公开(公告)号:US06875835B2
公开(公告)日:2005-04-05
申请号:US10321801
申请日:2002-12-16
CPC分类号: F16L9/127 , C08F10/00 , C08F210/16 , Y10T428/139 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/07 , C08F2500/13 , C08F2500/04 , C08F4/025
摘要: A copolymer of ethylene and a higher alpha olefin, preferably 1-hexene, can be produced using an activated chromium containing catalyst system and a cocatalyst selected from the group consisting of trialkylboron, trialkylsiloxyalutninum, and a combination of trialkylboron and thalkylaluminum compounds. The polymerization process must be carefully controlled to produce a copolymer resin having an exceptionally broad molecular weight distribution, extremely high PENT ESCR values, and a natural branch profile that impacts branching preferably into the high molecular weight portion of the polymer. The resulting copolymer resin is especially useful in high stiffness pipe applications.
-
公开(公告)号:US06525148B1
公开(公告)日:2003-02-25
申请号:US09640868
申请日:2000-08-18
IPC分类号: C08F452
CPC分类号: F16L9/127 , C08F10/00 , C08F210/16 , Y10T428/139 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/07 , C08F2500/13 , C08F2500/04 , C08F4/025
摘要: A copolymer of ethylene and a higher alpha olefin, preferably 1-hexene, can be produced using an activated chromium containing catalyst system and a cocatalyst selected from the group consisting of trialkylboron, trialkylsiloxyaluminum, and a combination of trialkylboron and trialkylaluminum compounds. The polymerization process must be carefully controlled to produce a copolymer resin having an exceptionally broad molecular weight distribution, extremely high PENT ESCR values, and a natural branch profile that impacts branching preferably into the high molecular weight portion of the polymer. The resulting copolymer resin is especially useful in high stiffness pipe applications.
摘要翻译: 可以使用活化的含铬催化剂体系和选自三烷基硼,三烷基硅氧烷铝和三烷基硼和三烷基铝化合物的组合的助催化剂来制备乙烯和较高级α-烯烃(优选1-己烯)的共聚物。 聚合过程必须仔细控制,以产生具有非常宽的分子量分布,极高的PENT ESCR值和天然分支分布的共聚物树脂,其优选地影响聚合物的高分子量部分的分支。 所得共聚物树脂在高刚度管道应用中特别有用。
-
公开(公告)号:US20100144910A1
公开(公告)日:2010-06-10
申请号:US12704425
申请日:2010-02-11
CPC分类号: C08F10/00 , C08F210/16 , C08F2410/04 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/13 , C08F2500/17 , C08F2500/05 , C08F4/6492 , C08F4/6543 , C08F4/6557
摘要: Catalyst systems for producing olefin polymers, methods of making such catalyst systems, and processes for producing olefin polymers using such catalyst systems are provided. The catalyst system comprises a first component and a second component, where the first component comprises chromium on a support, where the support comprises phosphated alumina, and the second component comprises: (1) a metal halide compound, a transition metal compound, and a precipitating agent, or (2) a substituted or unsubstituted dicyclopentadienyl chromium compound deposited onto a calcined oxide carrier, where the carrier includes silica, alumina, aluminophosphate, or any mixed oxide thereof.
摘要翻译: 提供了用于生产烯烃聚合物的催化剂体系,制备这种催化剂体系的方法,以及使用这种催化剂体系生产烯烃聚合物的方法。 催化剂体系包括第一组分和第二组分,其中第一组分在载体上包含铬,其中载体包含磷酸化氧化铝,第二组分包括:(1)金属卤化物化合物,过渡金属化合物和 沉淀剂,或(2)沉积在煅烧氧化物载体上的取代或未取代的二环戊二烯基铬化合物,其中载体包括二氧化硅,氧化铝,磷酸铝或其任何混合氧化物。
-
公开(公告)号:US07271124B2
公开(公告)日:2007-09-18
申请号:US10877191
申请日:2004-06-25
IPC分类号: B01J27/132
CPC分类号: C08F10/00 , C08F10/02 , C08F210/16 , C08F2410/04 , C08F4/69 , C08F4/646 , C08F4/24 , C08F210/14 , C08F2500/12 , C08F2500/07
摘要: A process to produce ethylene polymers is provided.
摘要翻译: 提供了生产乙烯聚合物的方法。
-
公开(公告)号:US07071276B2
公开(公告)日:2006-07-04
申请号:US10319393
申请日:2002-12-13
IPC分类号: C08F110/02
CPC分类号: C08F10/00 , C08F10/02 , C08F210/16 , C08F2410/04 , C08F4/69 , C08F4/646 , C08F4/24 , C08F210/14 , C08F2500/12 , C08F2500/07
摘要: A process to produce ethylene polymers is provided.
