摘要:
[Problem] The present invention provides a method for producing acrylamide from acrylonitrile using a biocatalyst with high productivity at low cost, in which reaction heat can be efficiently removed even at an industrial reaction scale.[Means for Solving] The present invention relates to a method for producing acrylamide by reacting acrylonitrile in the presence of a biocatalyst, wherein the reaction is performed using a reactor having a reaction volume of 1 m3 or more equipped with a tubular heat exchanger, and wherein the difference between a temperature of a cooling water to be introduced into the heat exchanger and a reaction temperature is maintained from 5 to 20° C.
摘要:
There is provided a method for maintaining the activity of a zeolite catalyst in the catalytic production of methylamines from methanol and ammonia using a zeolite catalyst as at least one of catalysts applied, which comprises controlling the amount of aldehyde compounds as impurities flowing into a zeolite catalyst layer to about 0.15 g/hr.kg-cat. or lower, as calculated in terms of formaldehyde.
摘要:
The present invention relates to a method for producing acrylamide comprising: supplying a raw material water to a reactor, supplying acrylonitrile to the reactor, and hydrating acrylonitrile using a biocatalyst, wherein a temperature of the raw material water in the supplying step of the raw material water to the reactor is equal to or more than freezing point of the raw material water and lower than the reaction temperature by 5° C. or more. The present invention can be provided to the method of producing acrylamide which can be removed the reaction heat produced at the hydration reaction of acrylonitrile effectively with a low cost.
摘要:
The present invention provides a method for producing an amide compound from a nitrile compound using a biocatalyst that realizes low cost, energy saving and low environmental burdens. The production method of the amide compound of the present invention is a method for producing an amide compound from a nitrile compound using a biocatalyst in a reactor, wherein the nitrile compound is reacted with the biocatalyst to produce the amide compound under such stirring conditions that the stirring power requirement is in the range of 0.08 to 0.7 kW/m3.
摘要:
Crystals of [S,S]-ethylenediamine-N,N′-disuccinic acid which have a bulk density of 0.45 to 1.2 g/cm3, and a process for obtaining these crystals comprising the steps of adjusting an aqueous solution of an [S,S]-ethylenediamine-N,N′-disuccinic acid metal salt to a temperature of 40 to 80° C. and a pH of 1.9 to 4.5, and cooling the solution to a temperature below 40° C. over a period of 0.2 to 10 hours while supplying a mineral acid so as to maintain the pH at 1.9 to 4.5 to precipitate [S,S]-ethylenediamine-N,N′-disuccinic acid in a high yield.
摘要:
There is provided a powdery S,S-EDDS iron complex improved in its caking property. An S,S-ethylenediamine-N,N′-disuccinic acid iron complex, which is crystalline and has an average particle diameter of from 10 to 1000 μm and a water content of not more than 7% by weight, a powdery S,S-ethylene-N,N′-disuccinic acid (S,S-EDDS) iron complex having a compressive strength of not more than 1 kg/cm2, the compressive strength being measured according to JIS A 1108 after a lapse of 2 months under conditions of a temperature of 50° C. and a load of 300 g/cm2, and a process for producing the same.
摘要翻译:提供粉末状S,S-EDDS铁络合物,其结块性能得到改善。 S,S-乙二胺-N,N'-二琥珀酸铁络合物,其结晶,平均粒径为10〜1000μm,水含量为7重量%以下,粉末状S,S 亚乙基-N,N'-二琥珀酸(S,S-EDDS)铁络合物,抗压强度不超过1kg / cm 2,抗压强度根据JIS A 1108 在温度为50℃,负荷为300g / cm 2的条件下经过2个月及其制造方法。
摘要:
Disclosed is an improvement in a process for catalytic production of methylamines from methanol and NH.sub.3, or methanol, a mixture of methylamines and NH.sub.3, or a mixture of methylamines and NH.sub.3, in a gaseous phase, over a bed of a zeolite catalyst, where the improvement is that the catalyst bed is divided into two or more sub-beds, and the difference between the inlet and outlet temperatures of each catalyst sub-bed is kept in the range of approximately 5.degree. C. to approximately 70.degree. C. while the reaction is carried out.
摘要:
The present invention relates to a method for producing acrylamide comprising: supplying a raw material water to a reactor, supplying acrylonitrile to the reactor, and hydrating acrylonitrile using a biocatalyst, wherein a temperature of the raw material water in the supplying step of the raw material water to the reactor is equal to or more than freezing point of the raw material water and lower than the reaction temperature by 5° C. or more. The present invention can be provided to the method of producing acrylamide which can be removed the reaction heat produced at the hydration reaction of acrylonitrile effectively with a low cost.
摘要:
The present invention provides a method for producing an amide compound from a nitrile compound using a biocatalyst that realizes low cost, energy saving and low environmental burdens. The production method of the amide compound of the present invention is a method for producing an amide compound from a nitrile compound using a biocatalyst in a reactor, wherein the nitrile compound is reacted with the biocatalyst to produce the amide compound under such stirring conditions that the stirring power requirement is in the range of 0.08 to 0.7 kW/m3.
摘要:
Crystals of [S,S]-ethylenediamine-N,N′-disuccinic acid which have a bulk density of 0.45 to 1.2 g/cm3, and a process for obtaining these crystals comprising the steps of adjusting an aqueous solution of an [S,S]-ethylenediamine-N,N′-disuccinic acid metal salt to a temperature of 40 to 80° C. and a pH of 1.9 to 4.5, and cooling the solution to a temperature below 40° C. over a period of 0.2 to 10 hours while supplying a mineral acid so as to maintain the pH at 1.9 to 4.5 to precipitate [S,S]-ethylenediamine-N,N′-disuccinic acid in a high yield.