    摘要: A method of making a fuser member having a support comprising the steps of: A) providing a support; B) coating from an organic solvent onto the support a coating composition comprising a fluorocarbon thermoplastic random copolymer, a curing agent having a bisphenol residue, a particulate filler containing zinc oxide, an aminosiloxane, and antimony-doped tin oxide particles, the fluorocarbon thermoplastic random copolymer having subunits of: —(CH2CF2)x—, —(CF2CF(CF3)y—, and —(CF2CF2)z—, wherein x is from 1 to 50 or 60 to 80 mole percent, y is from 10 to 90 mole percent, z is from 10 to 90 mole percent, x+y+z equals 100 mole percent; and C) curing the coating composition for 5 to 10 hours at a temperature in the range of 25° C. to 275° C.

    摘要翻译: 一种制造具有支撑件的定影器构件的方法,包括以下步骤:A)提供支撑件; B)从有机溶剂涂布到载体上,涂料组合物包含氟碳热塑性无规共聚物,具有双酚残基的固化剂,含氧化锌的颗粒填料,氨基硅氧烷和锑掺杂的氧化锡颗粒,碳氟化合物热塑性随机 具有亚基的共聚物:<?in-line-formula description =“In-line Formulas”end =“lead”? - (CH 2 2 CF 2)x- , - (CF 2 CF 3(CF 3)y - )和 - (CF 2 CF 2)z - ,<?in-line-formula description =“In-line Formulas”end =“tail”?>其中x为1至50或60至80摩尔%,y为10至90摩尔%,z为 10至90摩尔%,x + y + z等于100摩尔%;和C)在25℃至275℃的温度下将涂料组合物固化5至10小时。

    Fusing belt having polyurethane release layer
    3.
    发明授权
    Fusing belt having polyurethane release layer 失效
    具有聚氨酯脱模层的定影带

    公开(公告)号:US5956555A

    公开(公告)日:1999-09-21

    申请号:US123007

    申请日:1998-07-27

    IPC分类号: G03G15/20

    摘要: A toner fuser belt for use with electrophotographic apparatus including a thermally conductive substrate through which heat is applied; and a toner release layer formed over the substrate; and including an aliphatic cross-linked polyurethane which is stable at fusing temperatures and wherein the aliphatic cross-linked polyurethane is selected to provide good adhesion to the substrate, inorganic material selected to increase toner fuser belt durability and being in an amount 20 to 60 percent by volume of the toner release layer, and a lubricant which reduces surface energy to thereby promote toner release of the toner release layer.

    摘要翻译: 一种用于电子照相设备的调色剂定影带,包括通过其施加热量的导热基底; 以及形成在所述基板上的调色剂释放层; 并且包括在定影温度下稳定的脂族交联聚氨酯,并且其中选择脂族交联聚氨酯以提供对基材的良好粘合性,选择的增加调色剂定影带耐久性的无机材料并且其量为20至60% 的调色剂释放层的体积,以及降低表面能从而促进调色剂释放层的调色剂释放的润滑剂。

    Fuser member with fluorocarbon thermoplastics coating
    4.
    发明授权
    Fuser member with fluorocarbon thermoplastics coating 有权
    定影部件采用碳氟化合物热塑性涂层

    公开(公告)号:US06696158B1

    公开(公告)日:2004-02-24

    申请号:US09608290

    申请日:2000-06-30

    IPC分类号: B32B516

    摘要: A fuser member comprising a support and a layer overlying the support, the layer including a fluorocarbon thermoplastic random copolymer, a curing agent having a bisphenol residue, a particulate filler containing zinc oxide, an aminosiloxane, the cured fluorocarbon thermoplastics random copolymer having subunits of: —(CH2CF2)x—, —(CF2CF(CF3)y—, and —(CF2CF2)z—, wherein: x is from 1 to 40 or 60 to 80 mole percent, z is greater than 40 to no more than 89 mole percent, and y is such that x+y+z equals 100 mole percent.

