Abstract:
Provided is a method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, LiCoO2 (I) LizMO2 (II) wherein 0.95
Abstract:
Provided is a lithium transition metal oxide having an α-NaFeO2 layered crystal structure, as a cathode active material for lithium secondary battery, wherein the transition metal includes a blend of Ni and Mn, an average oxidation number of the transition metals except lithium is +3 or higher, and the lithium transition metal oxide satisfies Equations 1 and 2: 1.0
Abstract:
Provided is a method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, LiCoO2 (I) LizMO2 (II) wherein 0.95
Abstract:
Provided is a cathode for lithium secondary batteries comprising a combination of one or more compounds selected from Formula 1 and one or more compounds selected from Formula 2. The cathode provides a high power lithium secondary battery composed of a non-aqueous electrolyte which exhibits long lifespan, long-period storage properties and superior stability at ambient temperature and high temperatures.
Abstract:
Provided is an electrode active material comprising a nickel-based lithium transition metal oxide (LiMO2) wherein the nickel-based lithium transition metal oxide contains nickel (Ni) and at least one transition metal selected from the group consisting of manganese (Mn) and cobalt (Co), wherein the content of nickel is 50% or higher, based on the total weight of transition metals, and has a layered crystal structure and an average primary diameter of 3 μm or higher, wherein the amount of Ni2+ taking the lithium site in the layered crystal structure is 5.0 atom % or less.
Abstract:
Provided is a cathode for lithium secondary batteries comprising a combination of one or more compounds selected from Formula 1 and one or more compounds selected from Formula 2. The cathode provides a high-power lithium secondary battery composed of a non-aqueous electrolyte which exhibits long lifespan, long-period storage properties and superior stability at ambient temperature and high temperatures.
Abstract:
Provided is a lithium transition metal oxide having an α-NaFeO2 layered crystal structure, as a cathode active material for lithium secondary battery, wherein the transition metal includes a blend of Ni and Mn, an average oxidation number of the transition metals except lithium is +3 or higher, and the lithium transition metal oxide satisfies Equations 1 and 2: 1.0
Abstract:
Provided is an electrode active material comprising a nickel-based lithium transition metal oxide (LiMO2) wherein the nickel-based lithium transition metal oxide contains nickel (Ni) and at least one transition metal selected from the group consisting of manganese (Mn) and cobalt (Co), wherein the content of nickel is 50% or higher, based on the total weight of transition metals, and has a layered crystal structure and an average primary diameter of 3 μm or higher, wherein the amount of Ni2+ taking the lithium site in the layered crystal structure is 5.0 atom % or less.