METAL-FIBER REINFORCED PLASTIC COMPOSITE MATERIAL

    公开(公告)号:US20220097345A1

    公开(公告)日:2022-03-31

    申请号:US17418076

    申请日:2019-12-23

    摘要: To provide a metal-fiber reinforced plastic composite material which exhibits favorable impregnation of a matrix resin into a reinforcing fiber substrate and favorable adhesion to metal members, and excellent mechanical properties. The metal-fiber reinforced plastic composite material is a laminate of a metal member and a fiber reinforced plastic, wherein the fiber reinforced plastic includes a reinforcing fiber substrate (A) and a thermoplastic resin composition (B), the thermoplastic resin composition (B) contains a phenoxy resin (B-1) and a polyamide resin (B-2) at a mass ratio (B-1)/(B-2) of 80/20 to 20/80, an adhesive strength of the thermoplastic resin composition (B) to a monofilament of the reinforcing fiber substrate (A) is 40 MPa or more as an interfacial shear strength at 23° C. in a microdroplet method, and an adhesive strength between the metal member and the thermoplastic resin composition (B) is 7.0 MPa or more as a tensile shear strength at 23° C.

    HIGHLY HEAT-RESISTANT THERMOPLASTIC RESIN COMPOSITION AND MOLDED ARTICLE MANUFACTURED THEREFROM

    公开(公告)号:US20220235178A1

    公开(公告)日:2022-07-28

    申请号:US17418963

    申请日:2019-12-23

    摘要: Provided is a thermoplastic resin composition which has excellent heat resistance, mechanical characteristics, and adhesion properties with respect to a reinforcing fiber base material, which is a different kind of material, and from which a molded article particularly having excellent rigidity at a high temperature is obtained. A thermoplastic resin composition is provided, which includes: a phenoxy resin (A) having a hydroxy group and/or an epoxy group at a polymer chain terminal; and a polyamide resin (B), wherein a proportion of the phenoxy resin (A) is 50 to 90 mass % and a proportion of the polyamide resin (B) is 10 to 50 mass % relative to a total amount of 100 mass % of the phenoxy resin (A) and the polyamide resin (B), and a tensile modulus retention rate [Equation (i) below] of a dumbbell test piece (JIS K 7139, Type A1), and a molded article manufactured therefrom is also provided.