BONDED FLUX AND SOLID WIRE FOR SUBMERGED ARC WELDING, AND METHOD FOR SUBMERGED ARC WELDING OF STEEL FOR LOW TEMPERATURE SERVICE
    1.
    发明申请
    BONDED FLUX AND SOLID WIRE FOR SUBMERGED ARC WELDING, AND METHOD FOR SUBMERGED ARC WELDING OF STEEL FOR LOW TEMPERATURE SERVICE 审中-公开
    用于焊接电弧焊的焊接焊丝和固体焊丝,以及用于低温焊接的钢的电弧焊接方法

    公开(公告)号:US20120193327A1

    公开(公告)日:2012-08-02

    申请号:US13360967

    申请日:2012-01-30

    IPC分类号: B23K9/18

    摘要: Disclosed is a bonded flux and a solid wire for submerged arc welding, and a method for submerged arc welding of a low-temperature steel each of which gives a weld bead (weld metal) having excellent low-temperature fracture toughness with satisfactory weldability. The bonded flux includes 23-43% of MgO, 11-31% of Al2O3, 6-16% of CaF2, 7-20% of SiO2, 1.0-8.0% as CO2 equivalent of a metal carbonate, a total of 2-16% of CaO and/or BaO, 0.4-1.5% of metallic silicon, a total of 1.0-7.0% as titanium equivalent of metallic titanium and titanium oxide, a total of 0.01-0.20% as boron equivalent of metallic boron and/or boron oxide, and a total of 1.0-6.0% as equivalents of respective elements of at least one oxide of Na, K, and Li, and has a ratio ([Total Ti]+[Total B])/[SiO2] of from 0.05 to 0.55.

    摘要翻译: 本发明公开了一种用于埋弧焊的粘结焊剂和实心焊丝,以及低温钢的埋弧焊接方法,其中具有优异的低温断裂韧性和良好的焊接性的焊缝(焊接金属)。 粘结焊剂包括23-43%的MgO,11-31%的Al2O3,6-16%的CaF2,7-20%的SiO2,1.0-8.0%的二氧化碳当量的金属碳酸盐,总共2-16 %的CaO和/或BaO,0.4-1.5%的金属硅,总计为1.0-7.0%的钛当量的金属钛和氧化钛,总共为0.01-0.20%的硼当量的金属硼和/或硼 氧化物,并且总共为1.0-6.0%的Na,K和Li的至少一种氧化物的各元素的当量,并且比率([Total Ti] + [Total B])/ [SiO 2]为0.05 至0.55。