Thin cast strip formed of molten steel, process for its production, and
cooling drum for thin cast strip continuous casting apparatus
    2.
    发明授权
    Thin cast strip formed of molten steel, process for its production, and cooling drum for thin cast strip continuous casting apparatus 失效
    由钢水形成的薄铸造钢板,其生产方法,以及用于薄铸造连续铸造装置的冷却滚筒

    公开(公告)号:US6079480A

    公开(公告)日:2000-06-27

    申请号:US836445

    申请日:1997-06-11

    IPC分类号: B22D11/06

    CPC分类号: B22D11/0622

    摘要: A twin drum-type continuous casting process for casting thin cast strip by solidifying molten steel continuously fed between a pair of cooling drums placed parallel to each other, wherein the cooling drums are given an added degree of concave crown such that a solid fraction at the thickness center of the thin cast strip, when the distance from the edges toward the center of the thin cast strip at the closest position of the cooling drums is within 50 mm, is exhibited which is a value greater than the fluid critical solid fraction, or alternatively the cooling rate near the edges of the cooling drums is improved.

    摘要翻译: PCT No.PCT / JP96 / 02518 Sec。 371日期:1997年6月11日 102(e)1997年6月11日PCT PCT 1996年9月5日PCT公布。 公开号WO97 / 09138 日期1997年03月13日一种用于通过固化连续供给在彼此平行放置的一对冷却滚筒之间的钢水来铸造薄铸造带的双滚筒连续铸造方法,其中冷却滚筒被赋予相加程度的凹冠,使得 当在冷却鼓的最靠近的位置处从薄壁铸造带的边缘到中心的距离在50mm内时,在薄铸造带的厚度中心处的固体部分被显示出比液体大的值 临界固体分数,或替代地,冷却鼓边缘附近的冷却速度得到改善。

    Cooling drum for twin-drum continuous casting machine
    3.
    发明授权
    Cooling drum for twin-drum continuous casting machine 有权
    双滚筒连铸机冷却鼓

    公开(公告)号:US06371900B1

    公开(公告)日:2002-04-16

    申请号:US09413842

    申请日:1999-10-06

    IPC分类号: F28F502

    CPC分类号: B22D11/0682

    摘要: A cooling drum for a twin-drum continuous casting machine is capable of ensuring an excellent drum body interior cooling effect and advantageously overcoming both the problem of wear of the cooling drum end portions that are pressure-contacted with, and slide on, the side dams and the problem of their local deformation, and that, as a result, can ensure long-term maintenance of a suitable pressure-contact sliding state between the side dams and the cooling drum so as to enable stable continuous casting over a prolonged period. The cooling drum comprises a drum body portion of a material having a thermal conductivity of 100-400 W/mK and drum end portions part or all of whose portions in pressure-contact with the side dams and/or part or all of whose inner regions are formed of a reinforcing material that is a high-hardness material having a Vickers hardness HV (250 g) of 300-600.

    摘要翻译: 用于双滚筒连续铸造机的冷却滚筒能够确保良好的滚筒体内部冷却效果,并且有利地克服了侧坝的压力接触和滑动的冷却滚筒端部的磨损问题 以及局部变形的问题,能够确保侧坝与冷却鼓之间的长时间保持合适的压力接触滑动状态,能够在长时间内稳定连续铸造。 冷却鼓包括具有100-400W / mK的热导率的材料的鼓主体部分,并且鼓部分部分或全部部分与侧坝压力接触和/或其内部区域的一部分或全部 由维氏硬度HV(250g)为300-600的高硬度材料的增强材料形成。