Method for the reduction of the degree of shrinkage of hydraulic binders
    3.
    发明授权
    Method for the reduction of the degree of shrinkage of hydraulic binders 有权
    降低水硬性粘合剂的收缩程度的方法

    公开(公告)号:US06398866B1

    公开(公告)日:2002-06-04

    申请号:US09493266

    申请日:2000-01-28

    IPC分类号: C04B4000

    摘要: One object of the present invention is an agent for the reduction of the degree of shrinkage in hydraulic binders, whereby said agent comprises an alkanolamine of formula R—NH—(AOH) wherein R is hydrogen or a linear or branched aliphatic or cyclic C1-C6-alkyl group, and A is a C2H4-group or C3H6-group, alone or in combination with hydroxy compounds and/or ethers. Furthermore a method for the reduction of the dry shrinkage of binders such as cement, admixed cement, puzzolanas and thereof produced mortars and concretes by means of such a shrinkage reducing agent is described.

    摘要翻译: 本发明的一个目的是降低水硬性粘合剂的收缩度的试剂,其中所述试剂包括式R-NH-(AOH)的链烷醇胺,其中R是氢或直链或支链的脂族或环状C1- C6烷基,A是C2H4基或C3H6基,单独或与羟基化合物和/或醚组合。 此外,还描述了一种通过这种减缩剂来降低粘结剂如水泥,混合水泥,砌块及其生产的灰浆和混凝土的干收缩率的方法。

    Method for the reduction of the degree of shrinkage of hydraulic binders
    4.
    发明授权
    Method for the reduction of the degree of shrinkage of hydraulic binders 有权
    降低水硬性粘合剂的收缩程度的方法

    公开(公告)号:US06712900B2

    公开(公告)日:2004-03-30

    申请号:US10131075

    申请日:2002-04-25

    IPC分类号: C04B4000

    摘要: On object of the present invention is an agent for the reduction of the degree of shrinkage in hydraulic binders, whereby said comprises an alkanolamine of formula R—NH—(AOH) wherein R is hydrogen or a linear or branched aliphatic or cyclic C1-C6-alkyl group, and A is a C2H4-group or C3H6-group, alone or in combination with hydroxy compounds and/or ethers. Furthermore a method for the reduction of the dry shrinkage of binders such as cement, admixed cement, puzzolanas and thereof produced mortars and concretes by means of such a shrinkage reducing agent is described.

    摘要翻译: 本发明的目的是降低水硬性粘合剂的收缩度的试剂,其中所述的方法包括式R-NH-(AOH)的链烷醇胺,其中R是氢或直链或支链的脂族或环状C 1 -C 6 - 烷基,A是C2H4基或C3H6-基,单独或与羟基化合物和/或醚组合。 此外,还描述了一种通过这种减缩剂来降低粘结剂如水泥,混合水泥,砌块及其生产的灰浆和混凝土的干收缩率的方法。

    Method for rehabilitative and/or protective corrosion-inhibition of reinforcing steel embedded in a hardened structure by means of surface-applied corrosion-inhibiting compositions
    5.
    发明授权
    Method for rehabilitative and/or protective corrosion-inhibition of reinforcing steel embedded in a hardened structure by means of surface-applied corrosion-inhibiting compositions 有权
    通过表面施加的腐蚀抑制组合物对嵌入在硬化结构中的增强钢进行修复和/或保护性腐蚀抑制的方法

    公开(公告)号:US06402990B1

    公开(公告)日:2002-06-11

    申请号:US09309290

    申请日:1999-05-11

    IPC分类号: C23F1100

    摘要: The present invention provides methods and compositions for the reduction of the corrosion rate of already corroding steel reinforcements embedded in a hardened concrete structure as well as for the protective corrosion inhibition of uncorroded steel reinforcements embedded in a hardened concrete structure exposed to aggressive environments. The inventive new compositions employed for the novel method are essentially based on one or more amino- and/or hydroxyalkylamino compound(s), which are partially or completely neutralized with one or more inorganic acid(s) and/or derivatives thereof and/or aliphatic carboxylic- and/or aromatic carboxylic acid(s), one or more surfactant(s) and one or more water-based or water-thinnable water repellent agent(s) selected from the group of organosilicones.

    摘要翻译: 本发明提供了用于降低嵌入在硬化混凝土结构中的已经腐蚀的钢筋的腐蚀速率的方法和组合物,以及用于对暴露于侵蚀性环境的硬化混凝土结构中嵌入的未腐蚀钢筋的保护性腐蚀抑制。 用于该新方法的新组合物基本上基于一种或多种氨基 - 和/或羟烷基氨基化合物,其用一种或多种无机酸和/或其衍生物和/或脂族羧酸部分或完全中和 - 和/或芳族羧酸,一种或多种表面活性剂和一种或多种选自有机硅氧烷的水基或水可稀释的防水剂。

    Method for rehabilitative and/or protective corrosion-inhibition of reinforcing steel embedded in a hardened concrete structure by means of surface-applied corrosion-inhibiting compositions
    6.
    发明授权
    Method for rehabilitative and/or protective corrosion-inhibition of reinforcing steel embedded in a hardened concrete structure by means of surface-applied corrosion-inhibiting compositions 有权
    通过表面施用的腐蚀抑制组合物对嵌入硬化的混凝土结构中的钢筋进行修复和/或保护性腐蚀抑制的方法

    公开(公告)号:US06712995B2

    公开(公告)日:2004-03-30

    申请号:US10135762

    申请日:2002-05-01

    IPC分类号: C23F1100

    摘要: The present invention provides methods and compositions for the reduction of the corrosion rate of already corroding steel reinforcements embedded in a hardened concrete structure as well as for the protective corrosion inhibition of uncorroded steel reinforcements embedded in a hardened concrete structure exposed to aggressive environments. The inventive new compositions employed for the novel method are essentially based on one or more amino- and/or hydroxyalkylamino compound(s), which are partially or completely neutralized with one or more inorganic acid(s) and/or derivatives thereof and/or aliphatic carboxylic- and/or aromatic carboxylic acid(s), one or more surfactant(s) and one or more water-based or water-thinnable water repellent agent(s) selected from the group of organosilicones.

    摘要翻译: 本发明提供了用于降低嵌入在硬化混凝土结构中的已经腐蚀的钢筋的腐蚀速率的方法和组合物,以及用于对暴露于侵蚀性环境的硬化混凝土结构中嵌入的未腐蚀钢筋的保护性腐蚀抑制。 用于该新方法的新组合物基本上基于一种或多种氨基 - 和/或羟烷基氨基化合物,其用一种或多种无机酸和/或其衍生物和/或脂族羧酸部分或完全中和 - 和/或芳族羧酸,一种或多种表面活性剂和一种或多种选自有机硅氧烷的水基或水可稀释的防水剂。