceramic Plate That Has An Opaque, Colored Bottom Coating Over The Entire Surface Or Over Part Of The Surface
    6.
    发明申请
    Transparent Glass Ceramic Plate That Has An Opaque, Colored Bottom Coating Over The Entire Surface Or Over Part Of The Surface 有权
    透明玻璃陶瓷板,在整个表面或表面的一部分具有不透明的彩色底涂层

    公开(公告)号:US20100130342A1

    公开(公告)日:2010-05-27

    申请号:US12540881

    申请日:2009-08-13

    IPC分类号: C03C10/12

    摘要: A transparent, colorless lithium-aluminosilicate glass ceramic plate with high-quartz mixed crystals as the prevailing crystal phase, which is provided on one side with an opaque, colored, temperature-stable coating over the entire surface or over the entire surface to a large extent, is described, which has a content of Nd2O3 of 40 to 4000 ppm, a Yellowness Index of less than 10% with a 4 mm glass (ceramic) layer thickness, and a variegation of colors of the glass or the glass ceramic in the CIELAB color system of C* of less than 5. The glass ceramic plate preferably has a composition (in % by weight based on oxide) of: Li2O 3.0-4.5, Na2O 0-1.5, K2O 0-1.5, ΣNa2O+K2O 0.2-2.0, MgO 0-2.0, CaO 0-1.5, SrO 0-1.5, BaO 0-2.5, ZnO 0-2.5, B2O3 0-1.0, Al2O3 19-25, SiO2 55-69, TiO2 1-3, ZrO2 1-2.5, SnO2 0-0.4, ΣSnO2+TiO2

    摘要翻译: 一种透明,无色的铝硅铝酸盐玻璃陶瓷板,其具有高石英混晶作为主要晶相,其一面在整个表面或整个表面上设置为不透明,着色,温度稳定的涂层至大面积 描述了其具有40至4000ppm的Nd2O3含量,具有4mm玻璃(陶瓷)层厚度的小于10%的黄度指数,以及玻璃或玻璃陶瓷的颜色的变化 C *的CIELAB色系小于5.玻璃陶瓷板的组成(以氧化物重量计)为:Li2O 3.0-4.5,Na2O 0-1.5,K2O 0-1.5,Na2O + K2O 0.2-2.0,MgO 0-2.0,CaO 0-1.5,SrO 0-1.5,BaO 0-2.5,ZnO 0-2.5,B 2 O 3 0-1.0,Al 2 O 3 19-25,SiO 2 55-69,TiO 2 1-3,ZrO 2 1-2.5,SnO2 0-0.4,&lt; SnO2 + TiO2 <3,P2O5 0-3.0,Nd2O3 0.01-0.4,CoO 0.0-0.004

    Transparent glass ceramic plate that has an opaque, colored bottom coating over the entire surface or over part of the surface
    7.
    发明授权
    Transparent glass ceramic plate that has an opaque, colored bottom coating over the entire surface or over part of the surface 有权
    透明玻璃陶瓷板,在整个表面或表面的整个表面上具有不透明的彩色底涂层

    公开(公告)号:US07981823B2

    公开(公告)日:2011-07-19

    申请号:US12540881

    申请日:2009-08-13

    摘要: A transparent, colorless lithium-aluminosilicate glass ceramic plate with high-quartz mixed crystals as the prevailing crystal phase, which is provided on one side with an opaque, colored, temperature-stable coating over the entire surface or over the entire surface to a large extent, is described, which has a content of Nd2O3 of 40 to 4000 ppm, a Yellowness Index of less than 10% with a 4 mm glass (ceramic) layer thickness, and a variegation of colors of the glass or the glass ceramic in the CIELAB color system of C* of less than 5. The glass ceramic plate preferably has a composition (in % by weight based on oxide) of: Li2O 3.0-4.5, Na2O 0-1.5, K2O 0-1.5, ΣNa2O+K2O 0.2-2.0, MgO 0-2.0, CaO 0-1.5, SrO 0-1.5, BaO 0-2.5, ZnO 0-2.5, B2O3 0-1.0, Al2O3 19-25, SiO2 55-69, TiO2 1-3, ZrO2 1-2.5, SnO2 0-0.4, ΣSnO2+TiO2

