摘要:
To provide a toner that can keep its melt-sticking to sleeve from occurring and, even in double-sided printing, can keep high-temperature offset from occurring and obtain high-quality images on both the surface and the back. The toner comprises toner particles each of which contains a binder resin containing a resin formed by the reaction of i) a resin (A) having a softening point TA (° C.) of 70° C. to 105° C. and having a peak top of endothermic peaks at 55° C. to 120° C. with ii) a resin (B) having a softening point TB (° C.) of 120° C. to 160° C. and having a peak top of endothermic peaks at 55° C. to 120° C., and, in its viscoelasticity characteristics, has a storage elastic modulus at temperature 180° C. (G′180) of 3.0×103 Pa to 3.0×104 Pa, where the loss tangent tan δ has at least one peak having a peak top within the range of 50° C. to 70° C. and, when peak top temperature of the peak is represented by T(° C.), the loss tangent at T+10(° C.) [tan δ(T+10)] is 1.0 to 1.5 and the ratio of tan δ(T+10)/tan δ(110) is 0.8 to 1.5.
摘要:
A toner is provided which is superior in the long-term storage stability and has high low-temperature fixing properties. In a DSC curve as measured with a differential scanning calorimeter, the toner has a glass transition temperature of not less than 50° C. and not more than 60° C.; and the toner has, in regard to a resin composition contained therein, a difference of not less than 0.060 W/g in heat flow between a point on the curve at a temperature of 40° C. and a baseline in the range exceeding the glass transition temperature; and in viscoelastic characteristics measured at a frequency of 6.28 rad/sec, the toner has a storage elastic modulus (G′40) at a temperature of 40° C. of not less than 7.0×108 Pa and not more than 2.0×109 Pa, and a storage elastic modulus (G′70) at a temperature of 70° C. of not less than 1.0×105 Pa and not more than 1.0×107 Pa.
摘要翻译:提供了一种调色剂,其长期保存稳定性优异且具有高的低温定影性。 在用差示扫描量热计测量的DSC曲线中,调色剂的玻璃化转变温度不低于50℃且不超过60℃。 并且对于其中所含的树脂组合物,调色剂在温度为40℃的曲线上的点与在超过玻璃的范围内的基线之间的热流中的热流不同为0.060W / g 转变温度; 并且以6.28rad / sec的频率测量的粘弹特性中,调色剂在40℃的温度下的储能弹性模量(G'40)不小于7.0×10 8 Pa且不大于2.0×10 9 Pa ,并且在70℃的温度下的储能弹性模量(G'70)不小于1.0×10 5 Pa且不大于1.0×10 7 Pa。
摘要:
To provide a toner that can keep its melt-sticking to sleeve from occurring and, even in double-sided printing, can keep high-temperature offset from occurring and obtain high-quality images on both the surface and the back. The toner comprises toner particles each of which contains a binder resin containing a resin formed by the reaction of i) a resin (A) having a softening point TA (° C.) of 70° C. to 105° C. and having a peak top of endothermic peaks at 55° C. to 120° C. with ii) a resin (B) having a softening point TB (° C.) of 120° C. to 160° C. and having a peak top of endothermic peaks at 55° C. to 120° C., and, in its viscoelasticity characteristics, has a storage elastic modulus at temperature 180° C. (G′180) of 3.0×103 Pa to 3.0×104 Pa, where the loss tangent tan δ has at least one peak having a peak top within the range of 50° C. to 70° C. and, when peak top temperature of the peak is represented by T(° C.), the loss tangent at T+10(° C.) [tan δ(T+10)] is 1.0 to 1.5 and the ratio of tan δ(T+10)/tan δ(110) is 0.8 to 1.5.
摘要:
A toner is provided which is superior in the long-term storage stability and has high low-temperature fixing properties. In a DSC curve as measured with a differential scanning calorimeter, the toner has a glass transition temperature of not less than 50° C. and not more than 60° C.; and the toner has, in regard to a resin composition contained therein, a difference of not less than 0.060 W/g in heat flow between a point on the curve at a temperature of 40° C. and a baseline in the range exceeding the glass transition temperature; and in viscoelastic characteristics measured at a frequency of 6.28 rad/sec, the toner has a storage elastic modulus (G′40) at a temperature of 40° C. of not less than 7.0×108 Pa and not more than 2.0×109 Pa, and a storage elastic modulus (G′70) at a temperature of 70° C. of not less than 1.0×105 Pa and not more than 1.0×107 Pa.
