Process for the production of Raney nickel catalysts and their use in the hydrogenation of organic compounds
    7.
    发明授权
    Process for the production of Raney nickel catalysts and their use in the hydrogenation of organic compounds 有权
    生产阮内镍催化剂的方法及其在有机化合物氢化中的应用

    公开(公告)号:US07517829B2

    公开(公告)日:2009-04-14

    申请号:US10932627

    申请日:2004-09-02

    摘要: The invention relates to a process for the production of Raney nickel catalysts. In this process, the melt of an alloy comprising from 40 to 95 wt. % aluminum, from 5 to 50 wt. % nickel, 0 to 20 wt. % iron, from 0 to 15 wt. % of one or more transition metals selected from the group consisting of cerium, cerium mixed metal, vanadium, niobium, tantalum, chromium, molybdenum and manganese, and, optionally, additional glass-forming elements, is brought into contact with one or more rotating cooling rollers or cooling plates and is allowed to cool and solidify thereon. The cooling rollers have a surface structured by means of transverse grooves, and the cooling plates have a surface structured by means of grooves extending outwards from the axis of rotation. The rapidly solidified alloy on the cooling rollers or the cooling plates is then subjected to treatment with one or more organic or inorganic bases.

    摘要翻译: 本发明涉及一种生产阮内镍催化剂的方法。 在该方法中,包含40至95重量% %铝,5至50wt。 %镍,0〜20wt。 %铁,0至15wt。 选自铈,铈混合金属,钒,铌,钽,铬,钼和锰的一种或多种过渡金属和任选的另外的玻璃形成元素的%与一个或多个旋转 冷却辊或冷却板,并在其上冷却和固化。 冷却辊具有由横向槽构成的表面,并且冷却板具有由从旋转轴线向外延伸的槽构成的表面。 然后将冷却辊或冷却板上的快速凝固的合金用一个或多个有机或无机碱进行处理。

    Process for the production of Raney nickel catalysts and their use in the hydrogenation of organic compounds
    10.
    发明申请
    Process for the production of Raney nickel catalysts and their use in the hydrogenation of organic compounds 有权
    生产阮内镍催化剂的方法及其在有机化合物氢化中的应用

    公开(公告)号:US20050107251A1

    公开(公告)日:2005-05-19

    申请号:US10932627

    申请日:2004-09-02

    摘要: The invention relates to a process for the production of Raney nickel catalysts. In this process, the melt of an alloy comprising from 40 to 95 wt. % aluminium, from 5 to 50 wt. % nickel, 0 to 20 wt. % iron, from 0 to 15 wt. % of one or more transition metals selected from the group consisting of cerium, cerium mixed metal, vanadium, niobium, tantalum, chromium, molybdenum and manganese, and, optionally, additional glass-forming elements, is brought into contact with one or more rotating cooling rollers or cooling plates and is allowed to cool and solidify thereon. The cooling rollers have a surface structured by means of transverse grooves, and the cooling plates have a surface structured by means of grooves extending outwards from the axis of rotation. The rapidly solidified alloy on the cooling rollers or the cooling plates is then subjected to treatment with one or more organic or inorganic bases.

    摘要翻译: 本发明涉及一种生产阮内镍催化剂的方法。 在该方法中,包含40至95重量% %铝,5至50wt。 %镍,0〜20wt。 %铁,0至15wt。 选自铈,铈混合金属,钒,铌,钽,铬,钼和锰的一种或多种过渡金属和任选的另外的玻璃形成元素的%与一个或多个旋转 冷却辊或冷却板,并在其上冷却和固化。 冷却辊具有由横向槽构成的表面,并且冷却板具有由从旋转轴线向外延伸的槽构成的表面。 然后将冷却辊或冷却板上的快速凝固的合金用一个或多个有机或无机碱进行处理。