Abstract:
Provided is an electrostatic latent image developing toner comprising toner matrix particles that comprise resin components comprising a vinyl resin as a main component and a crystalline resin, and a mold release agent. The electrostatic latent image developing toner includes a structural body in which a portion of the crystalline resin is in contact with the mold release agent, and a portion of the crystalline resin having a thread-like structure that is not in contact with the mold release agent, in cross-sections of the toner matrix particles.
Abstract:
Provided is an electrostatic image developing toner incorporating toner mother particles containing a binder resin and a releasing agent, wherein the binder resin contains an amorphous polyester resin and a crystalline resin; and the toner mother particles have a region (A) including a structure a formed with the releasing agent and the crystalline resin being in contact with each other, and a region (B) in which the crystalline resin forms a lamellar crystalline structure b independently existing without contacting with the releasing agent.
Abstract:
An image forming method includes: charging a surface of an electrostatic latent image holder with a charging roller; exposing the charged surface so as to form an electrostatic latent image; and developing the formed electrostatic latent image with toner. The toner contains at least a toner base particle and an external additive minute particle. The external additive minute particle contains a silica-polymer composite minute particle. A silicon atom abundance ratio obtained from abundances of a carbon atom, an oxygen atom and a silicon atom present on an outermost surface and within 3 nm from the outermost surface in a depth direction of the silica-polymer composite minute particle are measured with an x-ray photoelectron spectrometer satisfies at least the following condition A. 15.0 atm %≦silicon atom abundance ratio ({Si/(C+O+Si)}×100)≦30.0 atm % [Condition A]
Abstract:
The invention provides an image formation method, a toner set, and a white toner, by which a masking function of an image layer formed by a white toner on a recording medium can be developed efficiently, and low temperature fixability can be improved. An image formation method for fixing an image forming layer (A) to be formed using a white toner, and an image forming layer (B) to be formed adjacent to the image forming layer (A) using a toner different from the white toner on a recording medium; wherein the following relational expressions (1) and (2) are satisfied: 1.000
Abstract:
An image forming method forms a color toner image and a white toner image using an image forming apparatus having a plurality of developing machines. The color toner image is formed using a color developer containing a first carrier and at least one color toner selected from a yellow toner, a magenta toner, and a cyan toner. The white toner image is formed using a white developer containing a second carrier and a white toner containing at least titanium oxide as a pigment. Formula (1): Iw
Abstract:
A toner for electrostatic latent image development of the present invention includes toner particles containing toner mother particles and an external additive. The external additive contains fatty acid metal salt particles, and a volume based particle diameter (size) distribution of the fatty acid metal salt particles has two peaks on a side of smaller size and a side of larger size, respectively. A volume based mean particle diameter of the fatty acid metal salt particles having the peak on the side of smaller size is 3.0 μm or smaller and a volume based mean particle diameter of the fatty acid metal salt particles having the peak on the side of larger size is larger than a volume based mean particle diameter of the toner mother particles.
Abstract:
It is an object to suppress yellowing of a binder resin while obtaining an image with a high degree of whiteness and to suppress occurrence of image defects when printing at a high temperature and a high humidity.A toner for developing an electrostatic image, the toner including: white toner base particles containing a binder resin and titanium oxide having an average particle size of from 130 to 600 nm; and an external additive including strontium titanate.
Abstract:
A high quality image excellent in low-temperature fixability and good in color stability can be formed by an image forming method of the present invention. In the image forming method, an image is formed by an electrophotographic method using toners of plural colors. Each of the toners of the plural colors contains a crystalline resin, methanol concentrations (%) at transmittance of 50% obtained for methanol wettability evaluation of the toners of the plural colors all fall in a range of 15 to 60%, and assuming that a maximum value and a minimum value of the methanol concentrations (%) at transmittance of 50% obtained for the methanol wettability evaluation of the toners of the plural colors are respectively WH (%) and WL (%), a relationship of 4≤WH−WL≤30 is satisfied.
Abstract:
An electrostatic charge image developing toner includes: toner matrix particles containing a binder resin; and an external additive added to the toner matrix particles, wherein the external additive includes joined particles each including a secondary particle including a plurality of spherical primary particles joined together, the joined particles include at least particles with a secondary particle size d2 in the range of 70 nm to 400 nm, and particles with a ratio d2/d1 in the range of 1.6 to 4.2 make up at least 50% by number of the particles with a secondary particle size d2 in the range of 70 nm to 400 nm, wherein d1 is the diameter of primary particles in the joined particle, and d2 is the secondary particle size.
Abstract:
An image forming method includes: charging a surface of an electrostatic latent image holder with a charging roller; exposing the charged surface so as to form an electrostatic latent image; and developing the formed electrostatic latent image with toner. The toner contains at least a toner base particle and an external additive minute particle. The external additive minute particle contains a silica-polymer composite minute particle. A silicon atom abundance ratio obtained from abundances of a carbon atom, an oxygen atom and a silicon atom present on an outermost surface and within 3 nm from the outermost surface in a depth direction of the silica-polymer composite minute particle are measured with an x-ray photoelectron spectrometer satisfies at least the following condition A. 15.0 atm %≦silicon atom abundance ratio ({Si/(C+O+Si)}×100)≦30.0 atm % [Condition A]