Polypropylene resin composition and monolayer and multilayer film

    公开(公告)号:US11492471B2

    公开(公告)日:2022-11-08

    申请号:US16316585

    申请日:2017-07-18

    摘要: A propylene polymer satisfying (a) below, a soft propylene copolymer satisfying (b) below, and a polyolefin containing a structural unit derived from an unsaturated carboxylic acid and/or a derivative thereof, wherein (a) a melting point is 100° C. or more, and (b) an MFR is in the range of 0.01 to 100 g/10 min, at least one of the following requirements (b-1) and (b-2) is satisfied: (b-1) a syndiotactic triad fraction s 60% or more, and (b-2) a structural unit derived from propylene is 55 to 90 mol % and a structural unit derived from at least one olefin having 2 to 20 carbon atoms (excluding propylene) is contained at 10 to 45 mol % (with provisos), and the relation between an intrinsic viscosity [η] (dL/g) and the MFR satisfies the relation: 1.50×MFR−0.20≤[η]≤2.65×MFR−0.20.

    Olefin resin and method for producing same

    公开(公告)号:US09714306B2

    公开(公告)日:2017-07-25

    申请号:US15128336

    申请日:2015-03-26

    IPC分类号: C08F210/00 C08F210/16

    摘要: The present invention provides an olefin resin with an improved heat resistance, reduced stickiness, excellent optical and low temperature properties, as well as the balance between these physical properties. The olefin resin according to the present invention satisfies the following requirements: (I) a melting peak (Tm) is observed within the range of from 60° C. to 130° C., and the heat of fusion ΔH at the melting peak is within the range of from 5 to 150 J/g; (II) the percentage E (wt %) of a portion soluble in o-dichlorobenzene at 20° C. or lower, and the heat of fusion ΔH satisfy certain relationships; (III) the glass transition temperature (Tg) is from −80 to −30° C.; (IV) the spin-spin relaxation time (T2) of a component having the highest mobility, as obtained in a four-component approximation with a Lorentzian function performed for a free induction decay curve, is within the range of from 150 to 500 ms, and the abundance ratio of the component is within the range of from 15 to 50%; and (V) the intrinsic viscosity [η] as measured in decalin at 135° C. is within the range of from 0.1 to 12 dl/g.

    Adhesive resin composition and laminate

    公开(公告)号:US11292945B2

    公开(公告)日:2022-04-05

    申请号:US17046626

    申请日:2019-04-05

    摘要: An adhesive resin composition of the invention includes an ethylene polymer (A) including an ethylene polymer graft-modified with an unsaturated carboxylic acid or a derivative thereof, and satisfies the following requirements (1) to (4). (1) The melt flow rate (MFR) measured at a temperature of 190° C. and a load of 2160 g in accordance with ASTM D 1238 is 0.1 to 3 g/10 min. (2) The density is 910 to 930 kg/m3. (3) The proportion of fractions that elute at 50° C. and below in crystallization elution fractionation chromatography measurement is not less than 20 mass %. (4) The proportion of fractions that elute at 90° C. and above in crystallization elution fractionation chromatography measurement is not less than 25 mass %.