Diffusion welding
    1.
    发明授权
    Diffusion welding 失效
    扩散焊接

    公开(公告)号:US3798748A

    公开(公告)日:1974-03-26

    申请号:US29372672

    申请日:1972-09-29

    Applicant: NASA

    Inventor: HOLKO K

    CPC classification number: B23K20/233

    Abstract: Dispersion-strengthened nickel alloys are sanded on one side and chemically polished. This is followed by a single-step welding process wherein the polished surfaces are forced into intimate contact at 1,400* F for one hour in a vacuum. Diffusion, recrystallization, and grain growth across the original weld interface are obtained during postheating at 2,150* F for two hours in hydrogen.

    Abstract translation: 分散强化的镍合金在一侧磨砂并进行化学抛光。 之后是单步焊接工艺,其中抛光表面在真空中被迫在1400°F紧密接触1小时。 在氢气中在2150°F后加热2小时,得到原始焊接界面的扩散,重结晶和晶粒生长。

    Diffusion welding in air
    2.
    发明授权
    Diffusion welding in air 失效
    扩散焊接在空气中

    公开(公告)号:US3787959A

    公开(公告)日:1974-01-29

    申请号:US3787959D

    申请日:1972-04-24

    Applicant: NASA

    Inventor: MOORE T HOLKO K

    CPC classification number: B23K28/003

    Abstract: Solid state welding a butt joint by fusion welding the peripheral surfaces to form a seal, autogenetically cleaning the faying or mating surfaces of the joint by heating the abutting surfaces to 1,200*C., and heating to the diffusion welding temperature in air.

    Abstract translation: 固态焊接对接接头,通过熔接外围表面形成密封,通过将邻接面加热到1200℃,并加热到空气中的扩散焊接温度,自发地清洗接头的接合表面。

    Enhanced diffusion welding
    3.
    发明授权
    Enhanced diffusion welding 失效
    增强扩散焊接

    公开(公告)号:US3758741A

    公开(公告)日:1973-09-11

    申请号:US3758741D

    申请日:1972-09-14

    Applicant: NASA

    Inventor: HOLKO K MOORE T

    CPC classification number: B23K20/00

    Abstract: Surfaces of unrecrystallized alloys are sanded and polished. This is followed by a two-step welding process wherein the strength of the parent metal is retained at the weld joint. The first step forces the surfaces into intimate contact at a temperature where the metal still has good ductility. The second step causes diffusion, rerystallization, and grain growth across the original weld interface.

    Apparatus for welding blades to rotors
    4.
    发明授权
    Apparatus for welding blades to rotors 失效
    焊接刀片到转子的装置

    公开(公告)号:US3770933A

    公开(公告)日:1973-11-06

    申请号:US3770933D

    申请日:1972-04-24

    Applicant: NASA

    Inventor: HOLKO K MOORE T

    CPC classification number: B23K11/002 B23K2201/001 F01D5/3061

    Abstract: Using magnetic force upset welding to form T-joints between dissimilar thickness parts. This type of resistance welding is used to join compressor and turbine parts thereby reducing the weight and cost of a jet engine.

    Abstract translation: 使用磁力镦锻焊接形成不同厚度部件之间的T型接头。 这种电阻焊接用于连接压缩机和涡轮机部件,从而降低喷气发动机的重量和成本。

    Welding blades to rotors
    5.
    发明授权
    Welding blades to rotors 失效
    焊接刀片到转子

    公开(公告)号:US3745300A

    公开(公告)日:1973-07-10

    申请号:US3745300D

    申请日:1971-04-16

    Applicant: NASA

    Inventor: HOLKO K MOORE T

    CPC classification number: B23K11/002 B23K2201/001

    Abstract: USING MAGNETIC FORCE UPSET WELDING TO FORM T-JOINTS BETWEEN DISSIMILAR THICKNESS PARTS. THIS TYPE OF RESISTANCE WELDING IS USED TO JOIN COMPRESSOR AND TURBINE PARTS THEREBY REDUCING THE WEIGHT AND COST OF A JET ENGINE.