Polyolefin thermoplastic silicone elastomers employing radical cure
    2.
    发明授权
    Polyolefin thermoplastic silicone elastomers employing radical cure 有权
    使用自由基固化的聚烯烃热塑性硅橡胶

    公开(公告)号:US06479580B1

    公开(公告)日:2002-11-12

    申请号:US09843906

    申请日:2001-04-30

    IPC分类号: C08L8307

    摘要: Polyolefin thermoplastic elastomers are disclosed which are prepared by; (I) mixing (A) a thermoplastic resin comprising more than 50 percent by volume of a polyolefin resin, said thermoplastic resin having a softening point of 23° C. to 300° C.; (B) a silicone base comprising (B′) 100 parts by weight of a diorganopolysiloxane gum having a plasticity of at least 30 and having an average of at least 2 alkenyl groups per molecule, and optionally, (B″) up to 200 parts by weight of a reinforcing filler, the weight ratio of said silicone base to said polyolefin thermoplastic resin is from 35:65 to 85:15; (C) a radical initiator, present in an amount sufficient to cure said diorganopolysiloxane gum (B′); and (II) dynamically vulcanizing said diorganopolysiloxane gum, wherein at least one property of the thermoplastic elastomer selected from tensile strength or elongation is at least 25% greater than the respective property for a corresponding simple blend wherein said diorganopolysiloxane gum is not cured and said thermoplastic elastomer has an elongation of at least 25%.

    摘要翻译: 公开了通过以下方法制备的聚烯烃热塑性弹性体:(I)混合(A)包含大于50体积%的聚烯烃树脂的热塑性树脂,所述热塑性树脂的软化点为23℃至300℃; (B)包含(B')100重量份塑料性至少为30并且每分子平均具有至少2个烯基的二有机基聚硅氧烷胶,以及任选的(B“)至多200 重量份的增强填料,所述硅氧烷基与所述聚烯烃热塑性树脂的重量比为35:65至85:15;(C)自由基引发剂,其量足以固化所述二有机聚硅氧烷胶(B' ); 和(II)动态硫化所述二有机聚硅氧烷胶,其中选自拉伸强度或伸长率的热塑性弹性体的至少一种性质比相应的简单混合物的相应性能大至少25%,其中所述二有机聚硅氧烷胶不固化,并且所述热塑性 弹性体的伸长率至少为25%。