Abstract:
The purpose of the present invention is to obtain an ethylene•α-olefin•non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene•α-olefin•non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4)125° C. is 5-100, and (4) the B value is 1.20 or more.
Abstract:
The purpose of the present invention is to obtain an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4) 125° C. is 5-100, and (4) the B value is 1.20 or more.
Abstract:
The purpose of the present invention is to obtain an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4)125° C. is 5-100, and (4) the B value is 1.20 or more.
Abstract:
A process capable of producing an ethylene/α-olefin copolymer having a high molecular weight even under the conditions of a high polymerization temperature is provided. The process for producing an ethylene/α-olefin copolymer includes copolymerizing ethylene and an α-olefin having 3 or more carbon atoms in the presence of an olefin polymerization catalyst including a crosslinked metallocene compound (A) represented by the following general formula [I] and a cocatalyst component (B). In the general formula [I], Y is selected from a carbon atom, etc., M is a hafnium atom or the like, R1 to R12 are each selected from a hydrogen atom, a hydrocarbon group, etc., R13 and R14 are each a substituted aryl group or the like, at least one of R13 and R14 is a substituted aryl group having one or more electron-donating substituents having a Hammett substituent constant σ of not more than −0.2, Q is selected from a halogen atom, etc., and j is an integer of 1 to 4.