X-RAY IMAGING PHOTOSTIMULABLE PHOSPHOR SCREEN OR PANEL
    1.
    发明申请
    X-RAY IMAGING PHOTOSTIMULABLE PHOSPHOR SCREEN OR PANEL 审中-公开
    X射线成像可光化荧光屏或面板

    公开(公告)号:US20090242836A1

    公开(公告)日:2009-10-01

    申请号:US12327187

    申请日:2008-12-03

    IPC分类号: C09K11/77 C23C16/00

    CPC分类号: G21K4/00 C09K11/7733

    摘要: In a method of preparing a phosphor or scintillator layer to become deposited on a support, a vapor depositing step is applied from a crucible unit by heating as phosphor precursor raw materials present in said crucible, a Cs(X,X′) matrix compound and an activator or dopant precursor compound, wherein said crucible unit comprises at least a bottom and surrounding side walls as a container for phosphor precursor raw materials present in said crucible in liquefied form after heating said crucible, and wherein said Cs(X,X′) matrix compound has a higher vapor pressure than said activator or dopant precursor compound, said method comprising a step of providing said activator or dopant compound in form of a precursor raw material represented by the formula CsxEuyX′(x+αy), wherein x, y and α are integers, wherein x/y is more than 0.25 and wherein α is at least 2, wherein X represents Br and wherein X′ stands for F, Cl, Br, I or a combination thereof; followed by an annealing step after a vapor depositing step, provided that said annealing step proceeds in an ambient atmosphere after cooling said phosphor or scintillator layer, deposited on said support; and wherein as a result a binderless needle-shaped Cs(X,X′):Eu phosphor or scintillator layer becomes provided, having on top of its needle-shaped phosphors, aligned in parallel, an average ratio of divalent to trivalent europium dopant of more than 1:1; wherein said average ratio decreases to an extent of less than 2% per hour, while being exposed to X-rays having an energy in the range from 1 to 100 keV.

    摘要翻译: 在制备荧光体或闪烁体层以沉积在载体上的方法中,通过加热坩埚单元中的荧光体前体原料,Cs(X,X')基质化合物和 活化剂或掺杂剂前体化合物,其中所述坩埚单元至少包括作为用于在加热所述坩埚之后以液化形式存在于所述坩埚中的荧光体前体原料的容器的底部和周围侧壁,并且其中所述Cs(X,X') 基质化合物具有比所述活化剂或掺杂剂前体化合物更高的蒸气压,所述方法包括以由式CsxEuyX'(x + alphay)表示的前体原料的形式提供所述活化剂或掺杂剂化合物的步骤,其中x,y 并且α是整数,其中x / y大于0.25,并且其中α是至少2,其中X表示Br,并且其中X'代表F,Cl,Br,I或它们的组合; 然后在气相沉积步骤之后进行退火步骤,只要所述退火步骤在冷却所述荧光体或闪烁体层之后在环境气氛中进行,沉积在所述载体上; 并且其中结果是提供无粘合剂的针状Cs(X,X'):Eu荧光体或闪烁体层,其在其针状荧光体的顶部平行排列,二价至三价铕掺杂剂的平均比例 超过1:1; 其中所述平均比例降低到小于2%/小时的程度,同时暴露于能量在1至100keV范围内的X射线。

    Method of making a lithographic printing plate
    2.
    发明授权
    Method of making a lithographic printing plate 有权
    制作平版印刷版的方法

    公开(公告)号:US09156529B2

    公开(公告)日:2015-10-13

    申请号:US14342684

    申请日:2012-08-29

    IPC分类号: G03F7/00 B63B27/24 G03F7/30

    摘要: A method of making a lithographic printing plate including the steps of a) image-wise exposing a lithographic printing plate precursor including a light or heat sensitive coating on a support having a hydrophilic surface or which is provided with a hydrophilic layer, and b) processing the precursor consecutively with a first solution and a second solution thereby removing the coating from the support in the non-printing areas. The first and second solutions are provided by a cascade system such that the second solution overflows into the first solution and the first solution overflows into a container to be further treated as waste, and the second solution is regenerated by adding a replenishing solution or a mixture of replenishing solutions at a rate of at least 5 ml/m2 of treated precursor and at most 30 ml/m2 of treated precursor.

    摘要翻译: 一种制备平版印刷版的方法,包括以下步骤:a)将包含光或热敏涂层的平版印刷版原版在具有亲水性表面的支持体上成像曝光,或者设置有亲水层,以及b)处理 该前驱体与第一溶液和第二溶液相连,从而在非印刷区域中从载体上除去涂层。 第一和第二溶液由级联系统提供,使得第二溶液溢出到第一溶液中,并且第一溶液溢出到容器中以进一步作为废物处理,并且通过加入补充溶液或混合物来再生第二溶液 以至少5毫升/平方米的处理前体和至多30毫升/平方米处理的前体的速率补充溶液。

    METHOD OF MAKING A LITHOGRAPHIC PRINTING PLATE
    5.
    发明申请
    METHOD OF MAKING A LITHOGRAPHIC PRINTING PLATE 有权
    制作平版印刷版的方法

    公开(公告)号:US20140272713A1

    公开(公告)日:2014-09-18

    申请号:US14342684

    申请日:2012-08-29

    IPC分类号: G03F7/30

    摘要: A method of making a lithographic printing plate including the steps of a) image-wise exposing a lithographic printing plate precursor including a light or heat sensitive coating on a support having a hydrophilic surface or which is provided with a hydrophilic layer, and b) processing the precursor consecutively with a first solution and a second solution thereby removing the coating from the support in the non-printing areas. The first and second solutions are provided by a cascade system such that the second solution overflows into the first solution and the first solution overflows into a container to be further treated as waste, and the second solution is regenerated by adding a replenishing solution or a mixture of replenishing solutions at a rate of at least 5 ml/m2 of treated precursor and at most 30 ml/m2 of treated precursor.

    摘要翻译: 一种制备平版印刷版的方法,包括以下步骤:a)将包含光或热敏涂层的平版印刷版原版在具有亲水性表面的支持体上成像曝光,或者设置有亲水层,以及b)处理 该前驱体与第一溶液和第二溶液相连,从而在非印刷区域中从载体上除去涂层。 第一和第二溶液由级联系统提供,使得第二溶液溢出到第一溶液中,并且第一溶液溢出到容器中以进一步作为废物处理,并且通过加入补充溶液或混合物来再生第二溶液 以至少5毫升/平方米的处理前体和至多30毫升/平方米处理的前体的速率补充溶液。