摘要:
Method of welding tailored blanks consisting of a material mostly containing steel and a proportion greater than 0.015% aluminium by weight, using at least one laser beam, in which at least one weld joint of the full-penetration type is made using a gas mixture consisting of 30% to 80% nitrogen by volume, the rest being helium (up to 100%) in order to assist the said laser beam. The method of the invention is particularly recommended for welding motor vehicle elements, especially bodywork, doors, bonnets or the like.
摘要:
Binary gas mixture for welding using a laser beam of up to 12 kW, consisting of 30% to 60% nitrogen by volume, the remainder (up to 100%) being helium. Application of this gas mixture to the welding of steel, stainless steel or titanium.
摘要:
Binary gas mixture for welding using a laser beam of up to 12 kW, consisting of 30% to 60% nitrogen by volume, the remainder (up to 100%) being helium. Application of this gas mixture to the welding of steel, stainless steel or titanium.
摘要:
Process for welding together the two longitudinal edges of a sheet of austenitic, ferritic or martensitic stainless steel so as to obtain a welded pipe, employing at least one laser beam having a power ranging up to 12 kW, and in which a gas mixture is used that consists of 30% to 80% nitrogen by volume and of helium for the remainder (up to 100%). The stainless steel sheet has a thickness of 0.5 to 4 mm and the pipe obtained has a diameter of 5 mm to 50 cm. The welding is full-penetration welding.
摘要:
Binary gas mixture for welding using a laser beam of up to 8 kW, consisting of 60% to 80% nitrogen by volume, the remainder (up to 100%) being helium. Application of this gas mixture to the welding of steel, stainless steel or titanium.
摘要:
A method and an apparatus for welding with a laser beam. A shielding gas mixture of nitrogen and helium is used and the proportions of the component gases are modified depending on the laser beam's power or power density. Plasma formation in the shield gas is minimized by increasing the proportion of helium as the laser beam's power or power density increases.
摘要:
A method and an apparatus for welding with a laser beam. A shielding gas mixture of nitrogen and helium is used and the proportions of the component gases are modified depending on the laser beam's power or power density. Plasma formation in the shield gas is minimized by increasing the proportion of helium as the laser beam's power or power density increases.
摘要:
The invention relates to a laser beam welding method and installation that makes use of a protective gas mixture containing argon and helium. The proportion of argon and/or helium in said gas mixture is chosen or adjusted according to the power or the power density of the laser beam. The laser power is included between 0.5 kW and 30 kW and, preferably, between 5 kW and 20 kW. The protective gas mixture comprises argon and/or helium and, preferably, the gas mixture contains a volume proportion of helium of between 30% and 80%, the remainder being argon and, possibly, inevitable impurities.
摘要:
The invention relates to a laser cutting method for cutting a C-Mn steel workpiece, characterized in that laser beam generation means comprising at least one silica fiber with an ytterbium-doped core is used to generate the laser beam. Preferably, the ytterbium-based fiber has a wavelength between 1.07 and 1.1 μm, preferably 1.07 μm, the quality factor of the laser beam is between 0.33 and 8 mm.mrad, and the laser beam has a power of between 0.1 and 25 kW. The assistance gas for the laser beam is chosen from nitrogen, helium, argon, oxygen, CO2 and mixtures thereof, and, optionally, it further contains one or more additional compounds chosen from H2 and CH4.
摘要:
The invention relates to a laser cutting method for cutting a stainless steel workpiece using laser beam generation means comprising a silica fibre with an ytterbium-doped core to generate the laser beam. Preferably, the laser beam generated by the ytterbium-based fibre has a wavelength between 1.07 and 1.09 μm, a quality factor of the laser beam is between 0.33 and 8 mm.mrad, and the laser beam has a power of between 0.1 and 25 kW. The assistance gas for the laser beam is chosen from nitrogen, helium, argon and mixtures thereof, and, optionally, it further contains one or more additional compounds chosen from O2, CO2, H2 and CH4.
摘要翻译:本发明涉及一种使用激光束产生装置切割不锈钢工件的激光切割方法,该装置包括具有镱掺杂芯的二氧化硅纤维以产生激光束。 优选地,由镱基光纤产生的激光束具有1.07和1.09μm之间的波长,激光束的质量因子在0.33和8mm.mrad之间,并且激光束具有在0.1和25kW之间的功率 。 用于激光束的辅助气体选自氮气,氦气,氩气及其混合物,并且任选地,其还含有一种或多种选自O 2,CO 2, H 2,H 2和CH 4。