摘要翻译:提供了一种调色剂,其长期保存稳定性优异且具有高的低温定影性。 在用差示扫描量热计测量的DSC曲线中,调色剂的玻璃化转变温度不低于50℃且不超过60℃。 并且对于其中所含的树脂组合物,调色剂在温度为40℃的曲线上的点与在超过玻璃的范围内的基线之间的热流中的热流不同为0.060W / g 转变温度; 并且以6.28rad / sec的频率测量的粘弹特性中,调色剂在40℃的温度下的储能弹性模量(G'40)不小于7.0×10 8 Pa且不大于2.0×10 9 Pa ,并且在70℃的温度下的储能弹性模量(G'70)不小于1.0×10 5 Pa且不大于1.0×10 7 Pa。
摘要:
A toner comprising toner particles, each of which contains a binder resin and a colorant, wherein the binder resin includes a resin having an endothermic peak at a temperature of 55° C. to 120° C. in a DSC curve; the toner has a softening point Tm of 90° C. to 140° C.; in the viscoelastic characteristic of the toner measured at a frequency of 6.28 rad/sec, the storage elastic modulus at a temperature of 180° C. is 1.0×102 Pa to 1.0×104 Pa; in a chart with the temperature on the x-axis and tan δ on the y-axis, tan δ has a peak having a peak top in the range of 50° C. to 70° C.; tan δ (P) at the peak top temperature is 2.0 to 10.0; the ratio of the tan δ (P) at the peak top temperature to tan δ (Tm) at a temperature of Tm (tan δ (P)/tan δ (Tm)) is in the range of 2.5 to 8.0.
摘要:
To provide a developer and an image forming method with each of which a high-resolution, high-definition image can be stably obtained over a long time period irrespective of an environment. The present invention provides a developer including at least: toner particles each containing at least a binder resin; and a composite inorganic fine powder, the developer being characterized in that: the composite inorganic fine powder has a peak at a Bragg angle (2θ±0.20 deg) of each of 32.20 deg, 25.80 deg, and 27.50 deg in a CuKα characteristic X-ray diffraction pattern; and the half width of the X-ray diffraction peak at a Bragg angle (2θ±0.20 deg) of 32.20 deg is 0.20 to 0.30 deg.
摘要:
The present invention aims to provide a toner having excellent developability and excellent low-temperature fixability without causing adhesion of ejected sheets even in a high-speed oilless fixing system and capable of preventing a frameless printing from causing a twisted offseting phenomenon. Specifically, provided is a toner having toner particles including at least a binder resin and a colorant, in which, when the toner is dissolved in a tetrahydrofuran (THF) solvent at 25° C. for 24 hours, the ratio of a THF-soluble matter having an intrinsic viscosity of 5.0×10−2 dl/g or less with respect to the total amount of the THF-soluble matter in a GPC-RALLS-viscometer analysis is 15.0 mass % to 60.0 mass %, and the ratio of a THF-soluble matter having an intrinsic viscosity of 1.5×10−1 dl/g or more with respect to the total amount of the THF-soluble matter in a GPC-RALLS-viscometer analysis is 20.0 mass % to 40.0 mass %.
摘要:
To provide a developer and an image forming method with each of which a high-resolution, high-definition image can be stably obtained over a long time period irrespective of an environment. The present invention provides a developer including at least: toner particles each containing at least a binder resin; and a composite inorganic fine powder, the developer being characterized in that: the composite inorganic fine powder has a peak at a Bragg angle (2θ±0.20 deg) of each of 32.20 deg, 25.80 deg, and 27.50 deg in a CuKα characteristic X-ray diffraction pattern; and the half width of the X-ray diffraction peak at a Bragg angle (2θ±0.20 deg) of 32.20 deg is 0.20 to 0.30 deg.
摘要:
Provide is a toner including toner particles each containing at least a binder resin and a colorant, and an inorganic fine powder, in which the inorganic fine powder has a ratio (A/B) of a total pore volume A measured in a pore diameter range of from 1.9 nm or more and to 8.0 nm or less to a total pore volume B measured in a pore diameter range of from 1.9 nm or more and to 300.0 nm or less of from 0.20 or more and to 1.00 or less, and the total pore volume A is from 1.00×10−2 cm3/g or more and to 1.00 cm3/g or less.
摘要:
Provide is a toner including toner particles each containing at least a binder resin and a colorant, and an inorganic fine powder, in which the inorganic fine powder has a ratio (A/B) of a total pore volume A measured in a pore diameter range of from 1.9 nm or more and to 8.0 nm or less to a total pore volume B measured in a pore diameter range of from 1.9 nm or more and to 300.0 nm or less of from 0.20 or more and to 1.00 or less, and the total pore volume A is from 1.00×10−2 cm3/g or more and to 1.00 cm3/g or less.