公开(公告)号:US20170073231A1
公开(公告)日:2017-03-16
申请号:US15362349
申请日:2016-11-28
Applicant: KANEKA CORPORATION
Inventor: Yusuke Ohta , Takashi lnada , Makoto Mishiro , Yasushi Nishikawa
CPC classification number: C01B31/04 , C04B35/522 , C04B35/524 , C04B35/62218 , C04B35/63444 , C08G69/26 , C08G69/28 , C08L77/06
Abstract: A graphite film which is low in graphite dust generation can be produced by properly selecting acid dianhydride and diamine which constitute a polyimide film, which polyimide film is a raw material of the graphite film. Specifically, the graphite film which is low in graphite dust generation can be obtained if (1) the acid dianhydride is PMDA and the diamine has a molar ratio of ODA/PDA in a range of 100:0 to 80:20, or (2) the acid dianhydride has a molar ratio of PMDA/BPDA in a range of 80:20 to 50:50, and the diamine has a molar ratio of ODA/PDA in a range of 30:70 to 90:10.
Abstract translation: 可以通过适当选择构成聚酰亚胺膜的酸二酐和二胺作为石墨膜的原料,来制造石墨粉生成量低的石墨膜。 具体而言,如果(1)酸二酐是PMDA,二胺的ODA / PDA的摩尔比在100:0〜80:20的范围内,则可以得到石墨粉尘产生低的石墨膜,或(2 )酸二酐具有80:20至50:50范围内的PMDA / BPDA的摩尔比,二胺的ODA / PDA的摩尔比在30:70至90:10的范围内。
-
公开(公告)号:US20170106641A1
公开(公告)日:2017-04-20
申请号:US14971765
申请日:2015-12-16
Applicant: Kaneka Corporation
Inventor: Yusuke Ohta , Takashi lnada , Makoto Mishiro , Yasushi Nishikawa , Takashi lnada
CPC classification number: B32B37/20 , B32B7/12 , B32B9/007 , B32B37/0053 , B32B37/12 , B32B38/10 , B32B38/18 , B32B2250/02 , B32B2313/04 , C01B32/20 , C04B35/522 , C04B35/524 , C04B35/62218 , C04B35/6269 , C04B35/63468 , C04B2235/604 , C04B2235/6581 , C04B2235/96 , C04B2235/9638
Abstract: A graphite film showing an extremely low average tearing force is more likely to suffer from various kinds of defects, such as splitting, winding deviation, wrinkling, and poor dimensional accuracy, in a step of producing the graphite film and in a step of processing the graphite film. However, these defects can be prevented by using a graphite film that satisfies the following requirements: 1) having an average tearing force of not more than 0.08 N as determined by Trouser tear method in accordance with JIS K7128; and 2) having sag of not less than 5 mm and not greater than 80 mm as determined by a method of film windability evaluation in accordance with JIS C2151.
-
公开(公告)号:US20160194250A1
公开(公告)日:2016-07-07
申请号:US14995016
申请日:2016-01-13
Applicant: Kaneka Corporation
Inventor: Yusuke Ohta , Makoto Mishiro , Takashi lnada , Yasushi Nishikawa
IPC: C04B35/524 , C01B31/04
CPC classification number: C04B35/524 , C01B32/19 , C01B32/20 , C01B32/205 , C01B32/225 , Y10T428/30
Abstract: Provided is a long and large-area graphite film having improved thermal diffusivity and flex resistance, and accompanied by ameliorated ruffling. According to a method for producing a graphite film, in which graphitization of a heat-treated film consisting of a carbonized polymer film is carried out in a state being wrapped around an internal core, the method being characterized in that a heat treatment is executed by controlling distance(s) between the internal core and the film, and/or between the layers of the film, a graphite film accompanied by significantly ameliorated ruffling can be obtained.
Abstract translation: 提供了具有改善的热扩散率和抗弯曲性的长且大面积的石墨膜,并伴随着改善的褶皱。 根据石墨膜的制造方法,其特征在于,在由碳化聚合物膜构成的热处理膜的石墨化被包裹在内部芯部的状态下进行,其特征在于,通过以下方式进行热处理: 可以获得控制内芯和薄膜之间和/或薄膜之间的距离,可以获得伴随显着改善的褶皱的石墨薄膜。
-
公开(公告)号:US20160194204A1
公开(公告)日:2016-07-07
申请号:US14995058
申请日:2016-01-13
Applicant: Kaneka Corporation
Inventor: Yusuke Ohta , Makoto Mishiro , Takashi lnada , Yasushi Nishikawa
IPC: C01B31/04
CPC classification number: C04B35/524 , C01B32/19 , C01B32/20 , C01B32/205 , C01B32/225 , Y10T428/30
Abstract: Provided is a long and large-area graphite film having improved thermal diffusivity and flex resistance, and accompanied by ameliorated ruffling. According to a method for producing a graphite film, in which graphitization of a heat-treated film consisting of a carbonized polymer film is carried out in a state being wrapped around an internal core, the method being characterized in that a heat treatment is executed by controlling distance(s) between the internal core and the film, and/or between the layers of the film, a graphite film accompanied by significantly ameliorated ruffling can be obtained.
Abstract translation: 提供了具有改善的热扩散率和抗弯曲性的长且大面积的石墨膜,并伴随着改善的褶皱。 根据石墨膜的制造方法,其特征在于,在由碳化聚合物膜构成的热处理膜的石墨化被包裹在内部芯部的状态下进行,其特征在于,通过以下方式进行热处理: 可以获得控制内芯和薄膜之间和/或薄膜之间的距离,可以获得伴随显着改善的褶皱的石墨薄膜。
-
-
-