THERMOPLASTIC MOLDING COMPOUNDS WITH OPTIMIZED FLOWABILITY-TOUGHNESS RATIO
    1.
    发明申请
    THERMOPLASTIC MOLDING COMPOUNDS WITH OPTIMIZED FLOWABILITY-TOUGHNESS RATIO 审中-公开
    具有优化流动性 - 热膨胀率的热塑性模塑料

    公开(公告)号:US20160340504A1

    公开(公告)日:2016-11-24

    申请号:US15114615

    申请日:2015-01-27

    Abstract: The invention relates to a thermoplastic composition containing the components A and B and optionally the additional components C and D, the sum of which equals 100 wt. %. The molding compound consists of: a) 60 to 75 wt. % of one or more styrene copolymers A, b) 25 to 40 wt. % of one or more graft copolymers B, c) 0 to 15 wt. % of a rubber C which is different from component B, and d) 0 to 5 wt.% of one or more additives D. The composition contains 0.2 to 3.0 wt. %, based on the total weight of the components A to D, of oligomers, can be readily processed, and leads to scratch-resistant molded parts.

    Abstract translation: 本发明涉及含有组分A和B以及任选的另外的组分C和D的热塑性组合物,其总和等于100wt。 %。 模塑料由以下组成:a)60至75wt。 %的一种或多种苯乙烯共聚物A,b)25〜40wt。 %的一种或多种接枝共聚物B,c)0-15wt。 %的不同于组分B的橡胶C,以及d)0-5重量%的一种或多种添加剂D.组合物含有0.2-3.0重量% 基于低聚物的组分A至D的总重量的%可以容易地加工,并且导致耐划伤的模制部件。

Patent Agency Ranking