公开(公告)号:US20090155554A1
公开(公告)日:2009-06-18
申请号:US11957773
申请日:2007-12-17
申请人: Molly Maureen Gentleman , Peter Joel Meschter , Yungyee Jennifer Su Saak , Curtis Alan Johnson , Krishan Lal Luthra
发明人: Molly Maureen Gentleman , Peter Joel Meschter , Yungyee Jennifer Su Saak , Curtis Alan Johnson , Krishan Lal Luthra
CPC分类号: B32B37/24 , B32B2037/243 , B32B2307/308 , B32B2309/105 , B32B2310/0875 , B32B2315/02 , B32B2319/00 , C04B41/009 , C04B41/52 , C04B41/89 , C23C28/04 , C23C28/42 , F01D5/288 , F05D2300/21 , Y10T428/24926 , C04B41/4527 , C04B41/5096 , C04B41/5071 , C04B41/522 , C04B41/5024 , C04B41/5037 , C04B41/524 , C04B35/565 , C04B35/584 , C04B35/806
摘要: An article resistant to recession in high temperature environments, and methods for making the article, are presented herein. The article comprises a substrate, an intermediate coating system disposed over the substrate, and a topcoat disposed over the intermediate coating system. The intermediate coating system comprises a separator layer comprising an oxygen getter material, and a barrier layer disposed over the separator layer, the barrier layer comprising a ceramic composition. The topcoat also comprises this ceramic composition. Moreover, at least about 50% by volume of the ceramic composition present in the barrier layer is a metastable precursor material that tends to transform over time into a product material. At least about 75% by volume of the ceramic composition present in the topcoat is the product material, and up to about 25% by volume of the ceramic composition present in the topcoat is the metastable precursor material.
摘要翻译: 本文给出了耐高温环境中的衰退的制品及其制造方法。 该制品包括基底,设置在基底上的中间涂层系统和设置在中间涂层系统上的顶涂层。 中间涂层系统包括包含吸氧剂材料的隔离层和设置在隔离层上的阻挡层,阻挡层包含陶瓷组合物。 面漆也包含该陶瓷组合物。 此外,阻挡层中存在的至少约50体积%的陶瓷组合物是易于随时间转变成产品材料的亚稳态前体材料。 存在于面漆中的至少约75体积%的陶瓷组合物是产品材料,并且高达约25体积%的外涂层中存在的陶瓷组合物是亚稳态前体材料。