Blood filter and method of manufacturing the same

    公开(公告)号:US10265456B2

    公开(公告)日:2019-04-23

    申请号:US15540817

    申请日:2015-12-28

    Abstract: Disclosed are a blood filter which exhibits excellent leukocyte elimination performance as well as significantly improved blood throughput per unit time and erythrocyte recovery rate and a method of manufacturing the same. The blood filter of the present invention includes a pre-treatment filter which is a laminate of first non-woven fabrics having a mean fiber diameter of 5 to 30 μm and a mean pore size of 10 to 30 μm, and a main filter which is a laminate of second non-woven fabrics having a mean fiber diameter of 1 to 5 μm, a mean pore size of 5 to 10 μm and a mean pore size distribution rate of 30% or more. A filling density of the pre-treatment filter and a filling density of the main filter, with respect to a target blood throughput of the blood filter, are 0.1 g/100 ml to 1 g/100 ml and 1 g/100 ml to 3 g/100 ml, respectively.

    POLYESTER NONWOVEN FABRIC AND METHOD FOR MANUFACTURING THE SAME
    2.
    发明申请
    POLYESTER NONWOVEN FABRIC AND METHOD FOR MANUFACTURING THE SAME 审中-公开
    聚酯非织造织物及其制造方法

    公开(公告)号:US20140154943A1

    公开(公告)日:2014-06-05

    申请号:US14232058

    申请日:2012-09-25

    Abstract: Disclosed are a polyester nonwoven fabric which can be used as an useful primary backing substrate for a carpet since it exhibits good physical properties even after tufting process, and a method for manufacturing the same. The polyester nonwoven fabric of the present invention comprises an one-component filament and a sheath-core type filament both of which have a fineness of 4 to 10 denier. The one-component filament comprises a first polyester polymer having a melting point of 250° C. or higher, the sheath-core type filament comprises the first polyester polymer of 70 to 95 wt % as a core component and a second polyester polymer of 5 to 30 wt % as a sheath component, and a melting point of the second polyester polymer is lower than the melting point of the first polyester polymer by 20° C. or more.

    Abstract translation: 公开了一种聚酯无纺布,其可以用作地毯的有用的主要背衬基材,因为即使在簇绒过程之后它也显示出良好的物理性能及其制造方法。 本发明的聚酯无纺布包括细长度为4〜10旦尼尔的单组分长丝和皮芯型丝。 单组分长丝包括熔点为250℃或更高的第一聚酯聚合物,皮芯型长丝包含70至95重量%的第一聚酯聚合物作为核心组分,第二聚酯聚合物为5 至30重量%,第二聚酯聚合物的熔点低于第一聚酯聚合物的熔点为20℃以上。