-
公开(公告)号:US07208441B2
公开(公告)日:2007-04-24
申请号:US10997727
申请日:2004-11-23
IPC分类号: B01J27/188 , B01J31/14 , C08F4/52 , C08F4/69
CPC分类号: F16L9/127 , C08F10/00 , C08F210/16 , Y10T428/139 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/07 , C08F2500/13 , C08F2500/04 , C08F4/025
摘要: A copolymer of ethylene and a higher alpha olefin, preferably 1-hexene, can be produced using an activated chromium containing catalyst system and a cocatalyst selected from the group consisting of trialkylboron, trialkylsiloxyalutninum, and a combination of trialkylboron and thalkylaluminum compounds. The polymerization process must be carefully controlled to produce a copolymer resin having an exceptionally broad molecular weight distribution, extremely high PENT ESCR values, and a natural branch profile that impacts branching preferably into the high molecular weight portion of the polymer. The resulting copolymer resin is especially useful in high stiffness pipe applications.
摘要翻译: 乙烯和较高级α-烯烃,优选1-己烯的共聚物可以使用活化的含铬催化剂体系和选自三烷基硼,三烷基硅氧烷和三烷基硼与三烷基铝化合物的组合的助催化剂来制备。 聚合过程必须仔细控制,以产生具有非常宽的分子量分布,极高的PENT ESCR值和天然分支分布的共聚物树脂,其优选地影响聚合物的高分子量部分的分支。 所得共聚物树脂在高刚度管道应用中特别有用。
-
公开(公告)号:US06867278B2
公开(公告)日:2005-03-15
申请号:US10373648
申请日:2003-02-24
申请人: Max P. McDaniel , Elizabeth A. Benham , Al R. Wolfe , Paul J. DesLauriers , Pamela L. Meager , William R. Coutant , David C. Rohlfing , Steven J. Secora
发明人: Max P. McDaniel , Elizabeth A. Benham , Al R. Wolfe , Paul J. DesLauriers , Pamela L. Meager , William R. Coutant , David C. Rohlfing , Steven J. Secora
IPC分类号: C08F4/12 , C08F4/22 , C08F4/24 , C08F4/52 , C08F4/69 , C08F10/00 , C08F210/16 , C08F210/14
CPC分类号: F16L9/127 , C08F10/00 , C08F210/16 , Y10T428/139 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/07 , C08F2500/13 , C08F2500/04 , C08F4/025
摘要: The present invention is directed to homo-polymers and copolymers of mono-1-olefins, a method of making such polymers,and uses of such polymers. Polymers of the present invention are formed by contacting at least one mono-1-olefin having from 2 to about 20 carbon atoms per molecule and at least one mono-1-olefin co-monomer having from 2 to about 10 carbon atoms per molecule in a reaction zone under polymerization conditions in the presence of a hydrocarbon diluent, a catalyst system, and a cocatalyst. In another aspect of the present invention, ethylene copolymers are employed to produce PE-100 pipe. Further, these ethylene copolymers may be employed to produce PE-100 pipe having both small diameters and diameters in excess of 42 inches substantially without sagging or other gravitational deformation. Copolymers of ethylene and 1-hexene are disclosed which are used to produce PE-100 pipe.
摘要翻译: 本发明涉及单-1-烯烃的均聚物和共聚物,制备这种聚合物的方法以及这种聚合物的用途。 本发明的聚合物通过使每分子具有2至约20个碳原子的至少一种单-1-烯烃和至少一种每分子具有2至约10个碳原子的单-1-烯烃共聚物接触而形成 在烃稀释剂,催化剂体系和助催化剂的存在下在聚合条件下的反应区。 在本发明的另一方面,乙烯共聚物用于生产PE-100管。 此外,这些乙烯共聚物可用于生产具有超过42英寸的小直径和直径的PE-100管,基本上不会下垂或其它引力变形。 公开了用于生产PE-100管的乙烯和1-己烯的共聚物。
-
公开(公告)号:US06495638B2
公开(公告)日:2002-12-17
申请号:US09222659
申请日:1998-12-30
IPC分类号: C08F422
CPC分类号: C08F10/00 , C08F10/02 , C08F210/16 , C08F2410/04 , C08F4/69 , C08F4/646 , C08F4/24 , C08F210/14 , C08F2500/12 , C08F2500/07
摘要: A process is provided to produce a catalyst system. The process comprises blending a first component and a second component. The first component of the catalyst system comprises chromium on a support. The amount of chromium on the support is from about 0.05 to about 5 weight percent based on the weight of the support. The support comprises fluorided alumina. The support has a surface area from about 200 to about 550 square meters per gram and a pore volume from about 0.7 to about 2.5 cubic centimeters per gram. The first component is activated at a temperature in the range of about 500° C. to about 900° C. The second component is a transition metal halide catalyst. A process comprising polymerizing ethylene or copolymerizing ethylene and at least one other monomer using the catalyst system to produce ethylene polymers is also provided.
