Process for producing carbide-containing alloy
    1.
    发明授权
    Process for producing carbide-containing alloy 失效
    生产含碳化合物的方法

    公开(公告)号:US3556780A

    公开(公告)日:1971-01-19

    申请号:US3556780D

    申请日:1966-01-03

    Applicant: IIT RES INST

    CPC classification number: C22C33/0257 C22C38/36 Y10S75/95 Y10S75/956

    Abstract: FULLY DENSE IRON-BASE ALLOYS CHARACTERIZED BY HAVING A MICROSTRUCTURE EXHIBITING A SUBSTANTIALLY UNIFORMLY DISPERSED CARBIDE PHASE OF PARTICLES SIZE PREDOMINANTLY LESS THAN 3 MICRONS ARE PRODUCED FROM PREALLOYED POWDERS BY RAPIDLY QUENCHING AN ATOMIZED ALLOY CHARGE AND SUBJECTING THE SOLIDIFIED PARTICLES TO THE STEP OF HOT CONSOLIDATION IN AN ENVIRONMENT PROTECTED AGAINST ADMISSION OF OXYGEN TO PRODUCE METAL STOCK DIRECTLY FROM PREALLOYED POWDER BY PLASTIC DEFORMATION.

    High speed tool alloys and process
    3.
    发明授权
    High speed tool alloys and process 失效
    高速工具合金和工艺

    公开(公告)号:US3655365A

    公开(公告)日:1972-04-11

    申请号:US3655365D

    申请日:1970-05-01

    Applicant: IIT RES INST

    CPC classification number: C22C29/06 C22C19/07 C22C27/04 C22C32/0052 C22C38/12

    Abstract: Compositions suitable for tool use and containing from about 10 to about 40% of a material selected from the group consisting of tungsten and molybdenum and mixtures thereof; from about 0.5 to about 4% carbon; at least one reactive metal selected from the group consisting of chromium, vanadium, niobium, tantalum, silicon and manganese; the balance a mixture of iron and cobalt. The alloy is formed by the hot consolidation of pre-alloyed powders and results in an alloy having a uniformly dispersed carbide phase of a grain size less than 3 microns.

    Abstract translation: 适用于工具使用并含有约10至约40%的选自钨和钼的材料及其混合物的组合物; 约0.5至约4%的碳; 选自铬,钒,铌,钽,硅和锰中的至少一种活性金属; 平衡铁和钴的混合物。 该合金通过预合金粉末的热固化而形成,并产生具有小于3微米的粒度的均匀分散的碳化物相的合金。