公开(公告)号:US11964910B2
公开(公告)日:2024-04-23
申请号:US17048464
申请日:2019-04-17
Applicant: LG Electronics Inc.
Inventor: Dong Gun Gwoo , Young Seok Kim
CPC classification number: C03C8/08 , C03C8/06 , C23D1/02 , F24C15/005 , C03C8/10 , C03C2207/00
Abstract: The present invention relates to an enamel composition capable of implementing cleaning without swelling using moisture, to a manufacturing method therefor, and to cooking utensils. The enamel composition according to the present invention comprises: 20-60 wt % of P2O5; 1-20 wt % of SiO2; 1-30 wt % of B2O3; 10-30 wt % of at least one of Li2O, Na2O, and K2O; 10-40 wt % of at least one selected from the group consisting of post-transition metal oxides and transition metal oxides. Therefore, the present invention provides an enamel composition capable of implementing cleaning without swelling using moisture, a manufacturing method therefor, and cooking utensils.
-
公开(公告)号:US11780766B2
公开(公告)日:2023-10-10
申请号:US16796102
申请日:2020-02-20
Applicant: LG ELECTRONICS INC.
Inventor: Dong Gun Gwoo , Jingon Kim , Young Seok Kim
IPC: C03C8/06 , C03C8/08 , A47J36/04 , F24C15/02 , A47J36/02 , C03C3/064 , C03C3/066 , C23D1/00 , C23D5/02 , F24C15/00 , C03C17/04
CPC classification number: C03C8/08 , A47J36/025 , A47J36/04 , C03C3/064 , C03C3/066 , C23D1/00 , C23D5/02 , F24C15/005 , F24C15/02 , C03C17/04 , C03C2207/04 , C03C2218/17
Abstract: An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include phosphorus pentoxide (P2O5) at 15 to 50 wt %; silicon dioxide (SiO2) at 10 to 20 wt %; boron oxide (B2O3) at 1 to 15 wt %; one or more of lithium oxide (Li2O), sodium oxide (Na2O), or potassium oxide (K2O) at 5 to 20 wt %; one or more of sodium fluoride (NaF), calcium fluoride (CaF2), or aluminum fluoride (AlF3) at 1 to 5 wt %; one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO) at 1 to 35 wt %; and one or more of titanium dioxide (TiO2), cerium dioxide (CeO2), molybdenum trioxide (MoO3), bismuth oxide (Bi2O3), or copper oxide (CuO) at 10 to 25 wt %, such that a heating time required for cleaning may be shortened and oil contaminants may be completely removed.
-
公开(公告)号:US11773007B2
公开(公告)日:2023-10-03
申请号:US16796052
申请日:2020-02-20
Applicant: LG ELECTRONICS INC.
Inventor: Dong Gun Gwoo , Jingon Kim , Young Seok Kim
IPC: C03C8/06 , C03C8/08 , A47J36/04 , F24C15/02 , A47J36/02 , C03C3/064 , C03C3/066 , C03C17/04 , F24C15/00 , C23D5/02 , C23D5/04
CPC classification number: C03C8/08 , A47J36/025 , A47J36/04 , C03C3/064 , C03C3/066 , C03C17/04 , F24C15/005 , F24C15/02 , C03C2207/04 , C03C2218/17 , C23D5/02 , C23D5/04
Abstract: An enamel composition, a method for preparing an enamel composition, and a cooking appliance are provided. The enamel composition may include 15 to 50 wt % of phosphorus pentoxide (P2O5); 5 to 20 wt % of one or more of lithium oxide (Li2O), sodium oxide (Na2O), or potassium oxide (K2O); 1 to 5 wt % of one or more of sodium fluoride (NaF), calcium fluoride (CaF2), or aluminum fluoride (AlF3); 1 to 35 wt % of one or more of magnesium oxide (MgO), barium oxide (BaO), or calcium oxide (CaO); and 5 to 30 wt % of one or more of manganese dioxide (MnO2), molybdenum trioxide (MoO3), bismuth oxide (Bi2O3), or nickel oxide (NiO). The enamel composition may be cleaned without being putting it into water.
-
-