Abstract:
An object of the present invention is to provide a modifier suitable for obtaining a lubricating oil, a coating material, an adhesive, and the like with better smoothness and few bumps and to provide a rubber composition for a tire, which is suitable for preparing a tire with both excellent braking performance and excellent fuel efficiency. The present invention relates to an organosilicon compound graft copolymer (X) including a main chain derived from an ethylene/a-olefin copolymer (A) and a graft part derived from an organosilicon compound (B) having one or more unsaturated groups; and a rubber composition for a tire, including 1 to 30 parts by mass of the organosilicon compound graft copolymer (X) based on 100 parts by mass of a diene rubber including an aromatic vinyl-conjugated diene copolymerized rubber.
Abstract:
The purpose of the present invention is to obtain an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4)125° C. is 5-100, and (4) the B value is 1.20 or more.
Abstract:
A railroad rail track pad composition including a particular ethylene•α-olefin•non-conjugated polyene random copolymer (A), clay (B), and a sulfur atom-containing silane coupling agent (C) is used in order to lower the viscosity of a rubber composition that is a raw material for molding while suppressing lowering of the rubber elasticity of a crosslinked and molded product to be obtained. In addition, a molded product obtained by crosslinking the composition, particularly a molded product obtained by crosslinking and foam-molding the composition, is provided with rubber elasticity that is suitable as a railroad rail track pad.
Abstract:
[Object] To provide an excellent foaming agent which does not have problems in handling and operation (example: risk of explosion or fire) and inhibition of cross-linking resulting from a foaming agent and problems, such as, mold pollution and environmental pollution, caused by a foaming agent residue, which has excellent uniform dispersibility in a subject of foaming, and which can be used as an alternative to the chemical decomposition type foaming agent.[Solution] A foaming agent formed from at least (A) a high molecular weight compound having a saturated water absorption of 10 to 1,000 g/g in ion-exchanged water (25° C.) and (B) water, wherein a storage modulus (G′) of the agent, determined on the basis of a viscoelasticity measurement at a temperature of 20° C., is 8.0×101 to 1.0×106 Pa at a frequency of 5 rad/s.
Abstract:
The present invention provides a sound insulator which includes: a flexible material (A) having a peak of loss tangent (tan δ), which is determined by dynamic viscoelasticity measurement, in a temperature range of −60° C. to lower than 0° C.; and a resin (B) having a peak of loss tangent (tan δ), which is determined by dynamic viscoelasticity measurement, in a temperature range of 0° C. to 60° C., the sound insulator including the resin (B) at a ratio of 1 to 50 parts by mass with respect to 100 parts by mass of the flexible material (A). The sound insulator of the present invention is a material which realizes excellent sound insulation properties without relying on a complex shape and an increase in weight.
Abstract:
The present invention relates to a polyamide-based thermoplastic elastomer composition [Y] in which a rubber composition [X] and a phenol resin-based crosslinking agent [IV] are dynamically crosslinked, the rubber composition [X] comprising a polyamide [I] including 30 to 100% by mole of a terephthalic acid structural unit and having a melting point of 220 to 290° C.; an ethylene-α-olefin-unconjugated polyene copolymer rubber [II] including structural units of ethylene, an α-olefin having 3 to 20 carbon atoms and an unconjugated polyene, respectively; and an olefin-based polymer [III] including 0.3 to 5.0% by mass of a functional group structural unit, (the total of [I] to [IV]: 100% by mass).
Abstract:
The purpose of the present invention is to obtain an ethylene•α-olefin•non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene•α-olefin•non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4)125° C. is 5-100, and (4) the B value is 1.20 or more.
Abstract:
The purpose of the present invention is to obtain an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that has a low permanent compression set at low temperatures, is flexible, and has an excellent balance of rubber elasticity at low temperatures and tensile strength at normal temperatures. This ethylene-based polymer is an ethylene⋅α-olefin⋅non-conjugated polyene copolymer that includes units derived from ethylene (A), units derived from an α-olefin (B) containing 4-20 carbon atoms, and units derived from a non-conjugated polyene (C) and satisfies (1)-(4). (1) The molar ratio of (A) to (B) is 40/60-90/10, (2) the contained amount of the units derived from (C) is 0.1-6.0 mol %, (3) ML(1+4) 125° C. is 5-100, and (4) the B value is 1.20 or more.