LEAD ACID STORAGE BATTERY
    1.
    发明申请

    公开(公告)号:US20180205072A1

    公开(公告)日:2018-07-19

    申请号:US15744534

    申请日:2016-05-24

    IPC分类号: H01M4/14 H01M10/06 H01M4/73

    摘要: A lead acid storage battery including: positive electrode plates each including a positive electrode grid and a positive electrode active material, and negative electrode plates each including a negative electrode grid and a negative electrode active material. The positive and negative electrode plates are stacked alternately with a separator therebetween to form an electrode plate group. The battery further includes: a battery container having cell chambers each containing the electrode plate group and electrolyte, and a cover sealing an opening of the battery container. The positive electrode active material has a pore distribution having a peak in region A from 0.03 μm to 0.1 μm and a peak in region B from 0.2 μm to 1.0 μm, and a ratio AM/BM of peak AM in region A to peak BM in region B is 0.34 or more and 0.70 or less. The negative electrode grid contains bismuth in an amount of 1 ppm or more and 300 ppm or less.

    LEAD STORAGE BATTERY
    2.
    发明申请

    公开(公告)号:US20190006660A1

    公开(公告)日:2019-01-03

    申请号:US15748965

    申请日:2016-07-21

    摘要: Disclosed is a lead-acid battery including: a battery container; an electrolyte and an electrode plate group in the battery container; and a battery container cover that hermetically seals an opening of the battery container, wherein the electrode plate group includes a positive electrode plate including a positive electrode active material, a negative electrode plate including a negative electrode active material, and a separator interposed between the positive electrode plate and the negative electrode plate, the battery container cover is provided with a liquid port, a liquid port plug that closes the liquid port, and a sleeve that hangs down from the liquid port to a prescribed liquid surface height of the electrolyte, a sodium ion concentration contained in the electrolyte is 1 mmol/L to 90 mmol/L, and a specific surface area of the positive electrode active material is 5 m2/g to 9 m2/g.