HOT-DIP PLATED STEEL SHEET
    1.
    发明申请

    公开(公告)号:US20250109473A1

    公开(公告)日:2025-04-03

    申请号:US18848434

    申请日:2023-06-09

    Abstract: A hot-dip plated steel sheet includes a hot-dip plated layer formed on a surface of a steel sheet, the hot-dip plated layer contains 4 to 22 mass % of Al and 1.0 to 10 mass % of Mg with a remainder including Zn and impurities, a pattern portion and a non-pattern portion are formed in the hot-dip plated layer, an element concentrated region containing an element M and an interface alloy layer containing Fe and Al are present at an interface between the steel sheet and the hot-dip plated layer in the pattern portion, an average concentration of the element M contained in the hot-dip plated layer present in the pattern portion and the element concentrated region is 0.0010 to 2 mass %, and in the element concentrated region, the element M is concentrated two or more times the hot-dip plated layer present in the pattern portion, or the element M is unevenly distributed.

    HOT-DIPPED Zn-Al-Mg-BASED PLATED STEEL
    2.
    发明公开

    公开(公告)号:US20230235437A1

    公开(公告)日:2023-07-27

    申请号:US18007650

    申请日:2021-03-19

    CPC classification number: C23C2/06 C22C18/04 B32B15/013 C23C2/40 C23C2/29

    Abstract: This hot-dip Zn—Al—Mg-based plated steel includes: a steel; and a plating layer formed on a surface of the steel, in which the plating layer contains, as an average composition, Mg: 1 to 10 mass %, Al: 4 to 22 mass %, and a remainder consisting of Zn and impurities, the plating layer includes an (Al—Zn mixed structure) in an area ratio of 10% to 70% in a cross section of the plating layer in a matrix of an (Al/Zn/MgZn2 ternary eutectic structure), the (Al—Zn mixed structure) includes a first region that has a Zn concentration in a range of 75 mass % or more and less than 85 mass % and a second region that is present inside the first region and has a Zn concentration in a range of 67 mass % or more and less than 75 mass %, and an area ratio of the second region in the (Al—Zn mixed structure) in the cross section of the plating layer is more than 0% and 40% or less.

Patent Agency Ranking