1.
公开(公告)号:US20180268971A1
公开(公告)日:2018-09-20
申请号:US15868063
申请日:2018-01-11
Applicant: GRIREM ADVANCED MATERIALS CO., LTD.
Inventor: Guiyong Wu , Yang Luo , Hongwei Li , Yuanfei Yang , Dunbo Yu , Ningtao Quan , Chao Yuan , Wenlong Yan
IPC: H01F1/059 , H01F41/02 , C22C38/00 , C22C38/14 , C22C38/04 , C22C38/06 , C22C38/02 , C22C38/10 , C22C38/12 , C22C38/28
Abstract: Provided are a highly thermostable rare-earth permanent magnetic material, a preparation method thereof and a magnet containing the same. A composition of the rare-earth permanent magnetic material by an atomic percentage is as follows: SMxRaFe100-x-y-z-aMyNz, wherein R is at least one of Zr and Hf, M is at least one of Co, Ti, Nb, Cr, V, Mo, Si, Ga, Ni, Mn and Al, x+a is 7-10%, a is 0-1.5%, y is 0-5% and z is 10-14%.
-
公开(公告)号:US11101057B2
公开(公告)日:2021-08-24
申请号:US15868063
申请日:2018-01-11
Applicant: GRIREM ADVANCED MATERIALS CO., LTD.
Inventor: Guiyong Wu , Yang Luo , Hongwei Li , Yuanfei Yang , Dunbo Yu , Ningtao Quan , Chao Yuan , Wenlong Yan
IPC: C22C38/00 , H01F1/059 , C23C8/24 , H01F1/08 , C22C38/02 , C22C38/04 , C22C38/06 , C22C38/10 , C22C38/12 , C22C38/14 , C22C38/28 , C23C8/26 , H01F41/02 , C22C33/02 , B22F9/04 , B22F9/08 , B22F3/02 , B22F5/00 , B22F1/00
Abstract: Provided are a highly thermostable rare-earth permanent magnetic material, a preparation method thereof and a magnet containing the same. A composition of the rare-earth permanent magnetic material by an atomic percentage is as follows: SmxRaFe100-x-y-z-aMyNz, wherein R is at least one of Zr and Hf, M is at least one of Co, Ti, Nb, Cr, V, Mo, Si, Ga, Ni, Mn and Al, x+a is 7-10%, a is 0-1.5%, y is 0-5% and z is 10-14%.
-
公开(公告)号:US11505852B2
公开(公告)日:2022-11-22
申请号:US16791088
申请日:2020-02-14
Applicant: GRIREM ADVANCED MATERIALS CO., LTD.
Inventor: Yang Luo , Xiao Lin , Guiyong Wu , Jiajun Xie , Zilong Wang , Wenlong Yan , Zhongkai Wang , Dunbo Yu
Abstract: The present disclosure discloses an yttrium (Y)-added rare-earth permanent magnetic material and a preparation method thereof. A chemical formula of the material expressed in atomic percentage is (YxRE1-x)aFebalMbNc, wherein 0.05≤x≤0.4, 7≤a≤13, 0≤b≤3, 5≤c≤20, and the balance is Fe, namely, bal=100-a-b-c; RE represents a rare-earth element Sm, or a combination of the rare-earth element Sm and any one or more elements of Zr, Nd and Pr; M represents Co and/or Nb; and N represents nitrogen. In the preparation method, the rare-earth element Y is utilized to replace the element Sm of a samarium-iron-nitrogen material. By regulating a ratio of the element Sm to the element Y, viscosity of an alloy liquid can be reduced, and an amorphous forming ability of the material is enhanced.
-
-