FIBER PREFORM AND METHOD FOR MANUFACTURING THEREOF
    1.
    发明申请
    FIBER PREFORM AND METHOD FOR MANUFACTURING THEREOF 审中-公开
    纤维预制件及其制造方法

    公开(公告)号:US20120087625A1

    公开(公告)日:2012-04-12

    申请号:US13327736

    申请日:2011-12-15

    摘要: A fiber preform, including: a fiber core rod and an outer cladding layer. The ratio of the diameter of the fiber core rod to the diameter of the core layer thereof is 2.1-2.8. The fiber core rod and a small fluorine-doped quartz glass tube are melted to form a core rod assembly. The ratio of the diameter difference between the core rod assembly and the fiber core rod to the diameter of the core layer is 0.5-2.2. The relative refractive index difference of fluorine-doped quartz glass relative to purified quartz glass ΔF is −0.20% to −0.35%. The core rod assembly is arranged with a large purified quartz glass tube, or directly deposited with a SiO2 glass cladding layer. A ratio of an effective diameter of the fiber preform to the diameter of the core rod assembly is 2.0-5.6. Methods for manufacturing the preform and a fiber are also provided.

    摘要翻译: 一种纤维预制件,包括:纤维芯棒和外包层。 纤维芯棒的直径与其芯层直径的比为2.1-2.8。 纤维芯棒和小的氟掺杂石英玻璃管被熔化以形成芯棒组件。 芯棒组件和纤维芯棒之间的直径差与芯层直径之比为0.5-2.2。 氟掺杂石英玻璃相对于纯化石英玻璃与Dgr F的相对折射率差为-0.20%至-0.35%。 芯棒组件布置有大的纯化石英玻璃管,或直接沉积有SiO 2玻璃包层。 纤维预制棒的有效直径与芯棒组件的直径之比为2.0-5.6。 还提供了用于制造预成型件和纤维的方法。

    SINGLE-MODE FIBER AND PRODUCTION METHOD THEREOF
    3.
    发明申请
    SINGLE-MODE FIBER AND PRODUCTION METHOD THEREOF 有权
    单模光纤及其生产方法

    公开(公告)号:US20110058780A1

    公开(公告)日:2011-03-10

    申请号:US12839432

    申请日:2010-07-20

    摘要: A single mode fiber having a core, an inner cladding, a depressed cladding, and an outer cladding composed of pure silica glass. The core is surrounded in sequence with the inner cladding and the depressed cladding. The core has silica glass doped with germanium and fluorine, with a diameter (a) of 8.0-8.8 μm, a relative refractive index difference (Δ1) of 0.35-0.38%, and the contribution of fluoride (ΔF) is −0.09±0.02%. The inner cladding has silica glass doped with germanium and fluorine, with a diameter (b) of 18-21 μm and a relative refractive index difference (Δ2) of 0±0.02%. The depressed cladding has silica glass doped with fluorine, with a diameter (c) of 26-36 μm and a relative refractive index difference (Δ32) at the external interface thereof is between −0.22 and −0.35%, and a relative refractive index difference (Δ31) at the internal interface thereof is between −0.20 and −0.35%, and Δ32≦Δ31. The fiber has a good bending resistance, good mechanical properties, and extended service lifetime, and prevents the additional stresses generated by bending from passing on to the core, thereby reducing attenuation.

    摘要翻译: 具有芯,内包层,凹陷包层和由纯二氧化硅玻璃构成的外包层的单模光纤。 芯部与内包层和凹陷包层依次包围。 芯具有掺杂有锗和氟的二氧化硅玻璃,直径(a)为8.0-8.8μm,相对折射率差(&Dgr; 1)为0.35-0.38%,氟化物(&Dgr; F)的贡献为 -0.09±0.02%。 内包层具有掺杂有锗和氟的二氧化硅玻璃,其直径(b)为18-21μm,相对折射率差(&Dgr; 2)为0±0.02%。 凹陷的包层具有掺杂有氟的二氧化硅玻璃,其直径(c)为26-36μm,其外界面处的相对折射率差(&Dgr; 32)在-0.22和-0.35%之间,相对折射率 在其内部界面处的指数差异(&Dgr; 31)在-0.20和-0.35%之间,&Dgr; 32≦̸&Dgr; 31。 纤维具有良好的抗弯曲性,良好的机械性能和延长的使用寿命,并且防止由弯曲产生的附加应力传递到芯上,从而减少衰减。

    MULTI-MODE BENDING-RESISTANT FIBER AND PRODUCTION METHOD THEREOF
    4.
    发明申请
    MULTI-MODE BENDING-RESISTANT FIBER AND PRODUCTION METHOD THEREOF 有权
    多模抗弯纤维及其生产方法

    公开(公告)号:US20110044596A1

    公开(公告)日:2011-02-24

    申请号:US12839396

    申请日:2010-07-19

    IPC分类号: G02B6/028 G02B6/10

    摘要: A multimode fiber including a core and a cladding. The core has a radius (R1) of 24-26 μm, the refractive index profile thereof is a parabola, and the maximum relative refractive index difference (Δ1) is 0.9-1.1%. The cladding surrounds the core and includes from inside to outside an inner cladding, a middle cladding, and an outer cladding; a radius (R2) of the inner cladding is 1.04-1.6 times that of the core, and a relative refractive index difference (Δ2) thereof is −0.01-0.01%; the middle cladding is a graded refractive index cladding whose radius (R3) is 1.06-1.8 times that of the core, and a relative refractive index difference thereof is decreased from Δ2 to Δ4; and a radius (R4) of the outer cladding is 2.38-2.63 times that of the core, and a relative refractive index difference (Δ4) thereof is between −0.20 and −0.40%. The invention reduces the additional bending loss of the fiber, improves the bending resistance and mechanical properties, basically eliminates the internal stress, and ensures the service life even working for a long term under the condition of low radius. The method for producing the fiber is simple, effective, and suitable for mass production.

    摘要翻译: 包括芯和包层的多模光纤。 芯的半径(R1)为24-26μm,其折射率分布为抛物线,最大相对折射率差(&Dgr; 1)为0.9-1.1%。 该包层围绕该芯并且包括从内到外的内包层,中包层和外包层; 内包层的半径(R2)为芯的1.04-1.6倍,折射率差(&Dgr; 2)为-0.01-0.01%。 中间包层是其半径(R3)为纤芯的1.06-1.8倍的渐变折射率包层,其相对折射率差从&Dgr; 2减小到&Dgr; 4; 并且外包层的半径(R 4)为芯的2.38-2.63倍,并且其相对折射率差(&Dgr; 4)在-0.20和-0.40%之间。 本发明减少了纤维的附加弯曲损耗,提高了抗弯曲性和机械性能,基本上消除了内部应力,并且在半径低的条件下长期保证使用寿命。 纤维的制造方法简单,有效,适合批量生产。