摘要翻译: 提供了一种制备催化剂体系的方法。 该方法包括混合第一组分和第二组分。 催化剂体系的第一组分在载体上包含铬。 基于载体的重量,载体上的铬的量为约0.05至约5重量%。 载体包括氟化氧化铝。 载体的表面积为约200至约550平方米/克,孔体积为约0.7至约2.5立方厘米/克。 第一组分在约500℃至约900℃的温度下活化。第二组分是过渡金属卤化物催化剂。 还提供了使用催化剂体系聚合乙烯或使乙烯和至少一种其它单体共聚以生产乙烯聚合物的方法。
-
公开(公告)号:US06174981B1
公开(公告)日:2001-01-16
申请号:US09213986
申请日:1998-12-17
申请人: Joseph J. Bergmeister , Al R. Wolfe , Steven J. Secora , Elizabeth A. Benham , William R. Coutant , Max P. McDaniel
发明人: Joseph J. Bergmeister , Al R. Wolfe , Steven J. Secora , Elizabeth A. Benham , William R. Coutant , Max P. McDaniel
IPC分类号: C08F21014
CPC分类号: C08F210/16 , C08F4/69 , C08F210/14 , C08F2500/04 , C08F2500/17 , C08F2500/12 , C08F4/22
摘要: Polymerization processes for ethylene and at least one mono-1-olefin comonomer having from about three to eight carbon atoms per molecule in the presence of a catalyst system comprising chromium supported on a silica-titania support and a trialkylboron compound is provided. Novel ethylene copolymers also are produced.
摘要翻译: 提供了在包含负载在二氧化硅 - 二氧化钛载体上的铬和三烷基硼化合物的催化剂体系存在下,每分子具有约3-8个碳原子的乙烯和至少一种单-1-烯烃共聚单体的聚合方法。 还生产新的乙烯共聚物。
-
公开(公告)号:US07829646B2
公开(公告)日:2010-11-09
申请号:US11227786
申请日:2005-09-15
申请人: Paul J. DesLauriers , Max P. McDaniel , Al R. Wolfe , Pamela L. Maeger , William R. Coutant , David C. Rohlfing , Steven J. Secora , William B. Beaulieu , Elizabeth A. Benham , David F. Register
发明人: Paul J. DesLauriers , Max P. McDaniel , Al R. Wolfe , Pamela L. Maeger , William R. Coutant , David C. Rohlfing , Steven J. Secora , William B. Beaulieu , Elizabeth A. Benham , David F. Register
IPC分类号: C08F210/16 , C08F210/14 , C08F10/14 , F16L9/12
CPC分类号: C08F10/00 , C08F210/16 , Y10T428/139 , C08F4/24 , C08F4/69 , C08F210/14 , C08F2500/12 , C08F2500/07 , C08F2500/13 , C08F2500/04 , C08F4/025
摘要: The present invention is directed to PE-100 ethylene copolymers and pipe made thereof having a Tabor abrasion between about 0.01 and about 0.001 grams lost/1000 revolutions. These copolymers are formed by contacting ethylene with at least one mono-1-olefin comonomer having from 2 to about 10 carbon atoms per molecule in a reaction zone under polymerization conditions in the presence of a hydrocarbon diluent, a catalyst system, and a cocatalyst. Additionally, the comonomers may be selected from mono-1-olefins having 4 to 10 carbon atoms, such as, 1-hexene, 1-butene, 4-methyl-1-pentene, 1-octene, and 1-decene. Further, these ethylene copolymers may be employed to produce PE-100 pipe having both small diameters and diameters in excess of 42 inches substantially without sagging or other gravitational deformation. Copolymers of ethylene and 1-hexene are disclosed which are used to produce PE-100 pipe.
摘要翻译: 本发明涉及PE-100乙烯共聚物和由其制成的管,其具有在约0.01至约0.001克损失/ 1000转之间的泰博尔磨损。 这些共聚物是通过在烃类稀释剂,催化剂体系和助催化剂的存在下,在聚合条件下,在反应区中使乙烯与至少一种每分子具有2至约10个碳原子的单-1-烯烃共聚单体接触而形成的。 此外,共聚单体可以选自具有4-10个碳原子的单-1-烯烃,例如1-己烯,1-丁烯,4-甲基-1-戊烯,1-辛烯和1-癸烯。 此外,这些乙烯共聚物可用于生产具有超过42英寸的小直径和直径的PE-100管,基本上不会下垂或其它引力变形。 公开了用于生产PE-100管的乙烯和1-己烯的共聚物。
-
-
-
-
-
-
-
-
-