公开(公告)号:US20230087017A1
公开(公告)日:2023-03-23
申请号:US17480085
申请日:2021-09-20
Applicant: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Inventor: Xingcheng XIAO , Mei CAI , Wei ZENG , Aijie CHEN
IPC: H01M10/658 , H01M50/293
Abstract: A thermal barrier component for an electrochemical cell (e.g., a battery) includes a mat, a functional material, and a polymer binder. The mat includes a porous matrix. The functional material is in pores of the porous matrix. The functional material includes an oxide. In certain aspects, the functional material may be a composite material. The polymer binder is in contact with the porous matrix and the functional material. At least one of the porous matrix, the functional material, and the polymer binder is configured to serve as an intumescent carbon source. The oxide is configured to catalyze thermal degradation of the intumescent carbon source to form intumescent carbon at a first temperature. The first temperature is greater than or equal to about 300° C. The thermal barrier component is configured to mitigate thermal runaway in an electrochemical cell. The thermal barrier component may include one or more layers.
-
公开(公告)号:US20230246241A1
公开(公告)日:2023-08-03
申请号:US17579144
申请日:2022-01-19
Applicant: GM GLOBAL TECHNOLOGY OPERATIONS LLC
Inventor: Jung Hwi CHO , Aijie CHEN , Xingcheng XIAO , Mei CAI
IPC: H01M10/058 , H01M10/0525 , H01M4/134 , H01M4/04
CPC classification number: H01M10/058 , H01M4/134 , H01M4/0445 , H01M10/0525 , H01M2004/027 , H01M2300/0068
Abstract: A method for forming a solid-state battery includes preparing a cell, heating the cell to a first temperature, and cycling the cell while maintaining the cell at the first temperature and/or while the cell is cooled to room temperature from the first temperature. The cell includes a solid-state electrolyte adjacent to a negative electrode, including a negative electroactive material selected from the group consisting of: lithium metal, lithium alloys, silicon, silicon alloys, and combinations thereof. The first temperature is between about 50° C. and about 175° C. The cell is cycled for between about 1 cycle and about 10 cycles, where current densities are between about 0.01 mA/cm2 and about 10 mA/cm2, and capacity per cycle between about 0.01 mAh/cm2 and about 1 mAh/cm2.
-