    摘要翻译: 一种定影器构件,其包括支撑体和覆盖所述载体的层,所述层包括氟碳热塑性无规共聚物,具有双酚残基的固化剂,含有氧化锌的颗粒填料,氨基硅氧烷,所述固化的碳氟化合物热塑性塑料无规共聚物具有以下基团: 其中:x为1至40或60至80摩尔%,z大于40至不大于89摩尔%,而且x + y + z等于100摩尔%。

    Method of preparing thermoplastic random copolymer composition containing zinc oxide and aminosiloxane
    5.
    发明授权
    Method of preparing thermoplastic random copolymer composition containing zinc oxide and aminosiloxane 失效
    制备含有氧化锌和氨基硅氧烷的热塑性无规共聚物组合物的方法

    公开(公告)号:US06444741B1

    公开(公告)日:2002-09-03

    申请号:US09607731

    申请日:2000-06-30

    IPC分类号: C08J328

    摘要: A method of preparing a composition containing a fluorocarbon thermoplastic random copolymer comprising the steps of: (a) providing a mixture having: (i) a fluorocarbon thermoplastic random copolymer having subunits of: —(CH2CF2)x—, —(CF2CF(CF3)y—, and —(CF2CF2)z—,  wherein x is from 1 to 50 or 60 to 80 mole percent, y is from 10 to 90 mole percent. z is from 10 to 90 mole percent. x+y+z equals 100 mole percent; (ii) a filler comprising zinc oxide; (iii) a curable amino functional polydimethyl siloxaie copolymer comprising aminofunctional units selected from tile group consisting of (aminoethylaminopropyl) methyl, ( aminopropyl) methyl and (aminopropyl) dimethyl; and (iv) a bisphenol residue curing agent; and (b) curing the mixture for 3 to 10 hours at a temperature in the range of 220° C. to 280° C. and for an additional 2 to 10 hours at a temperature in the range of 250° C. to 270° C.

    摘要翻译: 一种制备含有氟碳热塑性无规共聚物的组合物的方法,包括以下步骤:(a)提供具有以下物质的混合物:(i)具有亚基的氟碳热塑性无规共聚物,其中x为1至50或60至80摩尔% y为10至90摩尔%,z为10至90摩尔%,x + y + z为100摩尔%;(ii)包含氧化锌的填料;(iii)可固化的氨基官能的聚二甲基硅氧烷共聚物,其包含氨基官能单元 选自由(氨基乙基氨基丙基)甲基,(氨基丙基)甲基和(氨基丙基)二甲基组成的瓦片组; 和(iv)双酚残基固化剂; 和(b)在220℃至280℃的温度下将混合物固化3至10小时,并在250℃至270℃的温度下再固化2至10小时 C。

    Electrostatic charge-suppressing fuser roller
    6.
    发明授权
    Electrostatic charge-suppressing fuser roller 有权
    静电电荷抑制定影辊

    公开(公告)号:US6041210A

    公开(公告)日:2000-03-21

    申请号:US335371

    申请日:1999-06-17

    IPC分类号: G03G15/20

    CPC分类号: G03G15/2057

    摘要: A toner fuser roller with suppressed electrostatic charge build-up for fixing a toner image to a receiver includes a core; and an overcoat layer formed over the core and defining the surface that contacts the receiver, such overcoat layer including electrically conductive powders having a weight percentage between about 30 to 80 weight percent so as to make the overcoat layer electrically conductive and suppress electrostatic charge build-up and improve thermal conductivity.

    摘要翻译: 具有抑制的静电电荷积聚用于将调色剂图像定影到接收器的调色剂定影辊包括芯; 以及形成在所述芯上并且限定与所述接收器接触的表面的外涂层,所述外涂层包括重量百分比在约30至80重量%之间的导电粉末,以使外涂层导电并抑制静电电荷构成, 并提高导热性。

    Fluorocarbon thermoplastic random copolymer composition
    7.
    发明授权
    Fluorocarbon thermoplastic random copolymer composition 有权
    氟碳热塑性无规共聚物组成

    公开(公告)号:US06429249B1

    公开(公告)日:2002-08-06

    申请号:US09609561

    申请日:2000-06-30

    IPC分类号: C08K318

    摘要: A composition comprising a fluorocarbon thermoplastic random copolymer, a curing agent having a bisphenol residue, a particulate filler containing zinc oxide, and an aminosiloxane, the cured fluorocarbon thermoplastic random copolymer having subunits of: —(CH2CF2)x—,—(CF2CF(CF3)y—, and —(CF2CF2)z—, wherein x is from 1 to 50 or 60 to 80 mole percent, y is from 10 to 90 mole percent, z is from 10 to 90 mole percent, x+y+z equals 100 mole percent.

