ZN-AL-MG PLATED CHECKERED STEEL PLATE
    2.
    发明公开

    公开(公告)号:US20240183018A1

    公开(公告)日:2024-06-06

    申请号:US18553206

    申请日:2022-04-05

    Abstract: Provided is a Zn—Al—Mg alloy coated checkered steel sheet having on the sheet surface thereof convex part and flat part, wherein: the coating layer has a predetermined chemical composition, and when observing a cross section of cutting edge orthogonal to a longitudinal direction of the convex part and taken along a sheet thickness direction at a central part in the longitudinal direction of the convex part, a layer thickness ratio of the coating layer of the flat part on left and right of the convex part (layer thickness of left coating layer/layer thickness of right coating layer) is from 0.2 to 5.0, and a convex height T−t, where T is a sheet thickness of the substrate checkered steel sheet at the convex part and t is a sheet thickness of the substrate checkered steel sheet at the flat part, and a gap height x between a stationary surface and a sheet surface of the coated checkered steel sheet opposite to the stationary surface in a case in which the coated checkered steel sheet is placed in a stationary position satisfy the following Formulas 1 and 2 below.


    x/(T−t)≤1.5  Formula 1:



    0.5

    BATTERY CASE AND METHOD OF PRODUCTION OF SAME

    公开(公告)号:US20220216548A1

    公开(公告)日:2022-07-07

    申请号:US17608418

    申请日:2020-06-10

    Abstract: A battery case and method of production of the same realizing smaller size, higher mountability, longer service life, and lower cost than in the past, that is, a battery case comprising a container body and a container cover, in which battery case, one or both of the container body and the container cover are made from a laminated steel sheet comprised of a plated steel sheet on which a film having a polyolefin-based resin as a main constituent is laminated, a joined part of the container body and the container cover has a welded part of the plated steel sheet, a melt bonded part of the film, and a gap part between the welded part and the melt bonded part, where a length of gap part/thickness of plated steel sheet ≤10.0 and a length of gap part/length of joined part

    COATED STEEL MATERIAL
    5.
    发明申请

    公开(公告)号:US20220371302A1

    公开(公告)日:2022-11-24

    申请号:US17771012

    申请日:2020-10-16

    Abstract: A coated steel material including: a base steel, and a coating layer containing a Zn—Al—Mg alloy layer disposed on a surface of the base steel, wherein the coating layer has a predetermined chemical composition, and, in a backscattered electron image of the Zn—Al—Mg alloy layer that is obtained at a time of observing the surface of the Zn—Al—Mg alloy layer after polishing to ½ of the layer thickness, under a scanning electron microscope at a magnification of 100×, Al crystals are present, and the average value of the cumulative circumferential length of the Al crystals is 88 to 195 mm/mm2.

    COATED STEEL PRODUCT
    6.
    发明申请

    公开(公告)号:US20220356547A1

    公开(公告)日:2022-11-10

    申请号:US17619268

    申请日:2020-04-16

    Abstract: A hot-dip coated steel product including: a steel product; and a coating layer including a Zn—Al—Mg alloy layer disposed on a surface of the steel product, in which the Zn—Al—Mg alloy layer includes a Zn phase, an Al phase, and a MgZn2 phase, and contains a Mg—Sn intermetallic compound phase in the Zn phase, and the coating layer has a chemical composition satisfying a predetermined average composition, a total area proportion of the Al phase and the MgZn2 phase is 70% or more, an area proportion of the Zn phase is 30% or less, an average value of cumulative circumferential lengths of the Al phase is less than 88 mm/mm2, and a total frequency in number of the Al phase having a circumferential length of 50 μm or more is less than 100.

    Ni-COATED STEEL SHEET HAVING EXCELLENT CORROSION RESISTANCE AFTER WORKING AND METHOD FOR MANUFACTURING Ni-COATED STEEL SHEET

    公开(公告)号:US20220010450A1

    公开(公告)日:2022-01-13

    申请号:US17291846

    申请日:2019-12-20

    Abstract: A Ni-coated steel sheet according to an aspect of the present invention includes: a base steel sheet; a diffusion alloy layer disposed on the base steel sheet; and a Ni-coated layer disposed on the diffusion alloy layer, in which a depth-hardness curve obtained by continuously performing Vickers hardness measurement on a cross section perpendicular to a rolled surface of the base steel sheet from a surface layer of the Ni-coated layer to the base steel sheet using a nanoindenter includes, in the diffusion alloy layer, a peak indicating a Vickers hardness of 1.50 times or more a Vickers hardness of the surface layer of the Ni-coated layer.

    METALLIC COATED STEEL
    10.
    发明申请

    公开(公告)号:US20250109475A1

    公开(公告)日:2025-04-03

    申请号:US18840411

    申请日:2023-02-22

    Abstract: This metallic coated steel includes a steel material and a metallic coating layer. The metallic coating layer has an average chemical composition including Al: 0.2% to less than 4.0%, Mg: more than 4.0% and less than 12.5%, Ca: 0.15% to less than 3.00%, Zn: 65% or more, and impurities. In an any perpendicular cross section (in a thickness direction) in the metallic coating layer, a metallurgical structure observed in a scanning electron microscope observed visual field contains, in terms of area fraction, an MgZn2 phase: 10 to 40%, an Al—Zn phase: 0 to 15%, an Al phase: (Zn