公开(公告)号:US10807177B2
公开(公告)日:2020-10-20
申请号:US16487523
申请日:2018-02-21
发明人: Kazuaki Hosomi , Kouki Tomimura , Takefumi Nakako
IPC分类号: B23K1/19 , B23K1/20 , B23K35/28 , C22C18/04 , B23K103/08 , B23K103/10 , B23K101/18
摘要: The present invention provides a method for MIG brazing an Al alloy to a steel sheet so as to manufacture a lap joint member that excels in bonding strength with respect to the Al alloy. With the MIG brazing method, a bonding target sheet, specifically, an Al sheet or an Al alloy sheet is bonded to a hot dip Zn-based alloy coated steel sheet (1) whose coating layer contains Al in an amount of 1.0% by mass to 22.0% by mass. A target location of MIG brazing is a region between (i) an intersection (C) of one end of an end surface (6) of the bonding target sheet and the hot dip Zn-based alloy coated steel sheet and (ii) the other end (U) of the end surface of the bonding target sheet.
-
2.
公开(公告)号:US20200055133A1
公开(公告)日:2020-02-20
申请号:US16487523
申请日:2018-02-21
发明人: Kazuaki Hosomi , Kouki Tomimura , Takefumi Nakako
摘要: The present invention provides a method for MIG brazing an Al alloy to a steel sheet so as to manufacture a lap joint member that excels in bonding strength with respect to the Al alloy. With the MIG brazing method, a bonding target sheet, specifically, an Al sheet or an Al alloy sheet is bonded to a hot dip Zn-based alloy coated steel sheet (1) whose coating layer contains Al in an amount of 1.0% by mass to 22.0% by mass. A target location of MIG brazing is a region between (i) an intersection (C) of one end of an end surface (6) of the bonding target sheet and the hot dip Zn-based alloy coated steel sheet and (ii) the other end (U) of the end surface of the bonding target sheet.
-
公开(公告)号:US10792746B2
公开(公告)日:2020-10-06
申请号:US16487516
申请日:2018-02-21
发明人: Kazuaki Hosomi , Kouki Tomimura , Takefumi Nakako
摘要: The present invention provides a method for laser brazing an Al alloy to a steel sheet so as to produce a lap joint member that excels in bonding strength with respect to the Al alloy. The laser brazing method includes a brazing step of forming a brazed part (9) for bonding an Al alloy (3) to a hot dip Zn-based alloy coated steel sheet (1) in which a coating layer (2) contains 1.0 to 22.0% by mass of Al and a coating weight per surface is 15 to 250 g/m2.
-
公开(公告)号:US20200023453A1
公开(公告)日:2020-01-23
申请号:US16487516
申请日:2018-02-21
发明人: Kazuaki Hosomi , Kouki Tomimura , Takefumi Nakako
摘要: The present invention provides a method for laser brazing an Al alloy to a steel sheet so as to produce a lap joint member that excels in bonding strength with respect to the Al alloy. The laser brazing method includes a brazing step of forming a brazed part (9) for bonding an Al alloy (3) to a hot dip Zn-based alloy coated steel sheet (1) in which a coating layer (2) contains 1.0 to 22.0% by mass of Al and a coating weight per surface is 15 to 250 g/m2.
-
公开(公告)号:US10975899B2
公开(公告)日:2021-04-13
申请号:US16344435
申请日:2017-09-15
IPC分类号: C23C2/06 , C23C2/40 , C22C18/04 , B23K9/025 , F16B5/08 , B23K9/09 , B23K9/02 , B23K9/23 , B32B15/04 , B23K9/16 , C23C30/00 , B32B15/01 , B23K35/38 , C22C18/00 , B32B15/18 , B23K101/00 , B23K101/34
摘要: A welded member includes a hot dip Zn-based alloy coated steel sheet as a base material and has excellent corrosion resistance and weld bead shear strength. In the welded member in which a lower sheet and an upper sheet, which are hot dip Zn-based alloy coated steel sheets, are stacked and arc-welded together, a weld bead is formed so that a cross-sectional width W satisfies the following formula 2T≤W≤6T, and a blowhole occupancy Br represented by the following formula becomes not more than 50%: Br=(Σdi/L)×100, where T represents a thickness of the hot dip Zn-based alloy coated steel sheet, di represents a length of an i-th blowhole observed in X-ray radiography, and L represents a length of the weld bead.
-
公开(公告)号:US20200056643A1
公开(公告)日:2020-02-20
申请号:US16344435
申请日:2017-09-15
摘要: A welded member includes a hot dip Zn-based alloy coated steel sheet as a base material and has excellent corrosion resistance and weld bead shear strength. In the welded member in which a lower sheet and an upper sheet, which are hot dip Zn-based alloy coated steel sheets, are stacked and arc-welded together, a weld bead is formed so that a cross-sectional width W satisfies the following formula 2T≤W≤6T, and a blowhole occupancy Br represented by the following formula (2) becomes not more than 50%: Br=(Σdi/L)×100, where T represents a thickness of the hot dip Zn-based alloy coated steel sheet, di represents a length of an i-th blowhole observed in X-ray radiography, and L represents a length of the weld bead.
-
公开(公告)号:US10518351B2
公开(公告)日:2019-12-31
申请号:US15529233
申请日:2015-07-31
发明人: Tomokazu Nobutoki , Kazuaki Hosomi
IPC分类号: B23K9/00 , B23K9/02 , B23K9/23 , C23C2/06 , C22C18/04 , B23K9/032 , B23K9/095 , F16B5/08 , B23K103/04 , B23K101/18
摘要: Provided are: an arc welding method that suppresses occurrences of blow holes in initial parts and final parts in a Zn plated steel sheet and reduces the occupancy ratio for blow holes in the welded part as a whole; and a welded joint.
-
-
-
-
-
-