    摘要翻译: 包含氟碳热塑性无规共聚物,具有双酚残基的固化剂,含氧化锌的颗粒填料和氨基硅氧烷的组合物,所述固化的碳氟化合物热塑性无规共聚物具有以下的亚单位:其中x为1至50或60至80摩尔% ,y为10〜90摩尔%,z为10〜90摩尔%,x + y + z为100摩尔%。

    Electrostatic charge-suppressing fluoroplastic fuser roller
    8.
    发明授权
    Electrostatic charge-suppressing fluoroplastic fuser roller 失效
    静电抑制氟塑料定影辊

    公开(公告)号:US06419615B1

    公开(公告)日:2002-07-16

    申请号:US09609563

    申请日:2000-06-30

    IPC分类号: B23P1500

    CPC分类号: G03G15/2057

    摘要: A toner fuser roller with suppressed electrostatic charge build-up for fixing a toner image to a receiver comprising: (a) a core; and (b) an overcoat layer formed over the core and defining a surface that contacts the receiver, the overcoat layer including electrically conductive fine powder in an amount of 10 to 29 weight percent so as to make the overcoat layer electrically conductive and suppress electrostatic charge build-up and improve thermal conductivity.

    摘要翻译: 一种调色剂定影辊,其具有抑制的静电电荷积聚,用于将调色剂图像定影到接收器,包括:(a)芯; 和(b)形成在所述芯上并且限定与所述接收体接触的表面的外涂层,所述外涂层包含10至29重量%的导电细粉末,以使外涂层导电并抑制静电荷 积聚并提高热导率。

    Method of preparing low-temperature-cure polymer composition
    9.
    发明授权
    Method of preparing low-temperature-cure polymer composition 失效
    制备低温固化聚合物组合物的方法

    公开(公告)号:US06416819B1

    公开(公告)日:2002-07-09

    申请号:US09608289

    申请日:2000-06-30

    IPC分类号: B05D302

    摘要: A method of preparing a composition containing a fluorocarbon thermoplastic random copolymer comprising the steps of: (A) providing a mixture having: (i) a fluorocarbon thermoplastic random copolymer having subunits of: —(CH2CF2)x—, —(CF2CF(CF3)y—, and —(CF2 CF2)z—,  wherein x is from 1 to 50 or 60 to 80 mole percent, y is from 10 to 90 mole percent, z is from 10 to 90 mole percent, x+y+z equals 100 mole percent; (ii) a filler comprising zinc oxide; (iii) a curable amino functional polydimethyl siloxane copolymer comprising aminofunctional units selected from the group consisting of (aminoethylaminopropyl) methyl, (aminopropyl) methyl and (aminopropyl) dimethyl; and (iv) antimony-doped tin oxide particles; (v) a bisphenol residue curing agent; and (B) curing the mixture for 5 to 10 hours at a temperature in the range of 25° C. to 275° C.

    摘要翻译: 一种制备含有碳氟化合物热塑性无规共聚物的组合物的方法,包括以下步骤:(A)提供具有以下物质的混合物:(i)具有亚基的氟碳热塑性无规共聚物,其中x为1至50或60至80摩尔% y为10至90摩尔%,z为10至90摩尔%,x + y + z为100摩尔%;(ii)包含氧化锌的填料;(iii)可固化的氨基官能的聚二甲基硅氧烷共聚物,其包含氨基官能单元 选自(氨基乙基氨基丙基)甲基,(氨基丙基)甲基和(氨基丙基)二甲基; 和(iv)锑掺杂氧化锡颗粒;(v)双酚残余固化剂; 和(B)在25℃至275℃的温度下固化混合物5至10小时。