    摘要翻译: 一种透明,无色的铝硅铝酸盐玻璃陶瓷板,其具有高石英混晶作为主要晶相,其一面在整个表面或整个表面上设置为不透明,着色,温度稳定的涂层至大面积 描述了其具有40至4000ppm的Nd2O3含量,具有4mm玻璃(陶瓷)层厚度的小于10%的黄度指数,以及玻璃或玻璃陶瓷的颜色的变化 C *的CIELAB色系小于5.玻璃陶瓷板的组成(以氧化物重量计)为:Li2O 3.0-4.5,Na2O 0-1.5,K2O 0-1.5,Na2O + K2O 0.2-2.0,MgO 0-2.0,CaO 0-1.5,SrO 0-1.5,BaO 0-2.5,ZnO 0-2.5,B 2 O 3 0-1.0,Al 2 O 3 19-25,SiO 2 55-69,TiO 2 1-3,ZrO 2 1-2.5,SnO2 0-0.4,&lt; SnO2 + TiO2 <3,P2O5 0-3.0,Nd2O3 0.01-0.4,CoO 0.0-0.004。

    TRANSPARENT GLASS CERAMIC PLATE THAT HAS AN OPAQUE, COLORED BOTTOM COATING OVER THE ENTIRE SURFACE OR OVER PART OF THE SURFACE
    8.
    发明申请
    TRANSPARENT GLASS CERAMIC PLATE THAT HAS AN OPAQUE, COLORED BOTTOM COATING OVER THE ENTIRE SURFACE OR OVER PART OF THE SURFACE 审中-公开
    透明玻璃陶瓷板,在整个表面或表面的一部分上具有优质,有色底漆

    公开(公告)号:US20070232476A1

    公开(公告)日:2007-10-04

    申请号:US11688099

    申请日:2007-03-19

    IPC分类号: C03C10/14 C03C10/12

    摘要: A transparent, colorless lithium-aluminosilicate glass ceramic plate with high-quartz mixed crystals as the prevailing crystal phase, which is provided on one side with an opaque, colored, temperature-stable coating over the entire surface or over the entire surface to a large extent, is described, which has a content of Nd2O3 of 40 to 4000 ppm, a Yellowness Index of less than 10% with a 4 mm glass (ceramic) layer thickness, and a variegation of colors of the glass or the glass ceramic in the CIELAB color system of C* of less than 5. The glass ceramic plate preferably has a composition (in % by weight based on oxide) of: Li2O 3.0-4.5, Na2O 0-1.5, K2O 0-1.5, ΣNa2O+K2O 0.2-2.0, MgO 0-2.0, CaO 0-1.5, SrO 0-1.5, BaO 0-2.5, ZnO 0-2.5, B2O3 0-1.0, Al2O3 19-25, SiO2 55-69, TiO2 1-3, ZrO2 1-2.5, SnO2 0-0.4, ΣSnO2+TiO2

    摘要翻译: 一种透明,无色的铝硅铝酸盐玻璃陶瓷板,其具有高石英混晶作为主要晶相,其一面在整个表面或整个表面上设置为不透明,着色,温度稳定的涂层至大面积 描述了其具有40至4000ppm的Nd 2 O 3 3含量,使用4mm玻璃(陶瓷)的黄度指数小于10%的范围, 层厚度以及C *小于5的CIELAB色系中的玻璃或玻璃陶瓷的颜色的变化。玻璃陶瓷板优选具有以下成分(以氧化物计的重量%):Li 2 O 3.0-4.5,Na 2 O 0-1.5,K 2 O 0-1.5,SigmaNa 2 O + K 2 O 0.2-2.0,MgO 0-2.0,CaO 0-1.5,SrO 0-1.5,BaO 0-2.5,ZnO 0-2.5,B 2 O, 0> 3 0-1.0,Al 2 O 3 19-25,SiO 2 55-69,TiO 2, 2 1-3,ZrO 2 1-2.5,SnO 2 0-0.4,SigmaSnO 2, + TiO 2 <3,P O 0-3.0,Nd 2 O 3, /SUB>0.01-0.4,CoO 0.0-0.004