GRAPHITE FILM AND METHOD FOR PRODUCING GRAPHITE FILM
    3.
    发明申请
    GRAPHITE FILM AND METHOD FOR PRODUCING GRAPHITE FILM 有权
    石墨膜和石墨膜生产方法

    公开(公告)号:US20140308484A1

    公开(公告)日:2014-10-16

    申请号:US14361321

    申请日:2012-10-23

    Abstract: A re-forming process is carried out in which a material graphite film is heat-treated to not less than 2000° C. while the material graphite film is being pressured. Through the re-forming process, sag of a graphite film is controlled. By using, during the re-forming process, a plurality of inner cores having respective different surface states, it is possible to produce a graphite film having two or more sag forms which have respective effects.

    Abstract translation: 在材料石墨膜被加压的同时进行将材料石墨膜热处理至不低于2000℃的再成形工艺。 通过重新形成工艺,控制石墨膜的下垂。 通过在再成形过程中使用具有各自不同表面状态的多个内芯,可以生产具有两种或更多种具有各自效果的凹陷形式的石墨膜。

    Graphite Film and Graphite Composite Film
    4.
    发明申请
    Graphite Film and Graphite Composite Film 有权
    石墨膜和石墨复合膜

    公开(公告)号:US20130189180A1

    公开(公告)日:2013-07-25

    申请号:US13795767

    申请日:2013-03-12

    Abstract: An object of the present invention is to provide a graphite film, and a graphite composite film both having an excellent thermal diffusivity which can sufficiently manage heat dissipation of electronic instruments, precision instruments and the like, along with an excellent flex resistance which can withstand application to bent portions.Means for Resolution of the present invention is a graphite film exhibiting the number of reciprocal foldings being 10,000 times or more as measured using a rectangular strip test piece having a width of 15 mm until the test piece breaks in a MIT folding endurance test under conditions of: a curvature radius R of the bending clamp being 2 mm; a left-and-right bending angle being 135°; a bending rate being 90 times/min; and a load being 0.98 N.

    Abstract translation: 本发明的目的是提供一种具有优异的热扩散性的石墨膜和石墨复合膜,其能够充分地管理电子仪器,精密仪器等的散热,以及能够经受应用的优异的抗弯曲性 弯曲部分。 本发明的解决方法是使用宽度为15mm的矩形条状试验片测定的往复折叠数为10,000倍以上的石墨膜,直到试验片在MIT耐折性试验中断裂为止, 弯曲夹具的曲率半径R为2mm; 左右弯曲角度为135°; 弯曲率为90次/分钟; 负载为0.98N。

    ROLLED GRAPHITE SHEET
    5.
    发明申请

    公开(公告)号:US20190039845A1

    公开(公告)日:2019-02-07

    申请号:US16156099

    申请日:2018-10-10

    Abstract: A rolled graphite sheet includes a rod-shaped body and a graphite sheet having a length of 1 m or more and a width shorter than the length. The graphite sheet is wound around the rod-shaped body and is rolled in a length direction. When a length direction-end of the graphite sheet is pulled with a force of 1.5 N/cm in a direction parallel to a tangent of a cross-sectional circle of the rolled graphite sheet while fixing the rod-shaped body, the end moves 5 mm or less in the direction parallel to the tangent of the circle.

    GRAPHITE FILM AND PROCESS FOR PRODUCING GRAPHITE FILM
    8.
    发明申请
    GRAPHITE FILM AND PROCESS FOR PRODUCING GRAPHITE FILM 有权
    石墨膜和生产石墨膜的方法

    公开(公告)号:US20170073231A1

    公开(公告)日:2017-03-16

    申请号:US15362349

    申请日:2016-11-28

    Abstract: A graphite film which is low in graphite dust generation can be produced by properly selecting acid dianhydride and diamine which constitute a polyimide film, which polyimide film is a raw material of the graphite film. Specifically, the graphite film which is low in graphite dust generation can be obtained if (1) the acid dianhydride is PMDA and the diamine has a molar ratio of ODA/PDA in a range of 100:0 to 80:20, or (2) the acid dianhydride has a molar ratio of PMDA/BPDA in a range of 80:20 to 50:50, and the diamine has a molar ratio of ODA/PDA in a range of 30:70 to 90:10.

    Abstract translation: 可以通过适当选择构成聚酰亚胺膜的酸二酐和二胺作为石墨膜的原料,来制造石墨粉生成量低的石墨膜。 具体而言,如果(1)酸二酐是PMDA,二胺的ODA / PDA的摩尔比在100:0〜80:20的范围内,则可以得到石墨粉尘产生低的石墨膜,或(2 )酸二酐具有80:20至50:50范围内的PMDA / BPDA的摩尔比,二胺的ODA / PDA的摩尔比在30:70至90:10的范围内。