Gel sealing articles
    1.
    发明授权
    Gel sealing articles 有权
    凝胶密封用品

    公开(公告)号:US6132867A

    公开(公告)日:2000-10-17

    申请号:US142981

    申请日:1998-09-17

    IPC分类号: C09K3/10 F16J15/02 C08K3/10

    摘要: A gel profile article comprising a multi-filament yarn carrier carrying an elongate body of gel which encloses more than 50%, preferably more than 75%, more preferably substantially all, of the perimeter of the carrier as viewed in transverse cross-section, wherein the carrier is at least partly composed of synthetic polymeric material, preferably polyester filaments (e.g. polyethylene terephthalate) or spun yarns of a co-mingled blend of polyacrylonitrile staple fibres and polyamide staple fibres ("baby wool"), the proportion of polyamide preferably being at least 30%, more preferably 40-60%, by weight of the said spun yarn(s). The gel is preferably melt-coated, especially pressure-extruded, around the carrier at a gel temperature less than the softening temperature of at least a component of the carrier, and the selected class of carrier materials enhances the processability, cohesion, and appearance of the resulting profile.

    摘要翻译: PCT No.PCT / GB97 / 00775 Sec。 371日期:1998年9月17日 102(e)日期1998年9月17日PCT 1997年3月20日PCT公布。 出版物WO97 / 35127 日期1997年9月25日一种凝胶型材制品,其包含承载细长体凝胶体的复丝纱线载体,其包围载体周长的50%以上,优选大于75%,更优选基本上全部为横向 横截面,其中载体至少部分由合成聚合物材料,优选聚酯长丝(例如聚对苯二甲酸乙二醇酯)或聚丙烯腈短纤维和聚酰胺短纤维(“婴儿羊毛”)的共混混合物的短纤纱组成, 聚酰胺的比例优选为所述细纱的重量的至少30%,更优选为40-60%。 凝胶优选在低于载体组分的软化温度的凝胶温度下在载体周围进行熔融涂覆,特别是压力挤压,所选择的载体材料种类增强了加工性,内聚力和外观 生成的配置文件。

    Gels made from triblock copolymers
    2.
    发明授权
    Gels made from triblock copolymers 失效
    由三嵌段共聚物制成的凝胶

    公开(公告)号:US5994446A

    公开(公告)日:1999-11-30

    申请号:US981167

    申请日:1998-03-25

    IPC分类号: C08F220/18 C08L53/00 C08K5/01

    CPC分类号: C08F220/18 C08L53/00

    摘要: Gels of oil-extended methacrylate-alkylene-methacrylate (M-A-M) triblock copolymers having higher glass transition temperatures than known styrene-alkylene-styrene triblock gels. The preferred M-A-M triblocks for making the new gels have polymethylmethacrylate end blocks and butadiene or ethylene/butylene mid-block, and are synthesised by methods in the public domain (inter alia Shell EP-A-0431706). Includes gels of new triblocks having end blocks of higher alkyl (e.g. isobornyl) methacrylate homopolymer or copolymers. Mixed methyl- and higher alkyl-methacrylate end blocks are preferred to reduce gel-formation problems which may arise from solubility parameter of homo-isobornylmethacrylate end blocks being too close to that of extender oil. Includes gels of new multi- (preferably penta-) block copolymers including styrene (S) blocks, e.g. M-S-A-S-M.

    摘要翻译: PCT No.PCT / GB96 / 01381 Sec。 371日期:1998年5月25日 102(e)日期1998年5月25日PCT提交1996年6月10日PCT公布。 出版物WO97 / 00292 日期1997年1月3日具有比已知苯乙烯 - 亚烷基 - 苯乙烯三嵌段凝胶更高的玻璃化转变温度的油 - 甲基丙烯酸酯 - 亚烷基 - 甲基丙烯酸酯(M-A-M)三嵌段共聚物的凝胶。 用于制备新凝胶的优选的M-A-M三嵌段具有聚甲基丙烯酸甲酯端嵌段和丁二烯或乙烯/丁烯中嵌段,并且通过公共领域(尤其是Shell EP-A-0431706)中的方法合成。 包括具有高级烷基(如异冰片基)甲基丙烯酸酯均聚物或共聚物端嵌段的新三嵌段凝胶。 混合的甲基和高级烷基酯 - 甲基丙烯酸酯嵌段是优选的,以减少可能由甲基异丁烯酸异冰片酯末端嵌段的溶解度参数产生的凝胶形成问题太接近于增量油的溶解度参数。 包括新的多(优选五嵌段)嵌段共聚物的凝胶,包括苯乙烯(S)嵌段。 M-S-A-S-M。