摘要:
The present invention is a process for producing a polyester-polycarbonate type thermoplastic polyester elastomer in which a hard segment consisting of a polyester constructed of aromatic dicarboxylic acid, and an aliphatic or alicyclic diol, and a soft segment consisting mainly of aliphatic polycarbonate are connected, comprising at least a step of increasing the molecular weight of an aliphatic polycarbonate diol by a reaction of an aliphatic polycarbonate diol and a chain extender, and a step of reacting aliphatic polycarbonate and a polyester constructed of aromatic dicarboxylic acid and an aliphatic or alicyclic diol in the molten state.
摘要:
The present invention provides a thermoplastic polyester elastomer excellent in heat resistance, heat-aging resistance, water resistance, light resistance, low-temperature property and the like, and further excellent in block order-retaining ability, the thermoplastic polyester elastomer comprising a hard segment which comprises polyester constituted with aromatic dicarboxylic acid and aliphatic or alicyclic diol and a soft segment which comprises mainly aliphatic polycarbonate, wherein the hard segment and the soft segment being connected, and wherein when melting points of the thermoplastic polyester elastomer are obtained by measuring on a differential scanning calorimeter in three cycles in which a temperature is raised from room temperature to 300° C. at a heating rate of 20° C./min., maintained at 300° C. for 3 minutes and lowered to room temperature at a cooling rate of 100° C./min., a melting point difference (Tm1−Tm3) between a melting point obtained in the first cycle (Tm1) and a melting point obtained in the third cycle (Tm3) is 0-50° C., and a tensile strength at break is 15-100 MPa.
摘要:
The present invention provides a thermoplastic polyester elastomer excellent in heat resistance, heat-aging resistance, water resistance, light resistance, low-temperature property and the like, and further excellent in block order-retaining ability, the thermoplastic polyester elastomer comprising a hard segment which comprises polyester constituted with aromatic dicarboxylic acid and aliphatic or alicyclic diol and a soft segment which comprises mainly aliphatic polycarbonate, wherein the hard segment and the soft segment being connected, and wherein when melting points of the thermoplastic polyester elastomer are obtained by measuring on a differential scanning calorimeter in three cycles in which a temperature is raised from room temperature to 300° C. at a heating rate of 20° C./min., maintained at 300° C. for 3 minutes and lowered to room temperature at a cooling rate of 100° C./min., a melting point difference (Tm1−Tm3) between a melting point obtained in the first cycle (Tm1) and a melting point obtained in the third cycle (Tm3) is 0-50° C., and a tensile strength at break is 15-100 MPa.
摘要:
The present invention is a process for producing a polyester-polycarbonate type thermoplastic polyester elastomer in which a hard segment consisting of a polyester constructed of aromatic dicarboxylic acid, and an aliphatic or alicyclic diol, and a soft segment consisting mainly of aliphatic polycarbonate are connected, comprising at least a step of increasing the molecular weight of an aliphatic polycarbonate diol by a reaction of an aliphatic polycarbonate diol and a chain extender, and a step of reacting aliphatic polycarbonate and a polyester constructed of aromatic dicarboxylic acid and an aliphatic or alicyclic diol in the molten state.
摘要:
Provided is an air permeation resistant film in which flexibility can be imparted to the film without remarkably increasing the proportion of a rubber constituting a dispersed phase. An air permeation resistant film comprising (A) a thermoplastic polyester elastomer which comprises a block copolymer containing a polyester as a hard segment and has a melting point of from 180 to 230° C., and (B) a rubber, in a mass ratio (A)/(B) of from 90/10 to 40/60, wherein the component (A) and the component (B) are melt-kneaded to perform dynamic crosslink, thereby forming a continuous phase composed of the component (A) and a dispersed phase composed of the component (B), and the film has an air permeation coefficient at 80° C. of 5×1013 fm2/Pa·s or less and Young's modulus of 120 MPa or less.
摘要:
Provided is an air permeation resistant film in which flexibility can be imparted to the film without remarkably increasing the proportion of a rubber constituting a dispersed phase. An air permeation resistant film comprising (A) a thermoplastic polyester elastomer which comprises a block copolymer containing a polyester as a hard segment and has a melting point of from 180 to 230° C., and (B) a rubber, in a mass ratio (A)/(B) of from 90/10 to 40/60, wherein the component (A) and the component (B) are melt-kneaded to perform dynamic crosslink, thereby forming a continuous phase composed of the component (A) and a dispersed phase composed of the component (B), and the film has an air permeation coefficient at 80° C. of 5×1013 fm2/Pa·s or less and Young's modulus of 120 MPa or less.
摘要翻译:提供了一种防透气膜,其中可赋予膜的柔软性,而不显着增加构成分散相的橡胶的比例。 一种防透气膜,其包含(A)热塑性聚酯弹性体,其包含含有作为硬链段的聚酯的熔点为180-230℃的嵌段共聚物,和(B)以质量比计的橡胶 (A)/(B)为90/10〜40/60,其中将组分(A)和组分(B)熔融捏合以进行动态交联,从而形成由组分(A)组成的连续相, 和由组分(B)组成的分散相,并且该膜的80℃的透气系数为5×10 13 fm 2 / Pa·s以下,杨氏模量为120MPa以下。