摘要:
A polymer having a density of from about 0.94 g/cm3 to about 0.96 g/cm3 and a primary structure parameter 2 (PSP2 value) of greater than about 8.5, wherein an article formed from the polymer has an environmental stress crack resistance of equal to or greater than about 1000 hours when measured in accordance with ASTM D 1693 condition A. A polymer having at least one lower molecular weight component and at least one higher molecular weight component and having a PSP2 value of equal to or greater than about 8.5, wherein an article formed from the polymer has an environmental stress crack resistance of greater than about 1000 hours when measured in accordance with ASTM D 1693 condition A.
摘要翻译:密度为约0.94g / cm 3至约0.96g / cm 3,一次结构参数2(PSP2值)大于约8.5的聚合物,其中由聚合物形成的制品具有等于 或根据ASTM D1693条件A测量时大于约1000小时。具有至少一种较低分子量组分和至少一种较高分子量组分并且PSP2值等于或大于约8.5的聚合物,其中 根据ASTM D 1693条件A测量时,由聚合物形成的制品具有大于约1000小时的环境应力抗裂性。
摘要:
A unimodal polymeric resin having a density of from about 0.946 g/ml to about 0.97 g/ml and a zero shear viscosity of from about 8×102 Pa-s to about 6×104 Pa-s. A method comprising (a) providing a catalyst system comprising a half-sandwich transition metal complex; (b) contacting the catalyst system with an olefin under conditions suitable to form a polyolefin, wherein the polyolefin is unimodal; and (c) recovering the polyolefin, wherein the polyolefin has a density of from about 0.946 g/ml to about 0.97 g/ml and a zero shear viscosity of from about 8×102 Pa-s to about 6×104 Pa-s. A unimodal polymeric resin having a density of from about 0.946 g/ml to about 0.97 g/ml and a CY-a parameter of from about 0.5 to about 0.6.
摘要:
A catalyst system comprising a half-sandwich chromium complex, an activator support and an optional cocatalyst. A compound of formula Cp′Cr(Cl)2(Ln), where Cp′ is η5-C5H4CH2CH2CH═CH2 and Ln is pyridine, THF or diethylether. A compound of formula Cp″Cr(Cl)2(Ln), where Cp″ is η5-C5H4C(Me)2CH2CH2CH═CH2 and Ln is pyridine, THF or diethylether.